# US 2017/0283608 A1 · Polyacetal resin composition and sliding member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283608 A1
- Document ID: US20170283608A1
- Status: Published application
- Kind: A1
- Application number: 15/510,092
- Filed: 2015-06-11
- Published: 2017-10-05
- Earliest claimed: 2014-09-29
- Assignees: Polyplastics Co., Ltd.
- Applicants: Polyplastics Co., Ltd.
- Inventors: Akihide SHIMODA
- Web page: https://patentgrep.com/patent/US20170283608A1

## CPC

- C08L 59/00: Compositions of polyacetals; Compositions of derivatives of polyacetals (of polyvinyl acetals C08L29/14)
- C08L 59/04: Copolyoxymethylenes
- C08K 3/26: Carbonates; Bicarbonates
- C08K 5/103: with polyalcohols
- C08K 5/13: Phenols; Phenolates
- C08K 5/16: Nitrogen-containing compounds {(C08K5/0091 takes precedence)}
- C08L 23/02: not modified by chemical after-treatment
- C08L 23/26: modified by chemical after-treatment (saponified copolymers C08L23/0861; unsaturated acid salts C08L23/0876)
- C08L 71/02: Polyalkylene oxides
- F16C 17/00: Sliding-contact bearings for exclusively rotary movement (F16C32/06 takes precedence; adjustable bearings F16C23/00, F16C25/00)
- F16C 33/20: Sliding surface consisting mainly of plastics (F16C33/22 - F16C33/28 take precedence)
- F16C 33/201: {Composition of the plastic}
- C08K 2003/265: {Calcium, strontium or barium carbonate}
- C08L 2205/03: containing three or more polymers in a blend
- F16C 2208/66: Acetals, e.g. polyoxymethylene [POM]
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS

## Abstract

A polyoxymethylene (POM) resin composition which is used for a resin molded article having a superior sliding characteristic. The POM resin composition contains: (A) 100 parts by mass of a POM resin; (B) 0.01-1 parts by mass of a hindered phenolic antioxidant; (C) 0.05-1 parts by mass of a nitrogen-containing compound; (D) 0.5-10 parts by mass of a modified olefin polymer; (E) 0.01-5 parts by mass of an alkylene glycol polymer; (F) 0.1-20 parts by mass of calcium carbonate; (G) 0.1-10 parts by mass of a partial ester of a polyhydric alcohol; and (H) 0.1-10 parts by mass of an a-olefin oligomer. An ISO tensile test piece, which is obtained by injection molding at a die temperature of 90° C. and a cylinder temperature of 200° C., is crushed, Soxhlet extraction is performed for 3 hours at 70° C. using methanol, and the alkylene glycol polymer is measured. The weight of the alkylene glycol polymer is 0.001 wt % or less relative to 100 wt % of the test piece.

## Claims

### Claim 1

A polyacetal resin composition, comprising:
(A) 100 parts by mass of a polyacetal resin;
(B) from 0.01 parts by mass to 1 part by mass of a hindered phenol-based antioxidizing agents;
(C) from 0.05 parts by mass to 1 part by mass of a nitrogen-containing compound;
(D) from 0.5 parts by mass to 10 parts by mass of a modified olefin-based polymer;
(E) from 0.01 parts by mass to 5 parts by mass of an alkylene glycol-based polymer;
(F) from 0.1 parts by mass to 20 parts by mass of calcium carbonate;
(G) from 0.1 parts by mass to 10 parts by mass of a partial ester of a polyhydric alcohol; and
(H) from 0.1 parts by mass to 10 parts by mass of an alpha olefin oligomer,
wherein the weight of the alkylene glycol-based polymer is 0.001% by weight or less relative to 100% by weight of an ISO tensile test piece as measured after the test piece is pulverized and subjected to Soxhlet extraction with methanol at 70° C. for 3 hours, the test piece being obtained by performing injection molding at a mold temperature of 90° C. and a cylinder temperature of 200° C.

### Claim 2 (depends on 1)

The polyacetal resin composition according to claim 1, wherein particles with a three-dimensional network structure comprising (D) the modified olefin-based polymer are observed when the center of a sample is observed under a scanning electron microscope, the sample being obtained by cutting a cross section between marked lines of the test piece with a trimming diamond blade so as to obtain a mirror surface, and immersed in xylene at 90° C. for 3 hours, and the maximum particle size of the particles from the observation is 10 μm or less.

### Claim 3 (depends on 1)

A sliding member, comprising a resin molded body including the polyacetal resin composition according to claim 1.

### Claim 4 (depends on 2)