# US 2017/0283317 A1 · Phosphorous containing glass having antimicrobial efficacy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283317 A1
- Document ID: US20170283317A1
- Status: Published application
- Kind: A1
- Application number: 15/626,677
- Filed: 2017-06-19
- Published: 2017-10-05
- Earliest claimed: 2013-11-26
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Dana Craig Bookbinder; Nicholas Francis Borrelli; Matthew John Dejneka; Timothy Michael Gross
- Web page: https://patentgrep.com/patent/US20170283317A1

## CPC

- C03C 21/005: {to introduce in the glass such metals or metallic ions as Ag, Cu}
- A01N 59/00: Biocides, pest repellants or attractants, or plant growth regulators containing elements or inorganic compounds
- A01N 59/16: Heavy metals; Compounds thereof
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/00: Compositions for glass with special properties
- C03C 17/30: with silicon-containing compounds
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/02: Antibacterial glass, glaze or enamel
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- Y10T 428/31612: As silicone, silane or siloxane
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A strengthened antimicrobial glass including greater from about 50.0 mol. % to about 65.0 mol. % SiO2, about 14.0 mol. % to about 22.0 mol. % Al203, about 14.0 mol. % to about 22.0 mol. % R2O, wherein R is an alkali metal, and about 4.0 mol. % to 10.0 mol. % P2O5. The glass may have a compressive stress layer having a thickness of greater than or equal to about 20 μm less than or equal to about 60 μm and having a compressive stress of greater than or equal to about 700 MPa. The glass may have an antimicrobial activity greater than or equal to about 1.0 log kill at about 23 ° C. and about 40.0% relative humidity. A method for making the glass may include obtaining a glass article, strengthening the glass article by contact with a first ion-exchange liquid, and contacting the glass article with second ion-exchange liquid comprising an antimicrobial agent.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

A strengthened antimicrobial glass comprising:
SiO2;
Al2O3;
R2O, wherein R is an alkali metal; and
P2O5, wherein:
the glass comprises a compressive stress layer having a thickness of greater than or equal to about 20 μmand having a surface compressive stress; and
the glass has an antimicrobial activity greater than or equal to about 1.0 Log Kill at about 23° C. and about 40.0% relative humidity.

### Claim 22 (depends on 21)

The glass of claim 21, wherein the surface compressive stress is greater than or equal to about 700 MPa.

### Claim 23 (depends on 21)

The glass of claim 21, wherein the glass further comprises Ag.

### Claim 24 (depends on 23)

The glass of claim 23, wherein the glass has a maximum concentration of Ag within 60 nm of a free surface of the glass.

### Claim 25 (depends on 23)

The glass of claim 23, wherein an average concentration of Ag within 60 nm of a free surface of the glass is greater than or equal to about 10 mol. % to less than or equal to about 15 mol. %.

### Claim 26 (depends on 23)

The glass of claim 23, wherein the glass has a light transmission of greater than or equal to about 85% over wavelengths from greater than or equal to about 400 nm to less than or equal to about 750 nm.

### Claim 27 (depends on 21)

The glass of claim 21, wherein the glass has a molar ratio of Al2O3 to R2O that is greater than or equal to about 0.5:1 to less than or equal to about 1.5:1.

### Claim 28 (depends on 21)

The glass of claim 21, wherein the glass further comprises greater than 0.0 mol. % to less than or equal to about 4.0 mol. % ZnO.

### Claim 29 (depends on 21)

The glass of claim 21, wherein the glass has an antimicrobial activity greater than or equal to about 5.0 Log Kill at about 37° C. and a relative humidity greater than or equal to about 90%.

### Claim 30 (depends on 21)

The glass of claim 21, wherein R is selected from the group consisting of Li, Na, and K.

### Claim 31 (depends on 21)

The glass of claim 21, wherein the compressive stress layer has a depth of greater than or equal to about 40 μm to less than or equal to about 50 μm.

