# US 2017/0282516 A1 · Resin composition and compression-molded article of same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282516 A1
- Document ID: US20170282516A1
- Status: Published application
- Kind: A1
- Application number: 15/509,574
- Filed: 2015-10-14
- Published: 2017-10-05
- Earliest claimed: 2014-10-16
- Assignees: Mitsubishi Rayon Co., Ltd.
- Applicants: Mitsubishi Rayon Co., Ltd.
- Inventors: Takuya TERANISHI; Akira OOTA; Masahiro ICHINO; Toru KONDO
- Web page: https://patentgrep.com/patent/US20170282516A1

## CPC

- B32B 27/38: comprising epoxy resins
- B32B 5/022: {Non-woven fabric}
- B32B 5/28: impregnated with or embedded in a plastic substance {(not used)}
- C08G 59/226: {Mixtures of di-epoxy compounds}
- C08J 5/243: {using carbon fibres}
- C08J 5/244: {using glass fibres}
- C08L 51/00: Compositions of graft polymers in which the grafted component is obtained by reactions only involving carbon-to-carbon unsaturated bonds (for ABS polymers C08L55/02); Compositions of derivatives of such polymers
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- B32B 2307/718: Weight, e.g. weight per square meter
- C08J 2363/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C08J 2433/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- C08L 2207/53: Core-shell polymer
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A resin composition including an epoxy resin (A), a curing agent (B), and vinyl polymer particles (C), in which the contained amount of epoxy resin (a1) having a molecular weight of 100-480 is 30-90 parts by mass per 100 parts by mass of the epoxy resin (A), the contained amount of epoxy resin (a2) having a molecular weight of 2,000-40,000 is 10-70 parts by mass per 100 parts by mass of the epoxy resin (A), the contained amount of the vinyl polymer particles (C) is 2-30 parts by mass per 100 parts by mass of the epoxy resin (A), and the instantaneous maximum thickening value of the vinyl polymer particles obtained by the following method is 0.3-5.0 Pa·s/° C.

## Claims

### Claim 1

A resin composition, comprising:
an epoxy resin (A);
a curing agent (B); and
vinyl polymer particles (C),
wherein:
the content of epoxy resin (a1) with a molecular weight of 100 to 480 is 30 to 90 parts by mass based on 100 parts by mass of the epoxy resin (A),
the content of epoxy resin (a2) with a molecular weight of 2000 to 40000 is 10 to 70 parts by mass based on 100 parts by mass of the epoxy resin (A),
the content of the vinyl polymer particles (C) is 2 to 30 parts by mass based on 100 parts by mass of the epoxy resin (A), and
a maximum value of instantaneous increase in viscosity of the vinyl polymer particles (C) is 0.3 to 5.0 Pa·s/° C.

### Claim 2 (depends on 1)

The resin composition according to claim 1, having a viscosity at 30° C. of 1.0×102 to 1.0×105 Pa·s, and having a minimum viscosity measured at a rate of temperature rise of 2° C./min. of 0.8 to 10 Pa·s.

### Claim 3

A resin composition, comprising:
an epoxy resin (A);
a curing agent (B); and
vinyl polymer particles (C),
wherein:
the resin composition has a viscosity at 30° C. of 1.0×102 to 1.0×105 Pa·s,
the resin composition has a minimum viscosity measured at a rate of temperature rise of 2° C./min. of 0.8 to 10 Pa·s,
the content of the vinyl polymer particles (C) is 2 to 30 parts by mass based on 100 parts by mass of the epoxy resin (A), and
a maximum value of instantaneous increase in viscosity of the vinyl polymer particles (C) is 0.3 to 5.0 Pa·s/° C.

### Claim 4 (depends on 1)

The resin composition according to claim 1, wherein the vinyl polymer particles (C) are configured to be core-shell particles having a core layer and shell layer both made of acrylic resin.

### Claim 5 (depends on 4)

The resin composition according to claim 4, wherein a glass transition temperature of the shell layer of the core-shell particles is 85 to 115° C., a value of solubility parameter is 20.20 to 20.50 [(J/cm3)1/2], and a mass ratio of the core layer and shell layer is in a range of 90:10 to 50:50.

### Claim 6 (depends on 1)

The resin composition according to claim 1, wherein the vinyl polymer particles (C) are obtained by conducting two or more stages of emulsion polymerization on vinyl monomer mixtures having different compositions, and by spray-drying the emulsion of the vinyl polymer.

### Claim 7 (depends on 6)

The resin composition according to claim 6, wherein the vinyl monomer mixtures having different compositions are configured to have monomers selected from the group consisting of (i) (meth)acrylates that may have a functional group and (ii) (meth)acrylic acids.

### Claim 8 (depends on 6)

The resin composition according to claim 6, wherein a glass transition temperature of the outermost emulsion-polymerized layer (i) of the vinyl polymer particles (C) is 85 to 115° C., a value of solubility parameter is 20.20 to 20.50 [(J/cm3)1/2], and a mass ratio of the outermost emulsion-polymerized layer (i) and the other emulsion-polymerized layer (ii) is in a range of 90:10 to 50:50.

### Claim 9 (depends on 1)

The resin composition according to claim 1, wherein an average particle diameter of the vinyl polymer particles (C) is 0.5 to 1.0 μm.

### Claim 10 (depends on 1)

The resin composition according to claim 1, wherein the curing agent (B) comprises at least one member selected from the group consisting of an imidazole compound, dicyandiamide and a boron trichloride amine complex.

### Claim 11 (depends on 1)

A prepreg, comprising:
the resin composition according to claim 1; and
a reinforcing fiber material.

### Claim 12 (depends on 1)

A prepreg laminate, configured to have a plurality of sheets of any prepreg,
wherein a layer comprises the resin composition according to claim 1, and the layer is further laminated on at least either outermost layer.

### Claim 13 (depends on 1)

A prepreg laminate, configured to have a plurality of sheets of any prepreg,
wherein a prepreg layer of fiber-reinforced non-woven fabric, made by impregnating the resin composition according to claim 1 into a fiber-reinforced non-woven fabric with a fiber basis weight of 5 to 50 g/m2, is further laminated on at least either outermost layer.

### Claim 14 (depends on 11)

A prepreg laminate, comprising the prepreg according to claim 11.

### Claim 15 (depends on 11)

A molded article formed by compression molding the prepreg according to claim 11.

### Claim 16 (depends on 12)

A molded article formed by compression molding the prepreg laminate according to claim 12.