# US 2017/0282491 A1 · Veil-stabilized composite with improved tensile strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282491 A1
- Document ID: US20170282491A1
- Status: Published application
- Kind: A1
- Application number: 15/623,630
- Filed: 2017-06-15
- Published: 2017-10-05
- Earliest claimed: 2013-01-30
- Assignees: The Boeing Company
- Applicants: The Boeing Company
- Inventors: Thomas K. Tsotsis
- Web page: https://patentgrep.com/patent/US20170282491A1

## CPC

- B32B 5/022: {Non-woven fabric}
- B32B 5/028: {Net structure, e.g. spaced apart filaments bonded at the crossing points}
- B32B 5/06: characterised by a fibrous {or filamentary} layer {mechanically connected, e.g. by needling} to another layer, e.g. of fibres, of paper
- B32B 5/26: another layer {next to it} also being fibrous or filamentary {(relative arrangement of fibres or filaments of different layers B32B5/12)}
- B32B 37/14: characterised by the properties of the layers
- C08J 5/247: {using fibres of at least two types}
- B32B 2250/20: All layers being fibrous or filamentary
- B32B 2250/42: Alternating layers, e.g. ABAB(C), AABBAABB(C)
- B32B 2260/023: Two or more layers
- B32B 2260/046: Synthetic resin
- B32B 2262/02: Synthetic macromolecular fibres
- B32B 2262/106: Carbon fibres, e.g. graphite fibres
- B32B 2305/076: Prepregs
- B32B 2305/20: in the form of a non-woven mat
- B32B 2305/72: Cured, e.g. vulcanised, cross-linked
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/542: Shear strength
- B32B 2605/18: Aircraft
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A method for manufacturing a composite may include: selecting an interlayer material having a first distortional-deformation capability; selecting a matrix material having a second distortional-deformation capability, which is less than the first distortional-deformation capability; disposing at least one reinforcing layer, formed of reinforcing fibers of a reinforcing material, and at least one interlayer, formed of a nonwoven fabric of the interlayer material, in an alternating configuration; and infusing the at least one reinforcing layer and the at least one interlayer with the matrix material such that the matrix material flows though the at least one reinforcing layer and the at least one interlayer. Selection of the interlayer material having the first distortional-deformation capability and the matrix material having the second distortional-deformation capability is configured to increase tensile strength of the composite.

## Claims

### Claim 1

A method for manufacturing a composite, said method comprising:
selecting an interlayer material having a first distortional-deformation capability;
selecting a matrix material having a second distortional-deformation capability, which is less than said first distortional-deformation capability;
disposing at least one reinforcing layer, formed of reinforcing fibers of a reinforcing material, and at least one interlayer, formed of a nonwoven fabric of said interlayer material, in an alternating configuration; and
infusing said at least one reinforcing layer and said at least one interlayer with said matrix material such that said matrix material flows though said at least one reinforcing layer and said at least one interlayer,
wherein selection of said interlayer material having said first distortional-deformation capability and said matrix material having said second distortional-deformation capability is configured to increase tensile strength of said composite.

### Claim 2 (depends on 1)

The method of claim 1 wherein said first distortional-deformation capability is at least approximately 10 percent greater than said second distortional-deformation capability.

### Claim 3 (depends on 2)

The method of claim 2 wherein:
said first distortional-deformation capability corresponds to a first von Mises strain of said interlayer material, and
said second distortional-deformation capability corresponds to a second von Mises strain of said matrix material, which is less than said first von Mises strain.

### Claim 4 (depends on 3)

The method of claim 3 further comprising curing said matrix material to form a cured composite.

### Claim 5 (depends on 4)

The method of claim 4 wherein said cured composite has an overall distortional-deformation capability, which is greater than said second distortional-deformation capability, and wherein said overall distortional-deformation capability corresponds to an overall von Mises strain of said cured composite.

### Claim 6 (depends on 5)

The method of claim 5 wherein said overall von Mises strain is at least approximately 0.3.

### Claim 7 (depends on 1)

The method of claim 1 further comprising melt-bonding said at least one interlayer and said at least one reinforcing layer together.

