# US 2017/0283582 A1 · Thermoplastic Resin Composition Having Improved Weather Resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283582 A1
- Document ID: US20170283582A1
- Status: Published application
- Kind: A1
- Application number: 15/630,260
- Filed: 2017-06-22
- Published: 2017-10-05
- Earliest claimed: 2013-10-30
- Assignees: Lotte Advanced Materials Co., Ltd.
- Applicants: Lotte Advanced Materials Co., Ltd.
- Inventors: Ji Eun PARK; Kyun Ha BAN; Ja Yoon KIM; Chang Min HONG
- Web page: https://patentgrep.com/patent/US20170283582A1

## CPC

- C08L 25/12: with unsaturated nitriles
- C08K 3/22: of metals
- C08K 5/0041: {Optical brightening agents, organic pigments}
- C08L 25/16: Homopolymers or copolymers of alkyl-substituted styrenes
- C08L 51/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C08L51/04, C08L51/06 take precedence)}
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08L 51/04: grafted on to rubbers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/04: Thermoplastic elastomer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A thermoplastic resin composition having improved weather resistance includes an acrylic graft copolymer, an aromatic vinyl-vinyl cyanide copolymer, and a coloring agent including an inorganic pigment and an organic pigment mixed with each other at a predetermined ratio to maintain mechanical properties of the resin and have improved color mixing ability and weather resistance.

## Claims

### Claim 1

A thermoplastic resin composition for improving weather resistance comprising:
(A) an acrylic graft copolymer;
(B) an aromatic vinyl-vinyl cyanide copolymer; and
(C) a coloring agent including an inorganic pigment and an organic pigment,
wherein the inorganic pigment and the organic pigment are present in a weight ratio of inorganic pigment:organic pigment of about 1:1 to about 1:4.

### Claim 2 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, further comprising: (D) carbon black.

### Claim 3 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, wherein the inorganic pigment and the organic pigment are present in a weight ratio of inorganic pigment:organic pigment of about 1:1.1 to about 1:4.

### Claim 4 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, comprising the coloring agent (C) in an amount of about 0.1 to about 1 part by weight based on about 100 parts by weight of a base resin including about 30 to about 70 wt % of the acrylic graft copolymer (A) and about 70 to about 30 wt % of the aromatic vinyl-vinyl cyanide copolymer (B).

### Claim 5 (depends on 2)

The thermoplastic resin composition for improving weather resistance of claim 2, comprising the coloring agent (C) in an amount of about 0.1 to about 1 part by weight and the carbon black (D) in an amount of about 1 to about 5 parts by weight, based on about 100 parts by weight of a base resin including about 30 to about 70 wt % of the acrylic graft copolymer (A) and about 70 to about 30 wt % of the aromatic vinyl-vinyl cyanide copolymer (B).

### Claim 6 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, wherein the acrylic graft copolymer (A) is an acrylonitrile-styrene-acrylate graft copolymer (g-ASA) obtained by graft-polymerization of about 40 to about 60 wt % of an acrylic rubber-like polymer and about 40 to about 60 wt % of a mixture including an aromatic vinyl-based compound and a vinyl cyanide-based compound.

### Claim 7 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, wherein the aromatic vinyl-vinyl cyanide copolymer (B) comprises a styrene-acrylonitrile copolymer, an a-methyl styrene-acrylonitrile copolymer, a styrene-a-methyl styrene-acrylonitrile copolymer, or a combination thereof.

### Claim 8 (depends on 2)

The thermoplastic resin composition for improving weather resistance of claim 2, wherein the carbon black (D) has an average particle size of about 10 to about 50 nm, and a specific surface area of about 100 to about 300 m2/g.

### Claim 9 (depends on 5)

The thermoplastic resin composition for improving weather resistance of claim 5, wherein the carbon black (D) is a masterbatch including about 30 to about 70 wt % of the aromatic vinyl-vinyl cyanide copolymer and about 30 to about 70 wt % of the carbon black mixed with each other.

### Claim 10 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, wherein:
the inorganic pigment comprises an oxide including a metal element Fe, Cr, Mn, Cu, Co, or Ni, titanium oxide, zinc oxide, aluminum metal powder, copper metal powder, stainless steel powder, or a combination thereof, and
the organic pigment comprises anthraquinone pigment, perylene pigment, phthalocyanine pigment, azo pigment, indigo pigment, dioxazine pigment, quinacridone pigment, isoindolinone pigment, phthalone pigment, or a combination thereof.

