# US 2017/0283678 A1 · Modification of bentonite properties for drilling fluids

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283678 A1
- Document ID: US20170283678A1
- Status: Published application
- Kind: A1
- Application number: 15/088,990
- Filed: 2016-04-01
- Published: 2017-10-05
- Earliest claimed: 2016-04-01
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Mansour A. Al-Shafei; Akram A. Alfliow; Awad M. Al-Mofleh; Jamal M. Al-Aamri; Syed Rehan Ahmad Zaidi; Amer A. Al-Tuwailib
- Web page: https://patentgrep.com/patent/US20170283678A1

## CPC

- C09K 8/05: containing inorganic compounds only, e.g. mixtures of clay and salt
- C01B 33/40: Clays
- C09C 1/42: Clays
- C09K 8/03: Specific additives for general use in well-drilling compositions
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}

## Abstract

Disclosed is a method for modifying bentonite to allow the bentonite to be useful in drilling mud applications. The method includes the steps of: preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite; grinding the bentonite to a fine powder; sieving the fine powder to be between about 50 μm and about 150 μm in particle size to produce a sieved fine powder; mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition; adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and allowing the homogeneous solution of modified bentonite in water to rest for about 16 hours to form a composition useful in drilling mud applications.

## Claims

### Claim 1

A method for modifying bentonite to allow the bentonite to be useful in drilling mud applications, the method comprising the steps of:
preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite;
grinding the bentonite to a fine powder;
sieving the fine powder to be between about 50 μm and about 150 μm in particle size to produce a sieved fine powder;
mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition;
adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and
allowing the homogeneous solution of modified bentonite in water to sit at rest to form a composition useful in drilling mud applications.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the homogeneous solution of modified bentonite in water is formed in about 20 minutes.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the composition useful in drilling mud applications substantially meets the American Petroleum Institute's (API's) requirements for drilling mud.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the bentonite local to Saudi Arabia is a sodium-type bentonite and no hydroxide compositions are used in the method for modifying bentonite.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the bentonite local to Saudi Arabia comprises by weight percent about 58% sodium montmorillonite, about 5% feldspar, about 25% SiO2, about 8% kaolinite, about 2% halite, and about 2% illite.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises by weight percent about 71% sodium montmorillonite, about 5% feldspar, about 15% SiO2, about 6% kaolinite, about 0% halite, and about 1% illite.

### Claim 7 (depends on 1)

The method according to claim 1, further comprising the step of verifying that viscosity of the homogeneous solution of modified bentonite in water substantially meets the API's requirements for viscosity of drilling mud.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising the step of mixing the sieved fine powder with low viscosity sodium carboxymethyl cellulose.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises between about 3% and about 11% polyanionic cellulose polymer by weight.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises between about 4% and about 10% polyanionic cellulose polymer by weight.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises between about 4% and about 9% polyanionic cellulose polymer by weight.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises between about 5% and about 8% polyanionic cellulose polymer by weight.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the modified bentonite composition comprises about 8.5% polyanionic cellulose polymer by weight.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the polyanionic cellulose polymer comprises at least a first polyanionic cellulose polymer and a second polyanionic cellulose polymer.

### Claim 15 (depends on 1)

The method according to claim 1, further comprising the step of conducting x-ray powder diffraction (XRD) to verify that the composition useful in drilling mud applications substantially meets the API requirements for drilling mud.

### Claim 16 (depends on 1)

The method according to claim 1, further comprising the step of applying the composition useful in drilling mud applications to a wellbore hydrocarbon recovery operation.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the step of allowing the homogeneous solution of modified bentonite in water to sit at rest to form a composition useful in drilling mud applications continues for about 16 hours.

### Claim 18

A modified bentonite composition useful in drilling mud applications, the composition comprising:
a powdery mixture composition comprising:
about 90% by weight bentonite local to Saudi Arabia, the bentonite existing as a fine powder, the fine powder to be between about 50 μm and about 150 μm in particle size, and
about 10% by weight polyanionic cellulose polymer; and
water.

### Claim 19 (depends on 18)

The composition according to claim 18, wherein the powdery mixture composition comprises by weight percent about 71% sodium montmorillonite, about 5% feldspar, about 15% SiO2, about 6% kaolinite, about 0% halite, and about 1% illite.

### Claim 20 (depends on 18)

The composition according to claim 18, wherein the modified bentonite composition substantially meets the API's requirements for drilling mud.

### Claim 21 (depends on 18)

The composition according to claim 18, further comprising soda ash.