### Claim 8 (depends on 1)

The method of claim 1 further comprising knit-stitching said at least one interlayer and said at least one reinforcing layer together.

### Claim 9 (depends on 1)

The method of claim 1 wherein said infusing step comprises one of pre-impregnating said at least one reinforcing layer and said at least one interlayer with said matrix material or liquid molding said at least one reinforcing layer and said at least one interlayer with said matrix material.

### Claim 10 (depends on 1)

The method of claim 1 wherein:
said interlayer material is insoluble in said matrix material, and
said matrix material has a gel temperature that is below a melting temperature of said interlayer material.

### Claim 11 (depends on 1)

The method of claim 1 wherein said interlayer material comprises continuous polymeric fibers.

### Claim 12

A method for manufacturing a composite, said method comprising:
selecting an interlayer material having a first distortional-deformation capability;
selecting a matrix material having a second distortional-deformation capability, which is less than said first distortional-deformation capability;
disposing a plurality of reinforcing layers, formed of reinforcing fibers of a reinforcing material, and a plurality of interlayers, formed of a nonwoven fabric of said interlayer material, in an alternating configuration; and
infusing said plurality of reinforcing layers and said plurality of interlayers with said matrix material such that said matrix material flows though said plurality of reinforcing layers and said plurality of interlayers,
wherein selection of said interlayer material having said first distortional-deformation capability and said matrix material having said second distortional-deformation capability is configured to provide a cured composite having an overall distortional-deformation capability, which is greater than said second distortional-deformation capability, to increase tensile strength of said cured composite.

### Claim 13 (depends on 12)

The method of claim 12 wherein:
said first distortional-deformation capability corresponds to a first von Mises strain of said interlayer material,
said second distortional-deformation capability corresponds to a second von Mises strain of said matrix material, which is less than said first von Mises strain, and
said overall distortional-deformation capability corresponds to an overall von Mises strain of said cured composite, which is greater than said second von Mises strain.

### Claim 14 (depends on 12)

The method of claim 12 further comprising bonding one of said plurality of interlayers to at least one surface of one of said plurality of reinforcing layers to form an interlayer-stabilized fabric.

### Claim 15 (depends on 14)

The method of claim 14 wherein:
said infusing step comprises pre-impregnating said interlayer-stabilized fabric with said matrix material, and
said disposing step comprises laying up a plurality of layers of said interlayer-stabilized fabric pre-impregnating with said matrix material.

### Claim 16 (depends on 14)

The method of claim 14 wherein:
said disposing step comprises laying up a plurality of layers of said interlayer-stabilized fabric, and
said infusing step comprises liquid molding said plurality of layers of said interlayer-stabilized fabric with said matrix material.

### Claim 17

A method for improving tensile strength of a composite comprising at least one reinforcing layer, formed of reinforcing fibers of a reinforcing material, and at least one interlayer, formed of a nonwoven fabric of an interlayer material, disposed in an alternating configuration and infused with a matrix material, said method comprising:
selecting said interlayer material having a first distortional-deformation capability; and
selecting said matrix material having a second distortional-deformation capability, which is less than said first distortional-deformation capability,
wherein selection of said interlayer material having said first distortional-deformation capability and said matrix material having said second distortional-deformation capability is configured to increase tensile strength of said composite.

### Claim 18 (depends on 17)

The method of claim 17 wherein said first distortional-deformation capability is at least approximately 10 percent greater than said second distortional-deformation capability.

### Claim 19 (depends on 17)

The method of claim 17 wherein:
said composite has an overall distortional-deformation capability, which is greater than said second distortional-deformation capability, and
selection of said interlayer material having said first distortional-deformation capability and said matrix material having said second distortional-deformation capability is configured to increase said tensile strength of said composite by at least approximately 10 percent.

### Claim 20 (depends on 19)

The method of claim 19 wherein:
said first distortional-deformation capability corresponds to a first von Mises strain of said interlayer material,
said second distortional-deformation capability corresponds to a second von Mises strain of said matrix material, which is less than said first von Mises strain, and
said overall distortional-deformation capability corresponds to an overall von Mises strain of said cured composite, which is greater than said second von Mises strain.