# US 2017/0282506 A1 · Method of manufacturing a polarizing plate assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282506 A1
- Document ID: US20170282506A1
- Status: Published application
- Kind: A1
- Application number: 15/493,649
- Filed: 2017-04-21
- Published: 2017-10-05
- Earliest claimed: 2013-10-29
- Assignees: Sumitomo Chemical Company, Limited
- Applicants: Sumitomo Chemical Company, Limited
- Inventors: Kenji MATSUNO; Yuuhei INOKUCHI
- Web page: https://patentgrep.com/patent/US20170282506A1

## CPC

- B32B 27/06: as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a layer of a particular substance B32B9/045; next to a bituminous or tarry layer B32B11/046; next to a water setting substance layer B32B13/12; next to a metal layer B32B15/08; next to a glass layer B32B17/10; next to a layer formed of natural mineral fibres or particles B32B19/045; next to a wood layer B32B21/08; next to a cellulosic plastic layer B32B23/08; next to a natural or synthetic rubber layer B32B25/08)}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- B32B 2307/4026: within the layer by addition of a colorant, e.g. pigments, dyes
- B32B 2307/412: Transparent
- B32B 2307/42: Polarizing, birefringent, filtering
- B32B 2457/202: LCD, i.e. liquid crystal displays
- B32B 2457/206: Organic displays, e.g. OLED
- G02F 1/133528: {Polarisers}
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

There is provided a polarizing plate, including: a polarizing layer having a thickness not greater than 20 μm; a first protective film stacked on one surface of the polarizing layer, with a first adhesive layer formed from an active energy ray curing adhesive being interposed; and a second protective film stacked on the other surface of the polarizing layer, with a second adhesive layer formed from a water-soluble adhesive being interposed. There are also provided a polarizing plate with a pressure sensitive adhesive layer, a substrate having a polarizing plate bonded thereto, a liquid crystal display device, and an organic electroluminescence display device, all of which include the polarizing plate. Preferably, at least one of the first protective film and the second protective film has a moisture permeability not higher than 1000 g/m2/24 hr.

## Claims

### Claim 1

A method for manufacturing a polarizing plate assembly, comprising a polarizing plate and a transparent pressure sensitive adhesive layer, the method comprising in the following order:
bonding a second protective film to one surface of a polarizing layer having a thickness not greater than 20 μm, with a water-soluble adhesive interposed therebetween;
bonding a first protective film to the other surface of the polarizing layer, with an active energy ray curing adhesive interposed therebetween; and
providing the transparent pressure sensitive adhesive layer on a side of the polarizing plate having the first protective film.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
at least one of the first protective film and the second protective film has a moisture permeability not higher than 1000 g/m2/24 hr.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the second protective film has a moisture permeability of 10 to 1000 g/m2/24 hr.

### Claim 4 (depends on 1)

The method according to claim 1, wherein
the polarizing layer is a stretched polyvinyl alcohol-based resin layer containing a dichroic colorant.

### Claim 5 (depends on 1)

The method according to claim 1, wherein
the polarizing layer has a thickness not greater than 10 μm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein
the polarizing plate has a rectangular shape having a diagonal length of 3 to 32 cm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein
the polarizing plate further comprises a surface treatment layer stacked on a surface of the first protective film or the second protective film, the surface being a surface on an opposite side of the polarizing layer.

### Claim 8 (depends on 7)

The method according to claim 7, wherein
the surface treatment layer is a hard coat layer, an antireflective layer or an electroconductive layer.

### Claim 9 (depends on 1)

The method according to claim 1, wherein
the first protective film or the second protective film has a thickness not greater than 50 μm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein
a tensile elastic modulus at 80° C. of the first protective film or the second protective film is not lower than 1500 MPa.

### Claim 11

A method for manufacturing a polarizing plate assembly, comprising a polarizing plate and a transparent pressure sensitive adhesive layer, the method comprising:
bonding a second protective film on a polarizing layer having a thickness not greater than 20 μm of a polarizing laminated film, with a water-soluble adhesive interposed therebetween to obtain a bonded film, the polarizing laminated film comprising a substrate film and the polarizing layer;
separating the substrate film from the bonded film to obtain a polarizing plate with a protective film on one side;
bonding a first protective film on the polarizing layer of the polarizing plate with a protective film on one side, with an active energy ray curing adhesive interposed therebetween; and
providing the transparent pressure sensitive adhesive layer on a side of the polarizing plate having the first protective film.

### Claim 12 (depends on 11)

The method according to claim 11, wherein
at least one of the first protective film and the second protective film has a moisture permeability not higher than 1000 g/m2/24 hr.

### Claim 13 (depends on 11)

The method according to claim 11, wherein
the second protective film has a moisture permeability of 10 to 1000 g/m2/24 hr.

### Claim 14 (depends on 11)

The method according to claim 11, wherein
the polarizing layer is a stretched polyvinyl alcohol-based resin layer containing a dichroic colorant.

### Claim 15 (depends on 11)

The method according to claim 11, wherein
the polarizing layer has a thickness not greater than 10 μm.

### Claim 16 (depends on 11)

The method according to claim 11, wherein
the polarizing plate has a rectangular shape having a diagonal length of 3 to 32 cm.

### Claim 17 (depends on 11)

The method according to claim 11, wherein
the polarizing plate further comprises a surface treatment layer stacked on a surface of the first protective film or the second protective film, the surface being a surface on an opposite side of the polarizing layer.

### Claim 18 (depends on 17)

The method according to claim 17, wherein
the surface treatment layer is a hard coat layer, an antireflective layer or an electroconductive layer.

### Claim 19 (depends on 11)

The method according to claim 11, wherein
the first protective film or the second protective film has a thickness not greater than 50 μm.

### Claim 20 (depends on 11)

The method according to claim 11, wherein
a tensile elastic modulus at 80° C. of the first protective film or the second protective film is not lower than 1500 MPa.