# US 2017/0282246 A1 · Method and device for the additive manufacture of at least one component region of a component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0282246 A1
- Document ID: US20170282246A1
- Status: Published application
- Kind: A1
- Application number: 15/470,439
- Filed: 2017-03-27
- Published: 2017-10-05
- Earliest claimed: 2016-04-01
- Assignees: MTU Aero Engines AG
- Applicants: MTU Aero Engines AG
- Inventors: Christian Liebl; Alexander Ladewig; Laura Buerger; Georg Schlick; Steffen Schlothauer; Karl-Heinz Dusel
- Web page: https://patentgrep.com/patent/US20170282246A1

## CPC

- B23K 26/083: {Devices involving movement of the workpiece in at least one axial direction}
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/36: of energy beam parameters
- B22F 10/366: Scanning parameters, e.g. hatch distance or scanning strategy
- B23K 26/342: Build-up welding
- B23K 26/702: {Auxiliary equipment}
- B23K 31/125: {Weld quality monitoring}
- B33Y 10/00: Processes of additive manufacturing
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- B33Y 50/02: for controlling or regulating additive manufacturing processes
- B33Y 80/00: Products made by additive manufacturing
- B22F 5/009: {of turbine components other than turbine blades (of turbine blades B22F5/04)}
- B22F 10/385: {Overhang structures}
- B22F 12/41: characterised by the type, e.g. laser or electron beam
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B23K 2101/001: {Turbines}
- Y02P 10/25: Process efficiency
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method for the additive manufacture of at least one region (16) of a component. Here, at least the following steps are carried out: a) layer-wise application of at least one powder-form component material onto a component platform in the region of a build-up and joining zone (14); b) layer-wise and local solidifying of the component material by selective exposure of the component material by at least one high-energy beam (12) in the region of the build-up and joining zone (14), with the formation of a component layer (15); c) layer-wise lowering of the component platform by a pre-defined layer thickness; and d) repeating steps a) to c) until the component region (16) or the component has been completely fabricated.

## Claims

### Claim 1

A method for the additive manufacture of at least one region (16) of a component, comprising the following steps:
a) layer-wise application of at least one powder-form component material onto a component platform in the region of a build-up and joining zone (14);
b) layer-wise and local solidifying of the component material by selective exposure of the component material by at least one high-energy beam (12) in the region of the build-up and joining zone (14), with the formation of a component layer (15);
c) layer-wise lowering of the component platform by a pre-defined layer thickness; and
d) repeating steps a) to c) until the component region (16) or the component has been completely fabricated;
wherein during at least one step b), at least one exposure parameter of the high-energy beam from the group: power (P), velocity (v), and focal position (F), is adjusted as a function of at least one construction parameter from the group: component thickness (bteil), hatch distance (h) to an adjacent exposure trace, angle of incidence (c) of the high-energy beam (12) relative to the surface of the component layer (15), angle of deflection (β) of the high-energy beam (12) with respect to a vertical axis (z) of the component layer (15), overhang angle (γ) of the component layer (15), layer thickness (n) of the component layer (15), and distance (w) from a complete volume element of the component layer (15).

### Claim 2 (depends on 1)

The method according to claim 1, wherein
a laser sintering method and/or a laser melting method is used as the additive manufacturing method, and/or a laser beam is used as the high-energy beam (12).

### Claim 3 (depends on 1)

The method according to claim 1, wherein
at least the exposure parameter, power (P), of the high-energy beam (12) is reduced, when compared to the power in an inskin region (22), if the construction parameter, overhang angle (γ), of the component layer (15) in the exposed region corresponds to a downskin region (20), and/or in that at least the exposure parameter, power (P), of the high-energy beam (12) is increased, when compared to the power in an inskin region (22), if the construction parameter, overhang angle (γ), of the component layer (15) in the exposed region corresponds to an upskin region (18).

### Claim 4 (depends on 1)

The method according to claim 1, wherein
the at least one exposure parameter of the high-energy beam (12) from the group: power (P), velocity (v), and focal position (F), is determined in advance, prior to the manufacture of the component layer (15) in step b) as a function of at least one construction parameter from the group: component thickness (bteil), hatch distance (h) to an adjacent exposure trace, angle of incidence (α) of the high-energy beam relative to the surface of the component layer, angle of deflection (β) of the high-energy beam with respect to a vertical axis of the component layer, overhang angle (γ) of the component layer, layer thickness (n) of the component layer, and distance (w) from a complete volume element of the component layer, and is provided as a data set for control and/or regulation of the high-energy beam (12).

### Claim 5 (depends on 4)

The method according to claim 4, wherein
the at least one exposure parameter (P, v, F) of the high-energy beam (12) is pre-determined in the scope of a determination of a hatch geometry of the component layer (15).

### Claim 6 (depends on 1)

The method according to claim 1, wherein
during at least one step b) and/or after at least one step b), at least one measurement parameter characterizing a quality of the manufactured component layer (15) is determined, and the at least one exposure parameter of the high-energy beam (12) from the group: power (P), velocity (v) and focal position (F), is determined and/or modified as a function of the measurement parameter and of the at least one construction parameter (bteil, n, w, α, β, φ, h).

### Claim 7 (depends on 1)

The method according to claim 1, wherein
a radiation source (10), which generates the high-energy beam (12), is not moved, at least during one step b).

### Claim 8

A device for the additive manufacture of at least one region (15) of a component of a turbine or of a compressor, comprising:
at least one powder supply for applying at least one powder layer from a component material onto a build-up and joining zone (14) of a component platform that can be lowered; and
at least one radiation source (10) for generating at least one high-energy beam (12), by which the powder layer can be solidified locally into a component layer (15) in the region of the build-up and joining zone,
wherein this device
comprises a memory unit with a data set provided in a memory, whereby the data set comprises at least one construction parameter from the group: component thickness (bteil), hatch distance (h) to an adjacent exposure trace, angle of incidence (α) of the high-energy beam (12) relative to the surface of the component layer (15), angle of deflection (β) of the high-energy beam (12) with respect to a vertical axis (z) of the component layer (15), overhang angle (γ) of the component layer (15), layer thickness (n) of the component layer (15), and distance (w) from a complete volume element of the component layer (15); and
a control device for controlling and/or regulating the radiation source (10), wherein the control device is designed for the purpose of pre-determining at least one exposure parameter of the high-energy beam (12) from the group: power (P), velocity (v), and focal position (F), as a function of the data set.

### Claim 9

(canceled)

### Claim 10 (depends on 8)

The device according to claim 8 wherein
further comprising a measuring instrument, by which at least one measurement parameter characterizing a quality of the manufactured component layer (15) can be determined.

### Claim 11 (depends on 10)

The device according to claim 10, wherein
the control device is coupled to the measuring instrument for exchanging data, and is designed to determine in advance the at least one exposure parameter of the high-energy beam (12) from the group: power (P), velocity (v), and focal position (F), as a function of the data set and of the measurement parameter, and/or to modify at least one already pre-determined exposure parameter (P, v, F).