# US 2017/0283583 A1 · Polyacetal resin molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283583 A1
- Document ID: US20170283583A1
- Status: Published application
- Kind: A1
- Application number: 15/512,683
- Filed: 2014-10-16
- Published: 2017-10-05
- Earliest claimed: 2014-10-16
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Junichi TSUZUKI; Takaaki MIYOSHI
- Web page: https://patentgrep.com/patent/US20170283583A1

## CPC

- C08K 5/11: of acyclic polycarboxylic acids
- C08G 2/38: Block or graft polymers prepared by polymerisation of aldehydes or ketones on to macromolecular compounds
- C08K 3/22: of metals
- C08K 5/101: of monocarboxylic acids
- C08K 5/20: Carboxylic acid amides
- C08L 23/06: Polyethylene
- C08L 23/12: Polypropene
- C08L 59/04: Copolyoxymethylenes
- C08K 2003/2237: {of titanium}
- C08K 2003/2241: {Titanium dioxide}
- C08K 2003/2265: {of iron}
- C08K 2003/2296: {of zinc}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The resin molded article of the present invention comprises (B) 0.1 to 5 parts by mass of a sliding agent having a weight average molecular weight of 10,000 or less, and (C) 0.01 to 3 parts by mass of a coloring agent, based on (A) 100 parts by mass of a polyacetal resin, wherein a relative element concentration ratio between carbon and oxygen on a surface thereof [C/O] (atomic %) is 1.01 to 2.50.

## Claims

### Claim 1

A resin molded article comprising (B) 0.1 to 5 parts by mass of a sliding agent having a weight average molecular weight of 10,000 or less, and (C) 0.01 to 3 parts by mass of a coloring agent, based on (A) 100 parts by mass of a polyacetal resin, wherein
a relative element concentration ratio between carbon and oxygen on a surface thereof [C/O] (atomic %) is 1.01 to 2.50.

### Claim 2 (depends on 1)

The resin molded article according to claim 1, wherein a peak intensity ratio (C—O/C═O) between a C—O stretching vibration peak and a C═O stretching vibration peak on the surface thereof, which is obtained by infrared spectroscopy, is 10 to 200.

### Claim 3 (depends on 1)

The resin molded article according to claim 1, wherein (A) the polyacetal resin comprises a block copolymer.

### Claim 4 (depends on 3)

The resin molded article according to claim 3, wherein the block copolymer is an ABA-based block copolymer.

### Claim 5 (depends on 1)

The resin molded article according to claim 1, wherein (B) the sliding agent having the weight average molecular weight of 10,000 or less is at least one compound selected from the group consisting of alcohol, amine, carboxylic acid, an ester, an amide compound consisting of monovalent or divalent amine and carboxylic acid, and wax.

### Claim 6 (depends on 1)

The resin molded article according to claim 1, wherein a melting point of (B) the sliding agent having the weight average molecular weight of 10,000 or less is 40° C. to 150° C.

### Claim 7 (depends on 1)

The resin molded article according to claim 1, wherein an abundance of a particle having a major axis of 10 μm or more in (C) the coloring agent is 0.05 or less.

### Claim 8 (depends on 1)

The resin molded article according to claim 1, wherein (C) the coloring agent comprises at least one metal oxide selected from the group consisting of iron, zinc, and titanium.

### Claim 9 (depends on 1)

The resin molded article according to claim 1, comprising (D) 0.01 to 5 parts by mass of a polyolefin resin based on (A) 100 parts by mass of the polyacetal resin.

### Claim 10 (depends on 9)

The resin molded article according to claim 9, wherein (D) the polyolefin resin is at least one selected from the group consisting of (i) polyethylene, (ii) polypropylene, (iii) an ethylene-α-olefin copolymer, (iv) an ethylene-acrylic acid ester copolymer in which the content of the acrylic acid ester unit is 5% to 30% by mass, (v) a block polymer having a structure in which a block of polyolefin (d1) and a block of a hydrophilic polymer (d2) are repeatedly and alternatively bound to one another via at least one bond selected from the group consisting of an ester bond, an amide bond, an ether bond, a urethane bond, and an imide bond, and (vi) a modified product thereof.

### Claim 11 (depends on 1)

The resin molded article according to claim 1, wherein
(A) the polyacetal resin comprises a block copolymer,
(B) the sliding agent having the weight average molecular weight of 10,000 or less is at least one compound selected from the group consisting of alcohol, amine, carboxylic acid, an ester, an amide compound consisting of monovalent or divalent amine and carboxylic acid, and wax,
a melting point of (B) the sliding agent having the weight average molecular weight of 10,000 or less is 40° C. to 150° C.,
an abundance of a particle having a major axis of 10 μm or more in (C) the coloring agent is 0.05 or less, and
(C) the coloring agent comprises at least one metal oxide selected from the group consisting of iron, zinc, and titanium.