# US 2017/0283652 A9 · Can pretreatment for improved coating adhesion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283652 A9
- Document ID: US20170283652A9
- Status: Published application
- Kind: A9
- Application number: 14/702,076
- Filed: 2015-05-01
- Published: 2017-10-05
- Earliest claimed: 2012-11-08
- Assignees: Henkel AG & Co. KGaA
- Applicants: Henkel AG & Co. KGaA
- Inventors: Joerg Riesop
- Web page: https://patentgrep.com/patent/US20170283652A9

## CPC

- C09D 179/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08K 3/16: Halogen-containing compounds
- C23C 22/34: containing fluorides or complex fluorides
- C23C 22/361: {containing titanium, zirconium or hafnium compounds}
- C23C 22/83: Chemical after-treatment
- B21D 22/201: {Work-pieces; preparation of the work-pieces, e.g. lubricating, coating}
- B21D 51/26: cans or tins; Closing same in a permanent manner (making outlet arrangements B21D51/38; welding or soldering B23K)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)

## Abstract

The invention relates to the use of an acidic aqueous composition for pretreating cans, wherein an inorganic-organic conversion layer is formed in the course of the pretreatment, said conversion layer, as such, offering an excellent adhesive base for wax which improves sliding of the formed can and for the subsequent coating. The invention relates to a wet-chemical pretreatment method in which a can cylinder is first contacted with an acidic aqueous composition that contains water-soluble inorganic compounds of Zr, Ti, Si, Hf or Ce, and water-soluble polymers comprising carboxyl groups or hydroxyl groups; and subsequently is contacted with an aqueous wax dispersion. The invention further relates to an acidic aqueous composition suitable for the pretreatment method comprising water-soluble polymers selected from condensation products of glycoluril and aldehydes. The invention further relates to a method for producing can cylinders, said method including the pretreatment according to the invention.

## Claims

### Claim 1

A process for surface-treating a can cylinder which is deep-drawn from a metal sheet and is open at one end, comprising steps of:
(i) contacting at least an outer circumferential surface of a can cylinder that is open at one end with an acidic aqueous composition containing:
a) at least one water-soluble inorganic compound of an element selected from Zr, Ti, Si, Hf, Ce and combinations thereof; and
b) at least one water-soluble organic resin, which comprises at least carboxyl groups or hydroxyl groups, having an acid value and/ or a hydroxyl value wherein a sum of the acid value and/or hydroxyl value of the at least one water-soluble organic resin is at least 50 mg KOH/g;
and subsequently—with or without an intermediate flushing step—
(ii) contacting at least the outer circumferential surface of the can cylinder from step (i) with an aqueous dispersion of a wax.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the water-soluble compounds of component a) of the acidic aqueous composition in step (i) are selected from fluoro complexes of the elements Zr, Ti, and/or Si.

### Claim 3 (depends on 1)

The process according to claim 1 , wherein content of the at least one water-soluble inorganic compound of an element selected from Zr, Ti, Si, Hf, Ce and combinations thereof falling under component a) in the acidic aqueous composition in step (i) is in a range of 0.01 to 1 g/L with respect to a total content of said elements.

### Claim 4 (depends on 3)

The process according to claim 3, wherein amount of water-soluble inorganic compounds of Zr and/or Ti is at least 0.01 g/L, with respect to total content of the elements Zr and Ti.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the water-soluble organic resin falling under component b) of the acidic aqueous composition in step (i) is selected from polymers or copolymers based on vinyl ethers, vinyl alcohols, (meth)acrylic acid, maleic acid, or fumaric acid, from hydroxyl group-containing polyesters, and from condensation products of glycoluril or melamine with aldehydes.

### Claim 6 (depends on 1)

The process according to claim 1, wherein content of water-soluble organic resins falling under component b) in the acidic aqueous composition in step (i) is in a range of 0.1 to 50 g/L.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the acidic aqueous composition in step (i) additionally contains phosphate ions in an amount of at least 0.1 g/L, but not more than 10 g/L.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the acidic aqueous composition in step (i) has a pH value of not less than 2 and not greater than 6.

### Claim 9 (depends on 1)

The process according to claim 1, wherein the wax in the aqueous dispersion in step (ii) is selected from synthetic waxes present in the aqueous dispersion in a range of 0.1 to 50 g/L.

### Claim 10 (depends on 1)

The process according to claim 1, wherein steps (i) and (ii) is in each case carried out by spraying-on.

### Claim 11 (depends on 1)

The process according to claim 1, further comprising a step wherein at least the outer circumferential surface of the can cylinder that is open at one end is provided with a protective coat after step (ii) and optionally after a flushing step that directly follows step (ii).

### Claim 12 (depends on 1)

The process according to claim 1, wherein the can cylinder is not shaped in a rim region that is open at one end.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the can cylinder is deep-drawn from tinplate, steel sheet, or aluminum sheet.

### Claim 14 (depends on 10)

A production process for can cylinders, in which
A. a circular blank of a metal sheet is deep-drawn to form a can cylinder that is open at one end;
B. the can cylinder that is open at one end is pretreated and coated in a process according to claim 10; and
C. the pretreated and coated can cylinder is drawn-in in a rim region that is open at one end in order to taper a diameter of the can cylinder and/or is shaped to form a flange in a rim region that is open at one end.

### Claim 15

An acidic aqueous composition having a pH value in the range of 2 to 5, for surface-treating metallic cans, comprising:
a) 0.005 to 0.5 wt. % fluoro complexes of elements Zr, Ti, and/or Si, with respect to the respective elements; and
b) 0.1 to 3 wt. % water-soluble resins selected from condensation products of glycoluril with aldehydes.

### Claim 16 (depends on 15)

The acidic aqueous composition according to claim 15, wherein the condensation product of glycoluril with aldehydes has a hydroxyl value of at least 50 mg KOH/g.