# US 2017/0283674 A1 · A process for preparation of homogenous mixture for thermal storage and heat transfer applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283674 A1
- Document ID: US20170283674A1
- Status: Published application
- Kind: A1
- Application number: 15/511,485
- Filed: 2016-05-24
- Published: 2017-10-05
- Earliest claimed: 2015-05-25
- Assignees: Hindustan Petroleum Corporation Limited
- Applicants: Hindustan Petroleum Corporation Ltd.
- Inventors: Kanaparthi Ramesh; Kandoth Madathil Pramod; Peddy Venkat Chalapathi Rao; Nettem Venkateswarlu Choudary
- Web page: https://patentgrep.com/patent/US20170283674A1

## CPC

- C09K 5/063: {Materials absorbing or liberating heat during crystallisation; Heat storage materials}
- C01B 21/48: Methods for the preparation of nitrates in general (particular individual nitrates, see the relevant groups of subclasses C01B - C01G, according to the cation)
- C09K 5/12: Molten materials, i.e. materials solid at room temperature, e.g. metals or salts
- F24S 80/20: Working fluids specially adapted for solar heat collectors
- Y02E 10/40: Solar thermal energy, e.g. solar towers
- Y02E 60/14: Thermal energy storage
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- F24S: SOLAR HEAT COLLECTORS; SOLAR HEAT SYSTEMS (for producing mechanical power from solar energy F03G6/00)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

In accordance with the present subject matter there is provided a hygroscopic homogenous salt mixture including at least one alkali metal salt and a metal salt having water of crystallization. The subject matter also relates to a method for preparation of hygroscopic homogenous salt mixture.

## Claims

### Claim 1

A method for preparation of hygroscopic homogenous salt mixture, the method comprising:
a) contacting at least one alkali metal salt with a metal salt having water of crystallization to form a heterogeneous mixture;
b) subjecting said heterogeneous mixture to a temperature of 140 to 180° C. in a closed system to obtain a homogenous mixture; and
c) removing water from the homogeneous mixture to obtain a hygroscopic homogenous salt mixture.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the at least one alkali metal salt is selected from the group consisting of lithium salt of inorganic anions, sodium salt of inorganic anions, potassium salt of inorganic anions, and combinations thereof.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the at least one alkali metal salt is selected from the group consisting of lithium metal salt, potassium metal salt, and combinations thereof.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the at least one alkali metal salt weight ratio in the heterogeneous mixture is in the range of 65 to 90%.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the at least one alkali metal salt is a combination of lithium and potassium nitrate.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein potassium nitrate weight ratio in the heterogeneous mixture is in the range of 60 to 70% and lithium nitrate weight ratio in the heterogeneous mixture is in the range of 5 to 20%.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the-at least one alkali metal salt is dried at a temperature in the range of 80 to 120° C. under reduced pressure before carrying out the contacting at least one alkali metal salt with the metal salt having water of crystallization to form the heterogeneous mixture.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the metal salt having water of crystallization is selected from the group consisting of alkali metal salt, alkaline earth metal salt, and transitional metal salt.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the metal salt having water of crystallization has melting point in the range 40 to 120° C.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the metal salt having water of crystallization has melting point in the range 40 to 80° C.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein the metal salt having water of crystallization weight ratio in the heterogeneous mixture is in the range of 10 to 35%.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein the heterogeneous mixture has moisture content in the range 3 to 13 wt %.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the heterogeneous mixture is subjected to a temperature of 140 to 180° C. for 0.5 to 1.5 h.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the heterogeneous mixture is subjected to a temperature of 140 to 180° C. at a pressure in the range of 1.3 to 3 bars.

### Claim 15 (depends on 1)

The method as claimed in claim 1, wherein the hygroscopic homogenous salt mixture has a melting temperature in the range of 100 to 150° C.

### Claim 16

A method for preparation of hygroscopic homogenous salt mixture, the method comprising:
a) contacting 60 to 70 wt % potassium nitrate and 5 to 20 wt % lithium nitrate with 10 to 35 wt % of a metal salt having water of crystallization to form a heterogeneous mixture;
b) subjecting said heterogeneous mixture to a temperature of 140 to 180° C. in a pressure tube for 0.5 to 1.5 h to obtain a homogenous mixture; and
c) removing water from the homogeneous mixture to obtain a hygroscopic homogenous salt mixture with a melting temperature in the range of 100 to 150° C. .

### Claim 17

A hygroscopic homogenous salt mixture comprising: (a) at least one alkali metal salt; and (b) a metal salt having water of crystallization, wherein the hygroscopic homogenous salt mixture has a melting temperature in the range of 100 to 150° C,.
wherein the at least one alkali metal salt is a combination of lithium nitrate having weight ratio in the range of 5 to 20% and potassium nitrate having weight ratio in the range of 60 to 70%.

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20 (depends on 17)

The salt mixture as claimed in claim 17, wherein the metal salt having water of crystallization is selected from the group consisting of alkali metal salt, alkaline earth metal salt, and transitional metal salt and the weight ratio in the homogeneous mixture is in the range of 10 to 35%.

### Claim 21 (depends on 17)

The salt mixture as claimed in claim 17 for use as solar thermal energy storage.