# US 2017/0282252 A1 · Method of forming inorganic nanocages

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282252 A1
- Document ID: US20170282252A1
- Status: Published application
- Kind: A1
- Application number: 15/477,601
- Filed: 2017-04-03
- Published: 2017-10-05
- Earliest claimed: 2016-04-01
- Assignees: Research Foundation of the City University of New York
- Applicants: Research Foundation of the City University of New York
- Inventors: Hiroshi Matsui; Zengyan Wei; Justin Fang
- Web page: https://patentgrep.com/patent/US20170282252A1

## CPC

- B22F 1/054: Nanosized particles
- B22F 1/0553: {Complex form nanoparticles, e.g. prism, pyramid, octahedron}
- B22F 1/102: Metallic powder coated with organic material
- B22F 1/145: Chemical treatment, e.g. passivation or decarburisation
- C09C 1/24: Oxides of iron
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}

## Abstract

Nanocages are formed by etching nancubes. The nanocubes are added to an aqueous system having an amphiphilic lipid dissolved in an organic solvent (e.g. a hydrophobic alcohol) to form reverse micelles. As the water evaporates the micelles shrink as etching of the flat surface of the nanocubes occurs. In this fashion hollow nanocages are produced. In one embodiment, the nanocage is covalently attached to a polymer shell (e.g. a dextran shell).

## Claims

### Claim 1

A method of forming a nanocage, the method comprising steps of:
forming a reverse micelle system comprising an inorganic nanocube having a diameter of 15 nm or less, an amphiphilic lipid, water and an organic solvent that is immiscible with water and has a boiling point greater than 100° C.;
removing the water by evaporation, the step of removing causing the inorganic nanocube to be etched to form a nanocage, wherein the nanocage has a diameter less than the diameter of the inorganic nanocube;
covalently attaching a polymer shell to the nanocage, wherein the polymer shell has a diameter of less than 50 nm.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the inorganic nanocube is selected from a group consisting of a palladium nanocube, a gold nanocube and an iron oxide nanocube.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein the inorganic nanocube consists of iron oxide.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the inorganic nanocube consists of palladium.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the inorganic nanocube consists of gold.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the polymer shell comprises dextran.

### Claim 7 (depends on 6)

The method as recited in claim 6, wherein the nanocage is covalently attached to the polymer shell by a catechol linking group.

### Claim 8 (depends on 6)

The method as recited in claim 6, wherein the nanocage is covalently attached to the polymer shell by a dopamine linking group.

### Claim 9 (depends on 6)

The method as recited in claim 6, wherein the dextran comprises an aminodextran.

### Claim 10

A method of forming a nanocage, the method comprising sequential steps of:
forming a reverse micelle system comprising an inorganic nanocube consisting of iron oxide having a diameter of 15 nm or less, an amphiphilic lipid, water and an organic solvent that is immiscible with water and has a boiling point greater than 100° C.;
removing the water by evaporation, the step of removing causing the inorganic nanocube to be etched to form an iron oxide nanocage, wherein the iron oxide nanocage has a diameter less than the diameter of the inorganic nanocube;
covalently attaching a polymer shell to the iron oxide nanocage, wherein the polymer shell comprises dextran and has a diameter of less than 50 nm and the iron oxide nanocage is covalently attached to the polymer shell by a catechol linking group.

### Claim 11 (depends on 10)

The method as recited in claim 10, wherein the catechol is a dopamine.

### Claim 12 (depends on 10)

The method as recited in claim 10, wherein the dextran comprises an aminodextran.

### Claim 13

A composition of matter comprising:
an inorganic nanocage with a diameter less than 15 nm;
a polymer shell comprising dextran surrounding the inorganic nanocage, wherein the polymer shell has a diameter of less than 50 nm and the inorganic nanocage is covalently attached to the polymer shell by a catechol linking group.

### Claim 14 (depends on 13)

The composition of matter as recited in claim 13, wherein the inorganic nanocage consists of iron oxide.

### Claim 15 (depends on 13)

The composition of matter as recited in claim 13, wherein the catechol linking group is a dopamine.