# US 2017/0283312 A1 · Low temperature fluoride glasses and glazes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283312 A1
- Document ID: US20170283312A1
- Status: Published application
- Kind: A1
- Application number: 15/418,611
- Filed: 2017-01-27
- Published: 2017-10-05
- Earliest claimed: 2016-03-29
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Chengtsin Lee; Jennifer Y. Sun
- Web page: https://patentgrep.com/patent/US20170283312A1

## CPC

- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- C03C 4/18: for ion-sensitive glass
- C03C 8/06: containing halogen
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- C03C 10/16: Halogen containing crystalline phase
- C03C 17/245: by deposition from the vapour phase
- C03C 21/007: {in gaseous phase}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2209/00: Compositions specially applicable for the manufacture of vitreous glazes
- C03C 2217/214: Al2O3
- C03C 2217/285: Fluorides
- C03C 2218/13: from melts
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

An article comprises a body having a coating. The coating comprising a eutectic system having a super-lattice of a first fluoride and a second fluoride. The coating includes a glaze on a surface of the coating, the glaze comprising the eutectic system having the super-lattice of the first fluoride and the second fluoride.

## Claims

### Claim 1

A method comprising:
mixing a first fluoride having a first melting temperature with a second fluoride having a second melting temperature that is lower than the first melting temperature to form a mixture comprising the first fluoride and the second fluoride;
melting the first fluoride and the second fluoride by heating the mixture of the first fluoride and the second fluoride to a first temperature above at least the second melting temperature;
cooling the mixture to form a material comprising a eutectic system having a super-lattice of the first fluoride and the second fluoride, wherein the eutectic system has a third melting temperature that is below the first melting temperature and the second melting temperature;
grinding the material comprising the eutectic system into a powder;
forming an article or a coating using the powder; and
heating the article or the coating to a second temperature that is below the first melting temperature, below the second melting temperature and above the third melting temperature to cause at least a portion of the article or the coating to transform into at least one of a glaze or a glass ceramic comprising the eutectic system.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the article using the powder comprises:
forming a slurry from the powder; and
casting the slurry into a shape in a mold, wherein the article is heated to transform a surface of the article into the glaze comprising the eutectic system.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming the article using the powder comprises:
melting the powder into a molten mixture of the first fluoride and the second fluoride; and
casting the molten mixture into a shape in a mold.

### Claim 4 (depends on 1)

The method of claim 1, wherein forming the coating using the powder comprises:
forming a slurry from the powder; and
performing one of dip coating, spin casting, drop casting, spray coating, or doctor blade coating to apply the slurry to an object, wherein the coating is heated to transform at least the portion of the coating into the glaze comprising the eutectic system.

### Claim 5 (depends on 1)

The method of claim 1, wherein:
the coating has a first thickness of 1 micron to 200 microns; and
the glaze has a second thickness that is 50% to 100% of the first thickness of the coating.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first fluoride is ZrF4 and the second fluoride is selected from a group consisting of CaF2, MgF2, SrF2, AlF3, ErF3, LaF3, NdF3, ScF3, CeF4, HfF4, TiF3, and YF3.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first fluoride is ZrF4, the second fluoride is LaF3, the mixture comprises approximately 23-37 mole % ZrF4 and approximately 63-77 mole % LaF3, the first melting temperature is 910° C., the second melting temperature is 1490° C., and the third melting temperature is about 770° C.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
mixing a third fluoride having a fourth melting temperature with the first fluoride and the second fluoride to form the mixture;
melting the first fluoride, the second fluoride and the third fluoride by heating the mixture to the first temperature; and
cooling the mixture to form the material comprising the eutectic system having the super-lattice of the first fluoride, the second fluoride and the third fluoride.

### Claim at position 9

9-15. (canceled)

### Claim 16

A method comprising:
mixing a first fluoride having a first melting temperature with a second fluoride having a second melting temperature that is lower than the first melting temperature to form a mixture comprising the first fluoride and the second fluoride;
forming a molten mixture of the first fluoride and the second fluoride by heating the mixture of the first fluoride and the second fluoride to a first temperature above at least the second melting temperature;
casting the molten mixture of the first fluoride and the second fluoride in a mold; and
cooling the molten mixture to form an article comprising a eutectic system having a super-lattice of the first fluoride and the second fluoride, wherein the eutectic system has a third melting temperature that is below the first melting temperature and the second melting temperature.

### Claim 17 (depends on 16)

The method of claim 16, wherein the article is a glass ceramic comprising a network of the first fluoride and the second fluoride.

### Claim 18 (depends on 16)

The method of claim 16, wherein the first fluoride and the second fluoride are selected from a group consisting of CaF2, MgF2, SrF2, AlF3, ErF3, LaF3, NdF3, ScF3, CeF4, TiF3, HfF4, ZrF4, and YF3.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first fluoride is ZrF4 and the second fluoride is LaF3.

### Claim 20 (depends on 16)

The method of claim 16, wherein the first fluoride is ZrF4 and the second fluoride is selected from a group consisting of CaF2, MgF2, SrF2, AlF3, ErF3, NdF3, ScF3, CeF4, HfF4, TiF3, and YF3.