# US 2017/0283303 A1 · Ion exchangeable glasses with high crack initiation threshold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283303 A1
- Document ID: US20170283303A1
- Status: Published application
- Kind: A1
- Application number: 15/625,264
- Filed: 2017-06-16
- Published: 2017-10-05
- Earliest claimed: 2013-09-13
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Qiang FU; Xiaoju GU
- Web page: https://patentgrep.com/patent/US20170283303A1

## CPC

- C03C 3/091: containing aluminium
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Alkali boroaluminosilicate glasses with high resistance to crack initiation and damage due to sharp impact are provided. The glass compositions have melting and forming temperatures that allow forming the glass into sheets via float-based processes while still allowing for the glass to be efficiently ion exchanged. The glass compositions contain MgO, and when ion exchanged, have a Vickers indentation crack initiation load of at least about 10-15 kgf.

## Claims

### Claim 1

A glass composition comprising:
from about 60 to about 70 mol % SiO2
from about 8 to about 13 mol % A12O3
from about 9 to about 15 mol % B2O3
from about 2 to about 8 mol % MgO
from about 8 to about 13 mol % Na2O.

### Claim 2 (depends on 1)

The glass composition of claim 1, comprising:
from about 62 to about 69 mol % SiO2
from about 9 to about 12 mol % A12O3
from about 10 to about 14 mol % B2O3
from about 3 to about 7 mol % MgO
from about 9 to about 12 mol % Na2O.

### Claim 3 (depends on 1)

The glass composition of claim 1, wherein the glass is substantially free of phosphate or CaO.

### Claim 4 (depends on 1)

The glass composition of claim 1, wherein the glass has a strain point from about 500° C. to about 575° C.

### Claim 5 (depends on 1)

The glass composition of claim 1, wherein the glass has a viscosity of less than 104 Poise at 1300° C.

### Claim 6 (depends on 1)

The glass composition of claim 1, wherein the glass has a density of from about 2.320 to about 2.380.

### Claim 7 (depends on 1)

The glass composition of claim 1, wherein the glass has a coefficient of thermal expansion, CTE20-300° C. of from about 55 to about 75×10−7/° C.

### Claim 8 (depends on 1)

The glass composition of claim 1, wherein the glass is ion exchanged to a depth of layer of at least about 10 μm.

### Claim 9 (depends on 8)

The glass composition of claim 8, wherein the glass has a compressive layer extending from a surface of the glass to the depth of layer, and wherein the compressive layer is under a compressive stress of at least about 300 MPa.

### Claim 10 (depends on 9)

The glass composition of claim 9, wherein glass has a Vickers indentation crack initiation load of at least about 15 kgf.

### Claim 11

A method comprising making a glass sheet by floating a glass composition comprising:
from about 60 to about 70 mol % SiO2
from about 8 to about 13 mol % Al2O3
from about 9 to about 15 mol % B2O3
from about 2 to about 8 mol % MgO
from about 8 to about 13 mol % Na2O,
on a tin float bath.

### Claim 12 (depends on 11)

The method of claim 11, wherein the glass composition comprises,
from about 62 to about 69 mol % SiO2
from about 9 to about 12 mol % A12O3
from about 10 to about 14 mol % B2O3
from about 3 to about 7 mol % MgO
from about 9 to about 12 mol % Na2O.

### Claim 13 (depends on 12)

The method of claim 12, wherein the glass is substantially free of phosphate or CaO.

### Claim 14 (depends on 11)

The method of claim 11, wherein the glass has a viscosity of less than 104 Poise at 1300° C.

### Claim 15 (depends on 11)

The method of claim 11, wherein the glass has a density of from about 2.320 to about 2.380.

### Claim 16 (depends on 11)

The method of claim 11, wherein the glass has a coefficient of thermal expansion, CTE20-300° C. of from about 55 to about 75×10−7/° C.

### Claim 17 (depends on 11)

The method of claim 11, wherein the method further comprises subjecting the glasses above to a post-forming heat treatment comprising cooling the glasses to 25° C. at a rate of from about 150-350° C./min.

### Claim 18 (depends on 11)

The method of claim 11, wherein the method further comprises ion exchanging the glass sheets to a depth of layer of at least about 10 μm.

### Claim 19 (depends on 18)

The glass composition of claim 18, wherein the glass has a compressive layer extending from a surface of the glass to the depth of layer, and wherein the compressive layer is under a compressive stress of at least about 300 MPa.

### Claim 20 (depends on 19)

The glass composition of claim 19, wherein glass has a Vickers indentation crack initiation load of at least about 15 kgf.