# US 2017/0283682 A1 · Extended-life calcium aluminate cementing methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283682 A1
- Document ID: US20170283682A1
- Status: Published application
- Kind: A1
- Application number: 15/510,450
- Filed: 2014-10-10
- Published: 2017-10-05
- Earliest claimed: 2014-10-10
- Assignees: Halliburton Energy Services, Inc.
- Applicants: Halliburton Energy Services, Inc.
- Inventors: Kyriacos Agapiou; Samuel J. Lewis; Thomas Jason Pisklak
- Web page: https://patentgrep.com/patent/US20170283682A1

## CPC

- C09K 8/467: containing additives for specific purposes
- C04B 14/04: Silica-rich materials; Silicates
- C04B 18/08: Flue dust {, i.e. fly ash}
- C04B 18/146: {Silica fume}
- C04B 22/062: {of the alkali or alkaline-earth metals}
- C04B 22/082: {Acids}
- C04B 22/10: containing carbon in the anion, e.g. carbonates
- C04B 24/04: Carboxylic acids; Salts, anhydrides or esters thereof
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 40/0658: {Retarder inhibited mortars activated by the addition of accelerators or retarder-neutralising agents}
- E21B 33/14: for cementing casings into boreholes
- C04B 2103/12: Set accelerators
- C04B 2103/22: Set retarders
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Methods of using extended-life cement compositions are disclosed. A method comprises providing an extended-life cement composition comprising calcium-aluminate cement, water, and a cement set retarder. The method additionally comprises mixing the extended-life cement composition with a cement set activator to activate the extended-life cement composition. The method further comprises Introducing the activated extended-life cement composition into a subterranean formation and allowing the activated extended-life cement composition to set in the subterranean formation; wherein the activated extended-life cement composition has a thickening time of greater than about two hours.

## Claims

### Claim 1

A method of cementing comprising:
providing an extended-life cement composition comprising calcium-aluminate cement, water, and a cement set retarder;
mixing the extended-life cement composition with a cement set activator to activate the extended-life cement composition;
introducing the activated extended-life cement composition into a subterranean formation; and
allowing the activated extended-life cement composition to set in the subterranean formation; wherein the activated extended-life cement composition has a thickening time of greater than about two hours.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the cement set retarder is selected from the group consisting of hydroxycarboxylic acids or their respective salts, boric acid or its respective salt, and any combination thereof.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the cement set retarder is present in an amount of about 0.01% to about 10% by weight of the extended-life cement composition.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the cement set activator is selected from the group consisting of Groups IA and IIA hydroxides; alkaline aluminates; Portland cement, and the like.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the cement set activator is present in an amount of about 0.01% to about 10% by weight of the extended-life cement composition.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the extended-life cement composition further comprises at least one dispersant selected from the group consisting of a sulfonated-formaldehyde-based dispersant, a polycarboxylated ether dispersant, and any combination thereof.

### Claim 7 (depends on 6)

A method according to claim 6, wherein the dispersant is present in an amount of about 0.01% to about 5% by weight of the extended-life cement composition.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the extended-life cement composition further comprises at least one lithium salt selected from the group consisting of lithium sulfate, lithium carbonate, and any combination thereof.

### Claim 9 (depends on 8)

A method according to claim 8, wherein the lithium salt is present in an amount of about 0.01% to about 10% by weight of the extended-life cement composition.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the extended-life cement composition further comprises a filler material selected from the group consisting of silica, sand, fly ash, or silica fume, and any combination thereof.

### Claim 11 (depends on 10)

A method according to claim 10, wherein the filler material is present in an amount of about 0.01% to about 100% by weight of the calcium aluminate cement.

### Claim 12

A method of cementing comprising:
providing an extended-life cement composition comprising calcium-aluminate cement, water, and a cement set retarder;
storing the extended-life cement composition for a time period of about 1 day or longer in a vessel;
mixing the extended-life cement composition with a cement set activator to activate the extended-life cement composition;
introducing the activated extended-life cement composition into a subterranean formation; and
allowing the activated extended-life cement composition to set in the subterranean formation; wherein the activated extended-life cement composition has a thickening time of greater than about two hours.

### Claim 13 (depends on 12)

A method according to claim 12, further comprising storing the extended-life cement composition for a time period of at least about 7 days or longer prior to the step of mixing.

### Claim 14 (depends on 12)

A method according to claim 12, further comprising storing the extended-life cement composition for a time period of at least about 30 days or longer prior to the step of mixing.

### Claim 15 (depends on 12)

A method according to claim 12, wherein mixing the cement set activator with the extended-life cement composition comprises adding the cement set activator to mixing equipment comprising the extended-life cement composition.

### Claim 16 (depends on 12)

A method according to claim 12, wherein the cement set activator and the extended-life cement composition are continuously mixed as the extended-life cement composition is pumped into a well bore penetrating the subterranean formation.

### Claim 17 (depends on 12)

A method according to claim 12, further comprising pumping the activated extended-life cement composition through a conduit and into a wellbore annulus that is penetrating the subterranean formation.

### Claim 18 (depends on 12)

A method according to claim 12, wherein the activated extended-life cement composition has a thickening time of about six hours or greater.

### Claim 19 (depends on 12)

A method according to claim 12, wherein the subterranean formation has a temperature of about 100° F. or less.

### Claim 20 (depends on 12)

A method according to claim 12, wherein the activated extended-life cement composition is used in a primary cementing method.