# US 2017/0283555 A1 · Amide elastomer foam particles, method for producing same, foam molded body and method for producing foam molded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283555 A1
- Document ID: US20170283555A1
- Status: Published application
- Kind: A1
- Application number: 15/507,915
- Filed: 2015-09-28
- Published: 2017-10-05
- Earliest claimed: 2014-09-30
- Assignees: Sekisui Plastics Co., Ltd.
- Applicants: Sekisui Plastics Co., Ltd.
- Inventors: Masayuki TAKANO; Yuta FUKUZAKI; Ryo AKUTA
- Web page: https://patentgrep.com/patent/US20170283555A1

## CPC

- C08G 69/08: derived from amino-carboxylic acids
- C08J 9/18: by impregnating polymer particles with the blowing agent
- B29C 44/00: Shaping by internal pressure generated in the material, e.g. swelling or foaming {; Producing porous or cellular expanded plastics articles}
- C08J 9/0028: {containing nitrogen}
- C08J 9/16: Making expandable particles
- C08J 9/232: by sintering expandable particles
- G01N 25/20: by investigating the development of heat, i.e. calorimetry, e.g. by measuring specific heat, by measuring thermal conductivity (calorimeters per se G01K)
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- C08J 2201/034: Post-expanding of foam beads or sheets
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2205/044: Micropores, i.e. average diameter being between 0,1 micrometer and 0,1 millimeter
- C08J 2300/26: Elastomers
- C08J 2371/02: Polyalkylene oxides
- C08J 2377/00: Characterised by the use of polyamides obtained by reactions forming a carboxylic amide link in the main chain; Derivatives of such polymers
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Amide-based elastomer expanded particles comprising, as a base resin, a non-crosslinked amide-based elastomer having a Shore D hardness of 65 or less, and having an average cell diameter of 20 to 250 μm.

## Claims

### Claim 1

Amide-based elastomer expanded particles comprising, as a base resin, a non-crosslinked amide-based elastomer having a Shore D hardness of 85 or less, and having an average cell diameter of 20 to 250 μm.

### Claim 2 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, comprising, as a base resin, a non-crosslinked amide-based elastomer having a Shore D hardness of 65 or less, and having a bulk density of 0.015 to 0.5 g/cm3 and an average cell diameter of 20 to 250 μm.

### Claim 3 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, wherein said non-crosslinked amide-based elastomer is an elastomer having both of a storage modulus at a temperature of crystallization temperature −10° C. and a storage modulus at a temperature of crystallization temperature −15° C. in a range of 4×106 to 4×107 Pa.

### Claim 4 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, wherein said non-crosslinked amide-based elastomer is an elastomer having an absolute value of α of 0.08 or more when expressed by equation y=αx+β, obtained from a storage modulus measured at a crystallization temperature and a storage modulus corresponding to a temperature which is 5° C. lower than a crystallization temperature, in a graph obtained by expressing a logarithm of a storage modulus on a y axis and a temperature on an x axis.

### Claim 5 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, wherein said amide-based elastomer expanded particles have an average particle diameter of more than 5 mm and 15 mm or less.

### Claim 6 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, comprising, as a base resin, said non-crosslinked amide-based elastomer, and having an average cell diameter of 20 to 250 μm and an average particle diameter of 1.5 to 5 mm.

### Claim 7 (depends on 1)

The amide-based elastomer expanded particles according to claim 1, wherein said amide-based elastomer expanded particles have an outermost surface layer exhibiting an average cell diameter of 20 to 150 μm in a cross section thereof.

### Claim 8 (depends on 1)

A method for manufacturing amide-based elastomer expanded particles according to claim 1, the method comprising the steps of:
impregnating a blowing agent into resin particles comprising a non-crosslinked amide-based elastomer to obtain expandable particles; and
expanding said expandable particles.

### Claim 9 (depends on 8)

The method for manufacturing amide-based elastomer expanded particles according to claim 8, wherein said resin particles comprise 100 parts by mass of a non-crosslinked amide-based elastomer and 0.02 to 1 part by mass of a cell adjusting agent.

### Claim 10 (depends on 9)

The method for manufacturing amide-based elastomer expanded particles according to claim 9, wherein said cell adjusting agent is a fatty acid amide-based organic substance.

### Claim 11 (depends on 8)

The method for manufacturing amide-based elastomer expanded particles according to claim 8, wherein said expandable particles are obtained by impregnating said blowing agent into said resin particles in the presence of water, and said water is used at 0.5 to 4 parts by weight based on 100 parts by weight of said resin particles.

### Claim 12 (depends on 1)

An expanded molded article which is obtained by in-mold expanding the amide-based elastomer expanded particles according to claim 1.

### Claim 13 (depends on 12)

The expanded molded article according to claim 12, wherein said expanded molded article has a compression set of 10% or less and a restitution coefficient of 50 or more.

### Claim 14 (depends on 1)

A method for manufacturing an expanded molded article, the method comprising in-mold expanding the amide-based elastomer expanded particles according to claim 1.

### Claim 15 (depends on 14)

The method for manufacturing an expanded molded article according to claim 14, wherein said in-mold expansion is performed using said amide-based elastomer expanded particles exhibiting a secondary expansion ratio of 1.5 to 4.0 times when heated with water steam at a gauge pressure of 0.27 MPa for 20 seconds.