# US 2017/0283577 A1 · Electrostatic dissipating mat

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283577 A1
- Document ID: US20170283577A1
- Status: Published application
- Kind: A1
- Application number: 15/472,682
- Filed: 2017-03-29
- Published: 2017-10-05
- Earliest claimed: 2016-04-01
- Assignees: Zeon Chemicals L.P.
- Applicants: Zeon Chemicals L.P.
- Inventors: Andrew MITTERMILLER; Clark CABLE; Zhiyi BAO
- Web page: https://patentgrep.com/patent/US20170283577A1

## CPC

- C08K 3/26: Carbonates; Bicarbonates
- B29B 7/02: non-continuous, with mechanical mixing or kneading devices, i.e. batch type
- B29C 35/02: Heating or curing, e.g. crosslinking or vulcanizing {during moulding, e.g. in a mould}(cold vulcanisation B29C35/18 {; vulcanising tyres, presses therefor B29D30/0601})
- B29C 43/003: {characterised by the choice of material}
- B29C 43/24: Calendering
- B29C 43/305: {Making multilayered articles}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/08: flexible, e.g. films
- B29C 48/21: the layers being joined at their surfaces
- C08G 65/14: Unsaturated oxiranes
- C08G 65/22: Cyclic ethers having at least one atom other than carbon and hydrogen outside the ring
- C08G 65/24: Epihalohydrins
- C08K 3/22: of metals
- C08K 3/34: Silicon-containing compounds
- C08K 3/36: Silica
- H05F 3/025: {Floors or floor coverings specially adapted for discharging static charges}
- B29K 2071/00: Use of polyethers {, e.g. PEEK, i.e. polyether-etherketone or PEK, i.e. polyetherketone or derivatives thereof}, as moulding material
- B29K 2105/16: Fillers
- B29L 2031/7324: {Mats}
- C08K 2003/2241: {Titanium dioxide}
- C08K 2003/2296: {of zinc}
- C08K 2003/265: {Calcium, strontium or barium carbonate}
- C08K 2201/001: Conductive additives
- C09K 3/16: Anti-static materials
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- H05F: STATIC ELECTRICITY; NATURALLY-OCCURRING ELECTRICITY
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

An electrostatic mat, wherein the mat comprises at least one electrostatic layer, wherein the at least one layer comprises an elastomeric rubber, wherein the elastomeric rubber comprises 20-100 phr elastomeric polyether, wherein the elastomeric polyether comprises 10-75 wt % ethylene oxide, 20-70 wt % epihalohydrin, and 0-10% vinyloxirane. The mat prevents the generation of voltage when it is walked on and/or dissipates the charge that was generated.

## Claims

### Claim 1

An electrostatic mat, wherein the mat comprises at least one electrostatic layer, wherein the at least one layer comprises an elastomeric rubber, wherein the elastomeric rubber comprises 20-100 phr elastomeric polyether, wherein the elastomeric polyether comprises 10-75 wt % ethylene oxide, 20-70 wt % epihalohydrin, and 0-10% vinyloxirane.

### Claim 2 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber has a Shore A hardness of about 50 to about 80.

### Claim 3 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber has an elongation of about 100% to about 1500%.

### Claim 4 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber has a volume resistance of about 10̂5 ohms to about 10̂9 ohms.

### Claim 5 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber has a tensile strength of about 500 to about 3000 psi.

### Claim 6 (depends on 1)

The mat of claim 1, wherein the electrostatic layer has a thickness from about 0.1 mm to about 5 cm.

### Claim 7 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber comprises fillers selected from NBR, EPDM, SBR, CR, PVC, PMMA, ABS, and combinations thereof.

### Claim 8 (depends on 1)

The mat of claim 1, wherein the elastomeric polyether comprises vinyloxirane.

### Claim 9 (depends on 8)

The mat of claim 8, wherein the vinyloxirane comprises allyl glycidyl ether.

### Claim 10 (depends on 1)

The mat of claim 1, wherein the epihalohydrin is epichlorohydrin.

### Claim 11 (depends on 9)

The mat of claim 9, wherein the epihalohydrin is epichlorohydrin.

### Claim 12 (depends on 1)

The mat of claim 1, wherein the elastomeric polyether comprises about 30 to about 75 wt % ethylene oxide, about 40 to about 60 wt % epihalohydrin, and about 4 to about 10 wt % allyl glycidyl ether.

### Claim 13 (depends on 1)

The mat of claim 1, wherein the system used to cure the elastomeric rubber is selected from sulfur and sulfur donor curatives.

### Claim 14 (depends on 1)

The mat of claim 1, wherein the elastomeric rubber has a walking body voltage generation of about 5 volts to about 500 volts as measured by ANSI/ESD 520.20 STM97.2.

### Claim 15

A method for producing an electrostatic mat comprises the steps of:
a) polymerizing 10-75 wt % ethylene oxide, 20-70 wt % epihalohydrin, and 0-10% vinyloxirane to form an elastomeric polyether,
b) mixing the elastomeric polyether with a curative to form an elastomeric compound,
c) forming the elastomeric compound into a sheet, and
d) vulcanizing the elastomeric compound to form an elastomeric rubber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the mat comprises more than one layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the steps additionally comprise the step of:
d) molding, extruding, or calendaring the elastomeric rubber with at least one additional layer.

### Claim 18 (depends on 15)

The method of claim 15, wherein fillers are added to the elastomeric polyether before curing.

### Claim 19 (depends on 15)

The method of claim 15, wherein the elastomeric polyether comprises vinyloxirane and the vinyloxirane comprises allyl glycidyl ether.

### Claim 20 (depends on 15)

The mat of claim 15, wherein the epihalohydrin is epichlorohydrin.