### Claim 11 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, comprising the inorganic pigment and the organic pigment in a weight ratio represented by the following Equation 2, wherein in a molded article manufactured therefrom the following Equations 3 to 5 are simultaneously satisfied:
0.25≦PI/PO<1.0 [Equation 2]
wherein in Equation 2, PI is a content of the inorganic pigment (parts by weight), and PO is a content of the organic pigment (parts by weight),
dL=|La−Lb|≦1.5 [Equation 3]
da=|Aa−Ab|≦1.5 [Equation 4]
db=|Ba−Bb|≦2.0 [Equation 5]
wherein in Equation 3, La is an “L” value measured by a spectrophotometer after a weather resistance test and Lb is an “L” value measured by a spectrophotometer before a weather resistance test, in Equation 4, Aa is an “a” value measured by a spectrophotometer after a weather resistance test and Ab is an “a” value measured by a spectrophotometer before a weather resistance test, and in Equation 5, Ba is a “b” value measured by a spectrophotometer after a weather resistance test and Bb is a “b” value measured by a spectrophotometer before a weather resistance test.

### Claim 12 (depends on 1)

The thermoplastic resin composition for improving weather resistance of claim 1, wherein the coloring agent including the inorganic pigment and the organic pigment in a weight ratio inorganic pigment:organic pigment of about 1:3 to about 1:4.

### Claim 13 (depends on 4)

The thermoplastic resin composition for improving weather resistance of claim 4, wherein the inorganic pigment and the organic pigment both include a pigment in the same color family and wherein at least one of the inorganic pigment and the organic pigment further includes at least two different pigments in different color families.

### Claim 14 (depends on 13)

The thermoplastic resin composition for improving weather resistance of claim 13, wherein the inorganic pigment and the organic pigment both include a red pigment and wherein at least one of the inorganic pigment and the organic pigment further includes a yellow pigment.

### Claim 15 (depends on 14)

The thermoplastic resin composition for improving weather resistance of claim 14, further comprising (D) carbon black in an amount of about 1 to about 5 parts by weight, based on about 100 parts by weight of the base resin.

### Claim 16 (depends on 15)

The thermoplastic resin composition for improving weather resistance of claim 15, wherein in a molded article manufactured therefrom are simultaneously satisfies the following Equations 3 to 5
dL=|La−Lb|≦1.5 [Equation 3]
da=|Aa−Ab|≦1.5 [Equation 4]
db=|Ba−Bb|≦2.0 [Equation 5]
wherein in Equation 3, La is an “L” value measured by a spectrophotometer after a weather resistance test and Lb is an “L” value measured by a spectrophotometer before a weather resistance test, in Equation 4, Aa is an “a” value measured by a spectrophotometer after a weather resistance test and Ab is an “a” value measured by a spectrophotometer before a weather resistance test, and in Equation 5, Ba is a “b” value measured by a spectrophotometer after a weather resistance test and Bb is a “b” value measured by a spectrophotometer before a weather resistance test.

### Claim 17 (depends on 1)

A molded article manufactured from the thermoplastic resin composition for improving weather resistance according to claim 1.

### Claim 18 (depends on 2)

A molded article manufactured from the thermoplastic resin composition for improving weather resistance according to claim 2.

### Claim 19 (depends on 17)

The molded article of claim 17, comprising an inorganic pigment and an organic pigment in a weight ratio represented by the following Equation 2, wherein the following Equations 3 to 5 are simultaneously satisfied:
0.25≦PI/PO<1.0 [Equation 2]
wherein in Equation 2, PI is a content of the inorganic pigment (parts by weight), and PO is a content of the organic pigment (parts by weight),
dL=|La−Lb|≦1.5 [Equation 3]
da=|Aa−Ab|≦1.5 [Equation 4]
db=|Ba−Bb|≦2.0 [Equation 5]
wherein in Equation 3, La is an “L” value measured by a spectrophotometer after a weather resistance test and Lb is an “L” value measured by a spectrophotometer before a weather resistance test, in Equation 4, Aa is an “a” value measured by a spectrophotometer after a weather resistance test and Ab is an “a” value measured by a spectrophotometer before a weather resistance test, and in Equation 5, Ba is a “b” value measured by a spectrophotometer after a weather resistance test and Bb is a “b” value measured by a spectrophotometer before a weather resistance test.

### Claim 20 (depends on 17)

The molded article of claim 17, wherein the molded article has a “dE” value of less than about 3 measured in accordance with the following Equation 1:
dE=√{square root over ((dL)2+(da)2+(db)2)} [Equation 1]
wherein in Equation 1, dL is a variation of luminance, da is a variation of red green values, and db is a variation of yellow blue values, all of which are measured by a spectrophotometer.