# US 2017/0283624 A1 · Metal powder sintering paste and method of producing the same, and method of producing conductive material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283624 A1
- Document ID: US20170283624A1
- Status: Published application
- Kind: A1
- Application number: 15/477,868
- Filed: 2017-04-03
- Published: 2017-10-05
- Earliest claimed: 2016-04-04
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Teppei KUNIMUNE; Masafumi KURAMOTO
- Web page: https://patentgrep.com/patent/US20170283624A1

## CPC

- H01B 1/22: the conductive material comprising metals or alloys
- B22F 1/068: Flake-like particles
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- B22F 9/30: with decomposition of metal compounds, e.g. by pyrolysis
- C09D 5/24: Electrically-conducting paints {(conductive materials H01B1/00)}
- C09D 7/68: {Particle size between 100-1000 nm}
- B22F 2201/03: Oxygen
- B22F 2201/50: air
- B22F 2301/255: Silver or gold
- B22F 2998/10: Processes characterised by the sequence of their steps
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

There is a problem that when a silver powder sintering paste that is substantially free from resin is used, an organic solvent used as a dispersion medium bleeds, which results in contamination and wire bonding defects. In order to solve the problem, provided is a metal powder sintering paste that contains, as a principal component, silver particles having an average particle diameter (a median diameter) of 0.3 μm to 5 μm and further contains an anionic surfactant but is substantially free from resin.

## Claims

### Claim 1

A metal powder sintering paste,
the paste comprising, as a principal component, silver particles having an average particle diameter (a median diameter) of 0.3 μm to 5 μm, and
further comprising an anionic surfactant, and
being substantially free from resin.

### Claim 2 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the surfactant is one in which when the temperature is increased with TG-DTA from room temperature to 350° C. at 2° C./min, the residue is reduced to not more than 20% by mass with respect to the initial mass.

### Claim 3 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the surfactant is saturated carboxylic acid represented by Formula (I) below:
R1O(CH2CH(R2)O)n1CH2COOR3 (I)
wherein R1 is a linear or branched alkyl group having at least 7 carbon atoms,
R2 is any one of —H, —CH3, —CH2CH3, and —CH2CH2CH3,
R3 is —H or alkali metal, and
n1 is in a rage of 2 to 5.

### Claim 4 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the content of the surfactant is not more than 2% by mass with respect to the paste.

### Claim 5 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the surfactant is liquid at 25° C.

### Claim 6 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the silver particles are in a flake form.

### Claim 7 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
in the silver particles, the content of particles with a particle diameter of smaller than 0.3 μm is not more than 5% by mass.

### Claim 8 (depends on 7)

The metal powder sintering paste according to claim 7, wherein
in the silver particles, the content of particles with a particle diameter of smaller than 0.5 μm is not more than 15% by mass.

### Claim 9 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the metal powder sintering paste further comprises an organic solvent as a dispersion medium.

### Claim 10 (depends on 9)

The metal powder sintering paste according to claim 9, wherein
the organic solvent has a boiling point in a range of 150 to 250° C.

### Claim 11 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
a conductive material obtained after the metal powder sintering paste is sintered has an electric resistance of not higher than 6 μΩ·cm.

### Claim 12 (depends on 1)

The metal powder sintering paste according to claim 1, wherein
the content of the silver particles is at least 70% by mass with respect to the paste.

### Claim 13

A method of producing a metal powder sintering paste, comprising mixing an anionic surfactant and silver particles having an average particle diameter (a median diameter) of 0.3 μm to 5 μm together but substantially not with resin.

### Claim 14 (depends on 1)

A method of producing a conductive material, comprising a step of calcining a metal powder sintering paste according to claim 1.

### Claim 15 (depends on 14)

The method of producing a conductive material according to claim 14, wherein
the calcining is carried out at a temperature in a range of 160° C. to 300° C.

### Claim 16 (depends on 14)

The method of producing a conductive material according to claim 14, wherein
the calcining is carried out in an air oven at 160° C. to 250° C. for 30 to 120 minutes.