# US 2017/0283615 A1 · Improved asphalt products and materials and methods of producing them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283615 A1
- Document ID: US20170283615A1
- Status: Published application
- Kind: A1
- Application number: 15/507,475
- Filed: 2015-08-31
- Published: 2017-10-05
- Earliest claimed: 2014-08-29
- Assignees: Iowa State University Research Foundation, Inc.
- Applicants: Iowa State University Research Foundation, Inc.
- Inventors: R. Christopher WILLIAMS; Joseph Herbert PODOLSKY; Eric W. COCHRAN
- Web page: https://patentgrep.com/patent/US20170283615A1

## CPC

- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C07D 493/00: Heterocyclic compounds containing oxygen atoms as the only ring hetero atoms in the condensed system
- C07D 493/04: Ortho-condensed systems
- C08K 5/05: Alcohols; Metal alcoholates
- C08K 5/1515: Three-membered rings
- C08L 2555/24: Asphalt produced between 100°C and 140°C, e.g. warm mix asphalt
- C08L 2555/64: Oils, fats or waxes based upon fatty acid esters, e.g. fish oil, olive oil, lard, cocoa butter, bees wax or carnauba wax
- Y02A 30/30: in transportation, e.g. on roads, waterways or railways
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02A: TECHNOLOGIES FOR ADAPTATION TO CLIMATE CHANGE

## Abstract

The present invention relates to a method of producing an improved asphalt. The method involves providing an asphalt and providing a compound of formula (I), as described herein. The asphalt is mixed with the compound of formula (I) under conditions effective to produce an improved asphalt. Also disclosed are an asphalt product and a method of making asphalt material. The invention further discloses a method of producing an improved asphalt comprising providing a polymer modified asphalt and providing a compound of formula (IIa) or formula (II). The polymer modified asphalt is mixed with the compound of formula (IIa) or formula (IIb) under conditions effective to produce an improved asphalt, which is yet another aspect of the present invention.

## Claims

### Claim 1

A method of producing an improved asphalt comprising:
providing an asphalt;
providing a compound of formula (I)
wherein:
each A is selected independently at each occurrence thereof from the group consisting of
and
wherein at least one A is
each
represents the point of attachment to a —CH2— group;
n is 1;
R is methyl; and
mixing the asphalt with the compound of formula (I) under conditions effective to produce an improved asphalt.

### Claim 2 (depends on 1)

The method of claim 1, wherein the compound of formula (I) is the compound of any one of formulae (Ia)-(Ik):

### Claim 3 (depends on 1)

The method of claim 1, wherein the compound of formula (I) is epoxidized methyl soyate.

### Claim at position 4

-12. (canceled)

### Claim 13

An asphalt product comprising:
an asphalt and
a compound of formula (I)
wherein:
each A is selected independently at each occurrence thereof from the group consisting of
and
wherein at least one A is
each
represents the point of attachment to a —CH2— group;
n is 1;
R is methyl, mixed with the asphalt.

### Claim 14 (depends on 13)

The asphalt product of claim 13, wherein the compound of formula (I) is the compound of any one of formulae (Ia)-(Ik):

### Claim 15 (depends on 13)

The asphalt product of claim 13, wherein the compound of formula (I) is epoxidized methyl soyate.

### Claim 16 (depends on 13)

The asphalt product of claim 13, wherein the asphalt product has a viscosity of 0.23-0.33 Pa·s at a temperature ranging from 130° C. to 150° C.

### Claim 17 (depends on 13)

The asphalt product of claim 13, wherein the asphalt product has a viscosity of 0.13-0.21 Pa·s at a temperature ranging from 150° C. to 165° C.

### Claim 18 (depends on 13)

The asphalt product of claim 13 further comprising:
a mineral aggregate, wherein the asphalt product has a minimum compaction force index of 1050 at a temperature ranging from 100° C. to 140° C.

### Claim 19 (depends on 13)

The asphalt product of claim 13 further comprising:
a mineral aggregate, wherein the asphalt product has a maximum compaction force index energy of 1650 at a temperature ranging from 100° C. to 140° C.

### Claim 20 (depends on 13)

The asphalt product of claim 13 further comprising:
a mineral aggregate.

### Claim at position 13

-22. (canceled)

### Claim 23 (depends on 13)

The asphalt product of claim 13, wherein the asphalt product is in the form of an asphalt mixture.

### Claim 24

(canceled)

### Claim 25 (depends on 23)

In a roofing shingle, the improvement comprising the asphalt product of claim 23.

### Claim 26

A method of making an asphalt material comprising the steps of:
(a) providing an improved asphalt product comprising:
an asphalt and
a compound of formula (I)
wherein:
each A is selected independently at each occurrence thereof from the group consisting of
and
wherein at least one A is
each
represents the point of attachment to a —CH2— group;
n is 1;
R is methyl;
(b) mixing the improved asphalt product with a mineral aggregate at a temperature of 150° C. or lower, to coat the mineral aggregate and produce a heated paving material which, at a warm mix temperature, has a compaction production temperature at least 15-50° C. lower than that produced when the improved asphalt material is prepared in the absence of the compound of formula (I);
(c) applying the heated paving material to a surface to be paved to form an applied paving material, and
(d) compacting the applied paving material, to a void fraction of less than 8%, at a compacting temperature of 140° C. or lower to form a paved surface.

### Claim 27

(canceled)

### Claim 28 (depends on 26)

The method of claim 26, wherein the compound of formula (I) is epoxidized methyl soyate

### Claim at position 20

-34. (canceled)

### Claim 35

A method of producing an improved polymer modified asphalt comprising:
providing a polymer modified asphalt;
providing a compound of formula (IIa) or formula (IIb)
and
mixing the polymer modified asphalt with the compound of formula (IIa) or formula (IIb) under conditions effective to produce an improved polymer modified asphalt.

### Claim 36 (depends on 35)

The method of claim 35, wherein the compound of formula (IIa) or formula (IIb) is epoxidized methyl soyate.

### Claim at position 23

-40. (canceled)

### Claim 41

A polymer modified asphalt product comprising:
a polymer modified asphalt and
a compound of formula (IIa) or formula (IIb)
mixed with the polymer modified asphalt.

### Claim 42 (depends on 41)

The polymer modified asphalt product of claim 41, wherein the compound of formula (IIa) or formula (IIb) is epoxidized methyl soyate.

### Claim 43 (depends on 41)

The polymer modified asphalt product of claim 41, wherein the compound of formula (IIa) or formula (IIb) is mixed in an amount of 0.1 to 5.0 wt % with the asphalt.

### Claim at position 27

-45. (canceled)