### Claim 32 (depends on 21)

The glass of claim 21, wherein the glass has a compressive stress of greater than or equal to about 900 MPa.

### Claim 33 (depends on 21)

The glass of claim 21, further comprising greater than 0.0 mol. % to less than or equal to about 4.0 mol. % alkaline earth metal.

### Claim 34 (depends on 21)

The glass of claim 21, further comprising a fluorosilane coating on a free surface of the glass.

### Claim 35 (depends on 34)

The glass of claim 34, wherein the coating has a general formula of:
Ax-Si—B4-x, where
A is selected from the group consisting of perfluoroalkyl, perfluoroalkyl terminated perfluoropolyether, perfluoroalkyl-alkyl, copolymers of fluoroalkene silanes and alkene silanes, and mixtures of fluoroalkylsilanes and hydrophilic silanes; and
B is selected from the group consisting of Cl, acetoxy, and alkoxy; and
x=1 or 2.

### Claim 36 (depends on 21)

The glass of claim 21, wherein the glass comprises greater than or equal to about 50.0 mol. % to less than or equal to about 65.0 mol. % SiO2.

### Claim 37 (depends on 21)

The glass of claim 21, wherein the glass comprises greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % Al2O3.

### Claim 38 (depends on 21)

The glass of claim 21, wherein the glass comprises greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % R2O.

### Claim 39 (depends on 21)

The glass of claim 21, wherein the glass comprises greater than or equal to about 4.0 mol. % to less or equal to about 10.0 mol. % P2O5.

### Claim 40

A method for making strengthened antimicrobial glass, the method comprising:
obtaining a glass article comprising:
SiO2,
Al2O3,
R2O, wherein R is an alkali metal, and
P2O5;
strengthening the glass article by contact with a first ion-exchange liquid; and
contacting the glass article with a second ion-exchange liquid comprising an antimicrobial agent, wherein:
the glass comprises a compressive stress layer having a thickness of greater than or equal to about 20 μm and having a surface compressive stress; and
the glass has an antimicrobial activity greater than or equal to about 1.0 log kill at about 23° C. and a relative humidity of about 40%.

### Claim 41 (depends on 40)

The method of claim 40, wherein the surface compressive stress is greater than or equal to about 700 MPa.

### Claim 42 (depends on 40)

The method of claim 40, wherein the compressive stress layer has a thickness of less than or equal to about 60 μm.

### Claim 43 (depends on 40)

The method of claim 40, wherein the first ion-exchange liquid is selected from the group consisting of NaNO3, KNO3, and mixtures thereof.

### Claim 44 (depends on 40)

The method of claim 40, wherein the antimicrobial agent comprises Ag.

### Claim 45 (depends on 44)

The method of claim 44, wherein the second ion-exchange liquid further comprises a member selected from the group consisting of NaNO3, KNO3, and mixtures thereof.

### Claim 46 (depends on 44)

The method of claim 44, wherein a silver salt concentration in the second ion-exchange liquid is greater than or equal to about 5.0 mol. %.

### Claim 47 (depends on 40)

The method of claim 40, wherein the strengthening step comprises holding the glass article in a bath of the first ion-exchange liquid that has a temperature of greater than or equal to about 300° C. to less than or equal to about 500° C. for a duration of greater than or equal to about 40 minutes to less than or equal to about 6 hours.

### Claim 48 (depends on 40)

The method of claim 40, wherein the glass comprises greater than or equal to about 50.0 mol. % to less than or equal to about 65.0 mol. % SiO2.

### Claim 49 (depends on 40)

The method of claim 40, wherein the glass comprises greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % Al2O3.

### Claim 50 (depends on 40)

The method of claim 40, wherein the glass comprises greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % R2O.

### Claim 51 (depends on 40)

The method of claim 40, wherein the glass comprises greater than or equal to about 4.0 mol. % to less or equal to about 10.0 mol. % P2O5.