# US 2017/0283308 A1 · Scratch resistant glass and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283308 A1
- Document ID: US20170283308A1
- Status: Published application
- Kind: A1
- Application number: 15/585,817
- Filed: 2017-05-03
- Published: 2017-10-05
- Earliest claimed: 2014-05-20
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Sinue Gomez; Robert Michael Morena; Douglas Miles Noni, JR.; James Joseph Price; Sara Jean Sick
- Web page: https://patentgrep.com/patent/US20170283308A1

## CPC

- C03C 11/00: Multi-cellular glass {; Porous or hollow glass or glass particles}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/18: for ion-sensitive glass
- C03C 11/005: {obtained by leaching after a phase separation step}
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 23/008: {comprising a lixiviation step}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A scratch resistant alkali aluminoborosilicate glass. The glass is chemically strengthened and has a surface layer that is rich in silica with respect to the remainder of the glass article. The chemically strengthened glass is then treated with an aqueous solution of a mineral acid other than hydrofluoric acid, such as, for example, HCl, HNO3, H2SO4, or the like, to selective leach elements from the glass and leave behind a silica-rich surface layer. The silica-rich surface layer improves the Knoop scratch threshold of the ion exchanged glass compared to ion exchanged glass that are not treated with the acid solution as well as the post-scratch retained strength of the glass.

## Claims

### Claim at position 1

-18. (canceled)

### Claim 19

A method of improving the scratch resistance of a glass, the method comprising:
a. treating a surface of the glass with an acid at a predetermined temperature for a predetermined time;
b. removing non-silica components from the surface; and
c. forming a porous silica-rich layer on the surface of the glass, wherein the silica-rich layer extends from the surface to a depth of up to about 600 nm into the glass.

### Claim 20 (depends on 19)

The method of claim 19, further comprising ion exchanging the glass prior to treating the surface with an acid.

### Claim 21 (depends on 20)

The method of claim 20, wherein the glass article has a compressive layer extending from the depth of the silica-rich layer to a depth of layer of at least about 20 μm, and wherein the compressive layer has a maximum compressive stress of at least about 300 MPa.

### Claim 22 (depends on 20)

The method of claim 20, wherein the glass article has a Knoop scratch initiation threshold of at least about 12 N.

### Claim 23 (depends on 19)

The method of claim 19, wherein the glass article has a Vickers crack initiation threshold of at least about 5 kgf.

### Claim 24 (depends on 19)

The method of claim 19, wherein the glass article comprises an alkali aluminosilicate glass.

### Claim 25 (depends on 24)

The method of claim 24, wherein the glass article comprises an alkali aluminoborosilicate glass.

### Claim 26 (depends on 19)

The method of claim 19, wherein the glass comprises a borosilicate glass.

### Claim 27 (depends on 19)

The method of claim 19, wherein forming the porous silica-rich layer comprises treating the surface with at least one mineral acid other than hydrofluoric acid.

### Claim 28 (depends on 27)

The method of claim 27, wherein the at least one mineral acid comprises at least one of HCl, HNO3, and H2SO4.

### Claim 29 (depends on 27)

The method of claim 27, wherein the at least one mineral acid is present in a concentration of at least about 0.02 N.

### Claim 30 (depends on 29)

The method of claim 29, wherein the at least one mineral acid is present in a concentration in a range from about 0.02N up to about 60 N.

### Claim 31 (depends on 19)

The method of claim 19, wherein the predetermined temperature is in a range from about 25° C. up to about 95° C.

### Claim 32 (depends on 19)

The method of claim 19, wherein the predetermined time is in a range from about 1 hour up to about 24 hours.