# US 2017/0282625 A1 · Porous stamp material for laser processing, porous stamp using the same, and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282625 A1
- Document ID: US20170282625A1
- Status: Published application
- Kind: A1
- Application number: 15/345,729
- Filed: 2016-11-08
- Published: 2017-10-05
- Earliest claimed: 2016-04-05
- Assignees: Glory Industry Co., Ltd.; Sunlux Co., Ltd.
- Applicants: Glory Industry Co., Ltd.; Sunlux Co., Ltd.
- Inventors: Yoshitomo Tanaka; Masato Kitahara
- Web page: https://patentgrep.com/patent/US20170282625A1

## CPC

- B29C 67/202: {comprising elimination of a solid or a liquid ingredient}
- B29B 9/06: in the form of filamentary material, e.g. combined with extrusion
- B29C 48/03: characterised by the shape of the extruded material at extrusion
- B29C 48/92: Measuring, controlling or regulating
- B29C 48/002: {combined with surface shaping}
- B29C 48/04: Particle-shaped (making granules B29B9/00)
- B29C 48/08: flexible, e.g. films
- B29C 2948/92704: Temperature
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2101/12: Thermoplastic materials
- B29K 2223/083: {EVA, i.e. ethylene vinyl acetate copolymer}
- B29L 2031/767: {Printing equipment or accessories therefor}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The invention provides a porous stamp material for laser processing that is available for continuous extrusion molding. A material including at least 100 parts by weight of thermoplastic resin, 50-250 parts by weight of hydroxylated compound whose dehydration starting temperature is 100 to 500° C., and water-soluble pore-forming material that has 10-60 μm average particle diameter is mixed to obtain a mixed material. The obtained mixed material is extruded to obtain an extrusion molded product. The obtained extrusion molded product is processed with an aqueous solvent to elute the water-soluble pore-forming material, thereby yielding a porous stamp material that has continuous pores having 10-60 μm pore diameter. The obtained porous stamp material is laser-processed to manufacture a stamp.

## Claims

### Claim 1

A porous stamp material consisting of a porous substance having continuous pores having 10-60 μm pore diameter and comprising a thermoplastic resin and 50-250 parts by weight of hydroxylated compound with respect to 100 parts by weight of the thermoplastic resin, wherein the starting temperature of dehydration of the hydroxylated compound is 100 to 500° C.

### Claim 2 (depends on 1)

The porous stamp material according to claim 1, wherein said hydroxylated compound is aluminum hydroxide or magnesium hydroxide.

### Claim 3 (depends on 2)

The porous stamp material according to claim 2, wherein said hydroxylated compound has an average particle diameter of 5 μm or less.

### Claim 4 (depends on 1)

The porous stamp material according to claim 1, wherein said hydroxylated compound has an average particle diameter of 5 μm or less.

### Claim 5 (depends on 1)

A porous stamp manufactured with the use of the porous stamp material of claim 1.

### Claim 6 (depends on 2)

A porous stamp manufactured with the use of the porous stamp material of claim 2.

### Claim 7 (depends on 4)

A porous stamp manufactured with the use of the porous stamp material of claim 4.

### Claim 8

A method of manufacturing a porous stamp, comprising:
a) mixing a material including at least 100 parts by weight of thermoplastic resin, 50-250 parts by weight of hydroxylated compound whose dehydration starting temperature is 100 to 500° C., and water-soluble pore-forming material that has 10-60 μm average particle diameter, thereby obtaining a mixed material,
b) performing extrusion molding using the obtained mixed material to obtain an extrusion molded product,
c) processing the obtained extrusion molded product with an aqueous solvent and eluting the water-soluble pore-forming material from the processed product to obtain a porous stamp material that has continuous pores having 10-60 μm pore diameter, and,
d) manufacturing a stamp by laser processing of the obtained porous stamp material.