# US 2017/0283325 A1 · Super-smooth glaze and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283325 A1
- Document ID: US20170283325A1
- Status: Published application
- Kind: A1
- Application number: 14/900,281
- Filed: 2015-11-17
- Published: 2017-10-05
- Earliest claimed: 2014-12-09
- Assignees: Da-Han International Holding Limited
- Applicants: Da-Han International Holding Limited
- Inventors: ZHAOYANG HUANG
- Web page: https://patentgrep.com/patent/US20170283325A1

## CPC

- C04B 33/04: Clay; Kaolin
- C04B 35/14: based on silica
- C04B 41/009: {characterised by the material treated}
- C04B 41/5022: {with vitreous materials (composition of vitreous glazes and enamels C03C; ceramic pigments C09C1/0009)}
- C04B 41/86: Glazes; Cold glazes
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The present invention relates to a super-smooth glaze and a preparation method thereof, and belongs to the field of ceramic machining, wherein each component in parts by weight is: potassium feldspar, quartz, kaolin, calcite, dolomite, boric acid, aluminum oxide, silicon oxide, calcium oxide, potassium oxide, sodium oxide, zinc oxide, and barium oxide; a mixture weighed in proportion is disposed in a planetary quick ball mill, and pure water of 30˜40 wt % to the total weight of the mixture is added to ball-mill the mixture to particle sizes of 0.5˜1.0 μm, thus obtaining the super-smooth glaze. The method enables the surface of a glaze layer to be highly smooth and makes the roughness of the glaze be relatively reduced than that of an ordinary ceramic glaze.

## Claims

### Claim 1

A super-smooth glaze, comprising the following components in parts by weight:
18˜68 parts of potassium feldspar, 20˜98 parts of quartz, 10˜50 parts of kaolin, 20˜50 parts of calcite, 5˜40 parts of dolomite, 5˜40 parts of boric acid, 9˜17 parts of aluminum oxide, 5˜15 parts of silicon oxide, 1˜5 parts of calcium oxide, 5˜10 parts of potassium oxide, 5˜10 parts of sodium oxide, 5˜17 parts of zinc oxide, and 1˜5 parts of barium oxide.

### Claim 2 (depends on 1)

The super-smooth glaze according to claim 1, comprising the following components in parts by weight:
18˜38 parts of potassium feldspar, 20˜68 parts of quartz, 10˜30 parts of kaolin, 20˜40 parts of calcite, 5˜30 parts of dolomite, 5˜30 parts of boric acid, 9˜12 parts of aluminum oxide, 5˜12 parts of silicon oxide, 1˜3 parts of calcium oxide, 5˜8 parts of potassium oxide, 5˜8 parts of sodium oxide, 5˜12 parts of zinc oxide, and 1˜3 parts of barium oxide.

### Claim 3 (depends on 1)

The super-smooth glaze according to claim 1, comprising the following components in parts by weight:
28˜68 parts of potassium feldspar, 40˜98 parts of quartz, high 20˜50 parts of kaolin, 30˜50 parts of calcite, 15˜40 parts of dolomite, 15˜40 parts of boric acid, 10˜17 parts of aluminum oxide, 7˜15 parts of silicon oxide, 2˜5 parts of calcium oxide, 6˜10 parts of potassium oxide, 6˜10 parts of sodium oxide, 7˜17 parts of zinc oxide, and 2˜5 parts of barium oxide.

### Claim 4 (depends on 1)

The super-smooth glaze according to claim 1, comprising the following components in parts by weight:
20˜60 parts of potassium feldspar, 25˜90 parts of quartz, 15˜45 parts of kaolin, 25˜45 parts of calcite, 10˜35 parts of dolomite, 10˜35 parts of boric acid, 10˜15 parts of aluminum oxide, 8˜12 parts of silicon oxide, 2˜4 parts of calcium oxide, 7˜9 parts of potassium oxide, 7˜9 parts of sodium oxide, 8˜15 parts of zinc oxide, and 2˜4 parts of barium oxide.

### Claim 5 (depends on 4)

The super-smooth glaze according to claim 4, comprising the following components in parts by weight:
30˜60 parts of potassium feldspar, 30˜80 parts of quartz, 25˜35 parts of kaolin, 35˜50 parts of calcite, 20˜35 parts of dolomite, 20˜35 parts of boric acid, 12˜15 parts of aluminum oxide, 7˜10 parts of silicon oxide, 3˜4 parts of calcium oxide, 6˜9 parts of potassium oxide, 6˜9 parts of sodium oxide, 9˜12 parts of zinc oxide, and 3˜4 parts of barium oxide.

### Claim 6 (depends on 4)

The super-smooth glaze according to claim 4, comprising the following components in parts by weight:
38 parts of potassium feldspar, 75 parts of quartz, 45 parts of kaolin, 35 parts of calcite, 15 parts of dolomite, 30 parts of boric acid, 12 parts of aluminum oxide, 8 parts of silicon oxide, 2 parts of calcium oxide, 7 parts of potassium oxide, 8 parts of sodium oxide, 10 parts of zinc oxide, and 2 parts of barium oxide.

### Claim 7 (depends on 1)

The super-smooth glaze according to claim 1, comprising the following components in parts by weight:
55 parts of potassium feldspar, 35 parts of quartz, 30 parts of kaolin, 45 parts of calcite, 35 parts of dolomite, 15 parts of boric acid, 16 parts of aluminum oxide, 12 parts of silicon oxide, 4 parts of calcium oxide, 8 parts of potassium oxide, 6 parts of sodium oxide, 15 parts of zinc oxide, and 4 parts of barium oxide.

### Claim 8

A preparation method of super-smooth glaze, comprising the following steps of:
disposing a mixture weighed in proportion in a planetary quick ball mill, and adding water of 30˜40 wt % to the total weight of the mixture.