# US 2017/0282503 A1 · Laminated glass article with ion exchangeable core and clads layers having diffusivity contrast and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282503 A1
- Document ID: US20170282503A1
- Status: Published application
- Kind: A1
- Application number: 15/507,005
- Filed: 2015-08-25
- Published: 2017-10-05
- Earliest claimed: 2014-08-28
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Gaozhu Peng; Chunfeng Zhou
- Web page: https://patentgrep.com/patent/US20170282503A1

## CPC

- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- C03B 17/02: Forming {molten} glass coated with coloured layers; {Forming molten glass of different compositions or layers; Forming molten glass comprising reinforcements or inserts}
- C03B 17/064: {by the overflow downdraw fusion process; Isopipes therefor}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A laminated glass article has a first layer having a first ion exchange diffusivity, D0, and a second layer adjacent to the first layer and having a second ion exchange diffusivity, D1. D0/D1 is from about 1.2 to about 10, or D0/D1 is from about 0.05 to about 0.95. A method for manufacturing the laminated glass article includes forming a first layer having a first ion exchange diffusivity, D0, and forming a second layer adjacent to the first layer and having a second ion exchange diffusivity, D1. The laminated glass article can be strengthened by an ion exchange process to form a strengthened laminated glass article having a compressive stress layer with a depth of layer from about 8 μm to about 100 μm.

## Claims

### Claim 1

A laminated glass article comprising:
a first layer comprising a first ion exchange diffusivity, D0; and
a second layer adjacent to the first layer and comprising a second ion exchange diffusivity, D1,
wherein D0/D1 is from about 1.2 to about 10.

### Claim 2 (depends on 1)

The laminated glass article of claim 1, wherein the first layer is a core layer and the second layer is a clad layer.

### Claim 3 (depends on 1)

The laminated glass article of claim 1, wherein the first layer is a first clad layer and the second layer is a second clad layer.

### Claim 4 (depends on 1)

The laminated glass article of claim 1, wherein a central tension of the laminated glass article is less than a threshold central tension (TCT) calculated using formula (2):
TCT(MPa)=−38.7 (MPa/mm)·ln(t)(mm)+48.2 (MPa) (2),
wherein t represents a thickness of the laminated glass article.

### Claim 5 (depends on 1)

The laminated glass article of claim 1, wherein the laminated glass article comprises a compressive stress layer with a depth of layer from about 8 μm to about 150 μm.

### Claim 6 (depends on 5)

The laminated glass article of claim 5, wherein the depth of layer is from about 50 μm to about 150 μm.

### Claim 7 (depends on 5)

The laminated glass article of claim 5, wherein the compressive stress layer has a maximum compressive stress from about 300 MPa to about 1000 MPa.

### Claim 8 (depends on 1)

The laminated glass article of claim 1, wherein a thickness of the laminated glass article is from about 0.075 mm to about 4 mm.

### Claim 9 (depends on 8)

The laminated glass article of claim 8, wherein the thickness of the laminated glass article is from about 0.3 mm to about 2 mm.

### Claim 10 (depends on 1)

The laminated glass article of claim 1, wherein a thickness of the second layer is from about 3 μm to about 100 μm.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The laminated glass article of claim 1, wherein
D0/D1 is from about 5 to about 10,
the laminated glass article comprises a compressive stress layer with a depth of layer that is from about 8 μm to about 80 μm,
a maximum compressive stress in the compressive stress layer is from about 600 MPa to about 900 MPa, and
a central tension of the laminated glass article is less than a threshold central tension (TCT) calculated using formula (2):
TCT(MPa)=−38.7 (MPa/mm)·ln(t)(mm)+48.2 (MPa) (2),
wherein t represents a thickness of the laminated glass article.

### Claim 13

A method for manufacturing a laminated glass article, the method comprising:
forming a first layer having a first ion exchange diffusivity, D0; and
forming a second layer adjacent to the first layer and having a second ion exchange diffusivity, D1;
wherein D0/D1 is from about 1.2 to about 10.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first layer is a core layer and the second layer is a clad layer.

### Claim 15 (depends on 13)

The method of claim 13, wherein the first layer is a first clad layer and the second layer is a second clad layer.

### Claim 16 (depends on 13)

The method of claim 13, further comprising strengthening the laminated glass article by an ion exchange process to form a strengthened laminated glass article having a compressive stress layer with a depth of layer from about 8 μm to about 100 μm

### Claim 17 (depends on 16)

The method of claim 16, wherein the strengthening the laminated glass article comprises immersing the laminated glass article in a substantially pure molten KNO3 bath for a duration from about 2 hours to about 16 hours at a temperature from about 370° C. to about 530° C.

### Claim 18 (depends on 17)

The method of claim 17, wherein the strengthening the laminated glass article comprises immersing the laminated glass article in a second molten KNO3 bath having an effective mole fraction of K+ of less than about 90% for a duration of about 0.2 hours to about 1 hour at a temperature of about 400° C.

### Claim 19 (depends on 13)

The method of claim 13, wherein a thickness of the laminated glass article is from about 0.075 mm to about 4 mm.

### Claim 20

(canceled)

### Claim 21 (depends on 13)

The method of claim 13, wherein a thickness of the second layer is from about 3 μm to about 100 μm.

### Claim 22

(canceled)

### Claim 23 (depends on 13)

The method of claim 13, wherein
D0/D1 is from about 5 to about 10,
the depth of layer is from about 8 μm to about 80 μm,
a maximum compressive stress in the compressive stress layer is from about 500 MPa to about 900 MPa, and
a central tension of the laminated glass article is less than a threshold central tension (TCT) calculated using formula (2):
TCT(MPa)=−38.7 (MPa/mm)·ln(t)(mm)+48.2 (MPa) (2),
wherein t represents the thickness of the laminated glass article.