# US 2017/0283595 A1 · Olefin polymerization method using barium ferrite-containing catalyst nanoparticles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283595 A1
- Document ID: US20170283595A1
- Status: Published application
- Kind: A1
- Application number: 15/627,776
- Filed: 2017-06-20
- Published: 2017-10-05
- Earliest claimed: 2015-07-10
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Mamdouh Ahmad AL-HARTHI; Farrukh SHEHZAD
- Web page: https://patentgrep.com/patent/US20170283595A1

## CPC

- C08K 3/24: Acids; Salts thereof {(C08K3/16 takes precedence)}
- C08K 3/08: Metals
- C08K 9/02: Ingredients treated with inorganic substances
- C08F 210/02: Ethene
- C08K 2003/0856: {Iron}
- C08K 2201/011: Nanostructured additives
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method involving polymerizing ethylene in the presence of a catalyst composition containing BaFe12O19 nanoparticles, a zirconocene catalyst, and an alkylaluminoxane co-catalyst. A nanocomposite is formed by the polymerization, whereby the BaFe12O19 nanoparticles are dispersed in a matrix of polyethylene (PE), and the % crystallinity is lowered. The activity of the catalyst is increased in the presence of the BaFe12O19 nanoparticles.

## Claims

### Claim 1

A method, comprising:
polymerizing ethylene in the presence of a catalyst composition comprising BaFe12O19 nanoparticles, a zirconocene catalyst, and an alkylaluminoxane co-catalyst, wherein the BaFe12O19 nanoparticles are not pre-reacted or pre-mixed with the zirconocene catalyst or the alkylaluminoxane co-catalyst and wherein a weight ratio of the BaFe12O19 nanoparticles to the zirconocene catalyst is 0.5:1 to 3:1;
wherein the polymerizing forms a nanocomposite in which the BaFe12O19 nanoparticles are dispersed in a matrix of polyethylene (PE).

### Claim 2 (depends on 1)

The method of claim 1, wherein the zirconocene catalyst is zirconocene dichloride.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polymerizing is carried out in a liquid solvent.

### Claim 4 (depends on 3)

The method of claim 3, wherein the liquid solvent is a hydrocarbon solvent.

### Claim 5 (depends on 1)

The method of claim 1, wherein the alkylaluminoxane co-catalyst is methylaluminoxane.

### Claim 6 (depends on 1)

The method of claim 1, wherein the BaFe12O19 nanoparticles have a largest diameter of 1-100 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the polymerizing includes first mixing the zirconocene catalyst and the alkylaluminoxane co-catalyst with the ethylene to form a mixture, then adding the BaFe12O19 nanoparticles to the mixture.

### Claim 8 (depends on 1)

The method of claim 1, wherein a weight ratio of BaFe12O19 nanoparticles to the zirconocene catalyst is 0.5:1 to 1:1, and the catalyst composition has a catalyst activity of 300-350×10−3 kgPE·mol−1·h−1·bar−1.

### Claim 9 (depends on 1)

The method of claim 1, wherein a weight ratio of BaFe12O19 nanoparticles to the zirconocene catalyst is 1.5:1 to 2:1, and the catalyst composition has a catalyst activity of 350-370×10−3 kgPE·mol−1·h−1·bar−1.

### Claim 10 (depends on 1)

The method of claim 1, wherein a weight ratio of BaFe12O19 nanoparticles to the zirconocene catalyst is 2.5:1 to 3:1, and the catalyst composition has a catalyst activity of 280-300×10−3 kgPE·mol−1·h−1·bar−1.

### Claim 11 (depends on 1)

The method of claim 1, wherein the nanocomposite comprises 0.01-1.0 wt % of the BaFe12O19 nanoparticles.

### Claim 12 (depends on 1)

The method of claim 1, wherein the nanocomposite has a crystalline melting temperature of 133.3-134.0° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein the nanocomposite has a % crystallinity of 63-73.