# US 2017/0283319 A1 · Structural lightweight concrete with superior thermal insulation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283319 A1
- Document ID: US20170283319A1
- Status: Published application
- Kind: A1
- Application number: 15/084,653
- Filed: 2016-03-30
- Published: 2017-10-05
- Earliest claimed: 2016-03-30
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Mohammed Maslehuddin; Salah U. Al-Dulaijan; Mohammed Rizwan Ali
- Web page: https://patentgrep.com/patent/US20170283319A1

## CPC

- C04B 28/04: Portland cements
- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- C04B 28/065: {Calcium aluminosulfate cements, e.g. cements hydrating into ettringite}
- C04B 28/08: Slag cements
- C04B 28/10: Lime cements or magnesium oxide cements
- C04B 2111/28: Fire resistance, i.e. materials resistant to accidental fires or high temperatures
- C04B 2111/40: Porous or lightweight materials
- C04B 2201/32: for the thermal conductivity, e.g. K-factors
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A structural lightweight concrete composition comprising cement, a fine aggregate such as sand, a natural coarse aggregates, such as limestone, scoria or perlite or mixtures thereof, a synthetic coarse aggregate comprising a polymeric material, such as polypropylene beads, an industrial waste byproduct in the form of fine particles, such as silica fume or heavy oil ash, a superplasticizer, such as a polycarboxylate ether and water demonstrating lower thermal conductivity and sufficient compressive strength. Concrete products made therefrom and methods for producing such products are also provided.

## Claims

### Claim at position 1

1: A structural lightweight concrete composition, comprising:
cement;
a fine aggregate;
a natural coarse aggregate;
a synthetic coarse aggregate comprising a polymeric material;
an industrial waste byproduct in the form of fine particles;
a superplasticizer; and
water
wherein the average particle size of the fine aggregate and the industrial waste byproduct is less than or equal to 1 mm and the average particle size of the synthetic coarse aggregate and the natural coarse aggregate is greater than 1 mm; and
wherein the weight ratio of water to cement is in the range of 0.33 to 0.8 and is sufficient to affect hydraulic setting of the cement.

### Claim at position 2 (depends on 1)

2: The structural lightweight concrete composition of claim 1, wherein the synthetic coarse aggregate comprising a polymeric material is spherical polypropylene beads with an average particle size of 2-15 mm.

### Claim at position 3 (depends on 1)

3: The structural lightweight concrete composition of claim 1, which has a weight percentage of the synthetic coarse aggregate comprising a polymeric material ranging from 2-15% relative to the total weight of the composition.

### Claim at position 4 (depends on 1)

4: The structural lightweight concrete composition of claim 1, wherein the cement is present in the composition at 300-500 kg/m3.

### Claim at position 5 (depends on 1)

5: The structural lightweight concrete composition of claim 1, which has a weight percentage of cement ranging from 20-30% relative to the total weight of the composition.

### Claim at position 6 (depends on 1)

6: The structural lightweight concrete composition of claim 1, wherein the fine aggregate is sand with an average particle size of less than 700 μm.

### Claim at position 7 (depends on 1)

7: The structural lightweight concrete composition of claim 1, which has a weight percentage of the fine aggregate ranging from 15-30% relative to the total weight of the composition.

### Claim at position 8 (depends on 1)

8: The structural lightweight concrete composition of claim 1, wherein the natural coarse aggregate is at least one selected from the group consisting of limestone, perlite, and scoria.

### Claim at position 9 (depends on 1)

9: The structural lightweight concrete composition of claim 1, which has a weight percentage of the natural coarse aggregate ranging from 20-45% relative to the total weight of the composition.

### Claim at position 10 (depends on 1)

10: The structural lightweight concrete composition of claim 1, wherein the natural coarse aggregate comprises crushed limestone having an average particle size in the range of 1-20 mm.

### Claim at position 11 (depends on 1)

11: The structural lightweight concrete composition of claim 1, wherein the industrial waste byproduct is at least one selected from the group consisting of silica fume and heavy oil ash.

### Claim at position 12 (depends on 1)

12: The structural lightweight concrete composition of claim 1, which has a weight percentage of the industrial waste byproduct in the form of fine particles ranging from 0.5-10% relative to the total weight of the composition.

### Claim at position 13 (depends on 1)

13: The structural lightweight concrete composition of claim 1, wherein the superplasticizer is a polycarboxylate ether.

### Claim at position 14 (depends on 1)

14: The structural lightweight concrete composition of claim 1, which has a weight percentage of the superplasticizer ranging from 0.1-2.0% relative to the total weight of the composition.

### Claim at position 15 (depends on 1)

15: The structural lightweight concrete composition of claim 1, which has a weight percentage of water ranging from 10-20% relative to the total weight of the composition.

### Claim at position 16 (depends on 1)

16: The structural lightweight concrete composition of claim 1, which has a 28-day unit weight in the range of 1600-1900 kg/m3 after setting.

### Claim at position 17 (depends on 1)

17: The structural lightweight concrete composition of claim 1, which has a compressive strength in the range of 20-40 MPa after setting.

### Claim at position 18 (depends on 1)

18: The structural lightweight concrete composition of claim 1, which has a thermal conductivity in the range of 0.3-0.7 W/(m·K) after setting.

### Claim at position 19 (depends on 1)

19: A method for producing a cast concrete product comprising the structural lightweight concrete composition of claim 1, the method comprising:
mixing the cement, the fine aggregate, the natural coarse aggregate, the synthetic coarse aggregate and the industrial waste byproduct in the form of fine particles to form a solid cement mixture;
adding water and a superplasticizer to the cement mixture to affect hydraulic setting while maintaining a slump in the range of 50-100 mm to form a fluid concrete mixture;
casting the concrete mixture in a predetermined shape by placing the fluid concrete mixture in a mold to produce a cast concrete product after setting.

### Claim at position 20 (depends on 1)

20: A cast concrete product comprising the structural lightweight concrete composition of claim 1.