# US 2017/0283523 A1 · Method for producing fluorinated polymer particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283523 A1
- Document ID: US20170283523A1
- Status: Published application
- Kind: A1
- Application number: 15/628,672
- Filed: 2017-06-21
- Published: 2017-10-05
- Earliest claimed: 2014-12-25
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Susumu SAITO; Wakako HASHIMOTO; Tetsuji SHIMOHIRA; Kazuo HAMAZAKl; Satoshi OTSUGU; Hiroki MATOBA
- Web page: https://patentgrep.com/patent/US20170283523A1

## CPC

- C08F 6/12: Separation of polymers from solutions
- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- C08F 2/06: Organic solvent
- C08F 6/003: {from polymer solutions, suspensions, dispersions or emulsions without recovery of the polymer therefrom}
- C08F 6/16: Purification
- C08F 6/18: Increasing the size of the dispersed particles
- C08J 3/16: by coagulating dispersions {(C08J3/122 takes precedence)}
- C08L 27/12: containing fluorine atoms
- C08J 2327/12: containing fluorine atoms
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

To provide a method capable of producing fluorinated polymer particles in which formation of fine particles or formation of large aggregates is sufficiently suppressed even in the case of a fluorinated polymer having high solubility in a solvent. The method comprises the following steps (i) and (ii), being a method for producing particles of a fluorinated polymer (A) which has either one or both of structural units (u1) derived from tetrafluoroethylene and structural units (u2) having no sulfonic acid type functional group and having a cyclic structure and fluorine atoms, and which has structural units (u3) having a sulfonic acid type functional group, wherein the proportion of the structural units (u1) is from 0 to 82 mol % in all structural units (100 mol %) in the fluorinated polymer (A): (i) a step of preparing solution or dispersion of the fluorinated polymer (A) having the above fluorinated polymer (A) dissolved or dispersed in a solvent (B), wherein the following conditions (i-1) and (i-2) are satisfied: (i-1) the solvent (B) contains a good solvent (B2) wherein the solubility of the fluorinated polymer (A) is at least 30%, (i-2) even when the above solution or dispersion of the fluorinated polymer (A) is passed through a filter of 200 mesh made of stainless steel, no residue remains on the filter, (ii) a step of mixing the above solution or dispersion of the fluorinated polymer (A) and a solvent (C) to aggregate the fluorinated polymer (A) to form particles of the fluorinated polymer (A), wherein the following conditions (ii-1) to (ii-3) are satisfied: (ii-1) the solvent (C) contains a poor solvent (C1) whereby the degree of swelling of the fluorinated polymer (A) is at most 100%, (ii-2) the degree of swelling of the fluorinated polymer (A) by a mixed solvent (BC) of the solvent (B) and the solvent (C) is from 70 to 250%, (ii-3) the ratio of the mass (WC) of the solvent (C) to the mass (WB) of the solvent (B) is from 1 to 5.

## Claims

### Claim 1

A method for producing fluorinated polymer particles comprising the following steps (i) and (ii), being a method for producing particles of a fluorinated polymer (A) which has either one or both of structural units (u1) derived from tetrafluoroethylene and structural units (u2) having no sulfonic acid type functional group and having a cyclic structure and fluorine atoms, and which has structural units (u3) having a sulfonic acid type functional group, wherein the proportion of the structural units (u1) is from 0 to 82 mol % in all structural units (100 mol %) in the fluorinated polymer (A):
(i) a step of preparing solution or dispersion of the fluorinated polymer (A) having the above fluorinated polymer (A) dissolved or dispersed in a solvent (B), wherein the following conditions (i-1) and (i-2) are satisfied:
(i-1) the solvent (B) contains a good solvent (B2) wherein the solubility of the fluorinated polymer (A) is at least 30%, and
(i-2) even when the above solution or dispersion of the fluorinated polymer (A) is passed through a filter of 200 mesh made of stainless steel, no residue remains on the filter,
(ii) a step of mixing the above solution or dispersion of the fluorinated polymer (A) and a solvent (C) to aggregate the fluorinated polymer (A) to form particles of the fluorinated polymer (A), wherein the following conditions (ii-1) to (ii-3) are satisfied:
(ii-1) the solvent (C) contains a poor solvent (C1) whereby the degree of swelling of the fluorinated polymer (A) is at most 100%, and
(ii-2) the degree of swelling of the fluorinated polymer (A) by a mixed solvent (BC) of the solvent (B) and the solvent (C) is from 70 to 250%,
(ii-3) the ratio (WC/WB) of the mass (WC) of the solvent (C) to the mass (WB) of the solvent (B) is from 1 to 5.

### Claim 2 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC) is from 80 to 250%.

### Claim 3 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC) is from 105 to 250%.

### Claim 4 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the good solvent (B2) is a hydrofluorocarbon.

### Claim 5 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the good solvent (B2) is either one or both of C6F13H and CF3CFHCFHCF2CF3.

### Claim 6 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the poor solvent (C1) is at least one member selected from hydrofluoroethers, hydrofluorocarbons, non-fluorinated alcohols, hydrocarbons and fluorinated alcohols.

### Claim 7 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the poor solvent (C1) is at least one member selected from CF3CH2OCF2CF2H, CHF2CH2CF3, CF3CH2CF2CH3, methanol, hexane, CF3CF2CH2OH, CF3CH2OH and H(CF2)4CH2OH.

### Claim 8 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the poor solvent (C1) is at least two members selected from hydrofluoroethers, hydrofluorocarbons, non-fluorinated alcohols, hydrocarbons and fluorinated alcohols.

### Claim 9 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC), is adjusted by the mixing ratio of at least two members of the poor solvent (C1).

### Claim 10 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC), is adjusted by the temperature of the solvent (C) immediately before mixing it with the solution or dispersion of the fluorinated polymer (A) in the step (ii).

### Claim 11 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the temperature of the solvent (C) immediately before mixing it with the solution or dispersion of the fluorinated polymer (A) in the step (ii) is within a range of from −15 to 30° C.

### Claim 12 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein in all structural units (100 mol %) in the fluorinated polymer (A), the proportion of the structural units (u1) is from 35 to 82 mol %, the proportion of the structural units (u2) is at least 0 mol % and less than 30 mol %, and the proportion of the structural units (u3) is from 18 to 35 mol %.

### Claim 13 (depends on 12)

The method for producing fluorinated polymer particles according to claim 12, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC) is from 70 to 200%.

### Claim 14 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein in all structural units (100 mol %) in the fluorinated polymer (A), the proportion of the structural units (u1) is from 0 to 60 mol %, the proportion of the structural units (u2) is from 20 to 85 mol %, and the proportion of the structural units (u3) is from 10 to 35 mol %.

### Claim 15 (depends on 14)

The method for producing fluorinated polymer particles according to claim 14, wherein the degree of swelling of the fluorinated polymer (A) by the solvent (BC) is from 105 to 250%.

### Claim 16 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein following the steps (i) and (ii), the fluorinated polymer (A) is separated and recovered.

### Claim 17 (depends on 1)

The method for producing fluorinated polymer particles according to claim 1, wherein the ion-exchange capacity of a polymer having the sulfonic acid type functional groups of the fluorinated polymer (A) converted to ion exchange groups, is from 0.9 to 2.5 meq/g dry resin.