# US 2017/0283661 A1 · Surface protection sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283661 A1
- Document ID: US20170283661A1
- Status: Published application
- Kind: A1
- Application number: 15/472,413
- Filed: 2017-03-29
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: Nitto Denko Corporation; Nitto Belgium NV
- Applicants: Nitto Denko Corporation; Nitto Belgium NV
- Inventors: Kousuke YONEZAKI; Yutaka TOSAKI; Minoru HANAOKA; Bart FORIER; Greet BOSSAERT; Donald PINXTEN; Michael PELLENS
- Web page: https://patentgrep.com/patent/US20170283661A1

## CPC

- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 220/1808: {C8-(meth)acrylate, e.g. isooctyl (meth)acrylate or 2-ethylhexyl (meth)acrylate}
- C09J 7/22: Plastics; Metallised plastics
- C09J 7/243: {Ethylene or propylene polymers}
- C09J 7/38: Pressure-sensitive adhesives [PSA]
- C09J 7/385: {Acrylic polymers}
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2433/00: Presence of (meth)acrylic polymer
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

Provided is a surface protection sheet that is less susceptible to breaking and tearing caused by adherend processing and can be easily removed from the adherend. The surface protection sheet comprises a substrate and a PSA layer placed on one face of the substrate. The base polymer of the PSA layer has a glass transition temperature of −50° C. or higher. The surface protection sheet has at least 200% elongation at break in both the machine direction and the transverse direction.

## Claims

### Claim 1

A surface protection sheet comprising a substrate and a pressure-sensitive adhesive layer placed on one face of the substrate, wherein:
the surface protection sheet has 200% or greater elongation at break EbMD in its machine direction as well as 200% or greater elongation at break EbTD in its transverse direction, and the pressure-sensitive adhesive layer comprises a base polymer having a glass transition temperature of −50° C. or higher.

### Claim 2 (depends on 1)

The surface protection sheet according to claim 1, wherein the pressure-sensitive adhesive layer has toluene-insoluble fractions having a weight fraction GC of 60% or higher and toluene-soluble fractions having a weight average molecular weight SMw of 10×104 or higher.

### Claim 3 (depends on 1)

The surface protection sheet according to claim 1, wherein, by nanoindentation, the pressure-sensitive adhesive layer shows an unloading curve having a minimum load of less than −2.0 μN.

### Claim 4 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer has a glass transition temperature of −40° C. or higher and −10° C. or lower.

### Claim 5 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer is a polymer of a starting monomer mixture comprising a monomer whose homopolymer has a glass transition temperature of 10° C. or higher in an amount of 20% by weight or more of the total monomer content.

### Claim 6 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer is a polymer of a starting monomer mixture that comprises a monomer whose homopolymer has a glass transition temperature of 60° C. or higher in an amount of 10% by weight or more of the total monomer content.

### Claim 7 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer comprises an acrylic polymer.

### Claim 8 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer is a polymer of a starting monomer mixture that comprises an alkyl (meth)acrylate whose homopolymer has a glass transition temperature of 10° C. or higher in an amount of 10% by weight or more of the total monomer content.

### Claim 9 (depends on 1)

The surface protection sheet according to claim 1, wherein the base polymer is a polymer of a starting monomer mixture that comprises methyl methacrylate in an amount of 10% by weight or more of the total monomer content.

### Claim 10 (depends on 1)

The surface protection sheet according to claim 1, wherein the pressure-sensitive adhesive layer is an acrylic pressure-sensitive adhesive layer.

### Claim 11 (depends on 1)

The surface protection sheet according to claim 1, wherein the substrate has a thickness of 100 μm or less.

### Claim 12 (depends on 1)

The surface protection sheet according to claim 1, wherein the substrate comprises polyolefinic resin film.

### Claim 13 (depends on 1)

The surface protection sheet according to claim 1 having an aged peel strength PA of 0.70 N/20 mm or less, determined at a peeling rate of 3 m/min after the surface protection sheet is applied to a stainless steel plate and stored at 60° C. for seven days.

### Claim 14 (depends on 13)

The surface protection sheet according to claim 13 having an initial peel strength P0 (in N/20 mm), determined at a peeling rate of 3 m/min at 15 minutes after the surface protection sheet is applied to a stainless steel plate, wherein the aged peel strength PA (in N/20 mm) is up to 2.0 times the initial peel strength P0.

### Claim 15 (depends on 1)

The surface protection sheet according to claim 1 used on a metal plate to be drawn.

### Claim 16 (depends on 1)

The surface protection sheet according to claim 1, wherein the pressure-sensitive adhesive layer is formed from an emulsion pressure-sensitive adhesive composition.

### Claim 17 (depends on 16)

The surface protection sheet according to claim 16, wherein the emulsion pressure-sensitive adhesive composition comprises an acrylic polymer synthesized using a reactive surfactant.

### Claim 18

A surface protection sheet comprising a substrate and a pressure-sensitive adhesive layer placed on one face of the substrate, wherein
the pressure-sensitive adhesive layer has toluene-insoluble fractions having a weight fraction GC of 60% or higher and toluene-soluble fractions having a weight average molecular weight SMw of 10×104 or higher,
the pressure-sensitive adhesive layer is an acrylic pressure-sensitive adhesive layer comprising an acrylic polymer as its base polymer,
the acrylic polymer is a polymer of a starting monomer mixture that comprises methyl methacrylate in an amount of 20% by weight or more of the total monomer content, with the acrylic polymer having a glass transition temperature of −40° C. or higher and −10° C. or lower,
the substrate is a linear low density polyethylene film or a low density polyethylene film, the substrate having a thickness of 40 μm or larger and 100 μm or smaller, and
the surface protection sheet has 500% or greater elongation at break EbMD in its machine direction as well as 500% or greater elongation at break EbTD in its transverse direction.