# US 2017/0271725 A1 · Method for recovering lead oxide from waste lead paste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0271725 A1
- Document ID: US20170271725A1
- Status: Published application
- Kind: A1
- Application number: 15/505,608
- Filed: 2015-06-10
- Published: 2017-09-21
- Earliest claimed: 2014-08-20
- Assignees: Beijing University of Chemical Technology
- Applicants: Beijing University of Chemical Technology
- Inventors: Junqing PAN; Yaru BIAN; Yanzhi SUN; Yinjian NIU
- Web page: https://patentgrep.com/patent/US20170271725A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- C01G 21/06: Lead monoxide [PbO]
- C01G 21/14: Carbonates
- C22B 7/006: {Wet processes}
- C22B 13/045: {Recovery from waste materials}
- H01M 4/56: of lead
- H01M 10/06: Lead-acid accumulators (semi-lead accumulators H01M10/20)
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for recovering lead oxide from a pre-desalted lead paste, comprising the following steps: a. dissolving the pre-desalted lead plaster by using a complexing agent solution, and making all of PbO therein react with the complexing agent to generate lead complexing ions, obtaining a lead-containing solution and a filter residue; b. adding a precipitant to the lead-containing solution, and then the precipitant reacting with the lead complexing ions to generate a lead salt precipitate and the regenerated complexing agent; c. calcining the lead salt precipitate to obtain lead oxide and regenerate the precipitant. The final recovery rate of lead oxide of the method can reach 99% or more.

## Claims

### Claim 1

A method for recovering lead oxide from pre-desalted lead paste, comprising the following steps:
a. dissolving pre-desalted lead paste by using a complexing agent solution, so that all PbO in the pre-desalted lead paste reacts with the complexing agent to generate lead complexing ions and thereby obtain a lead-containing solution and a filter residue, wherein, the PbO is from the original PbO in the pre-desalted lead paste and PbO generated in a reaction between the original Pb and PbO2 from the pre-desalted lead paste in the complexing agent solution, and further includes PbO obtained from oxidation of the original Pb in the pre-desalted lead paste or reduction of the original PbO2, wherein, the complexing agent is selected from compound with amino and carboxyl groups, organic amine, alcohol amine, or salts of them;
b. adding a precipitant into the lead-containing solution, so that the precipitant reacts with the lead complexing ions to generate a lead salt precipitate and a regenerated complexing agent, wherein, the precipitant is selected from CO2, SO2 or SO3. or a water solution of them;
c. calcining the lead salt precipitate to obtain lead oxide and regenerate the precipitant.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, the pre-desalted lead paste refers to a product obtained through a reaction between the lead paste and an alkaline liquor in which the lead salts included in the lead paste are removed, the lead salt is PbSO4, PbSO3, Pb(CH3COO)2, Pb(NO3)2, Pb(ClO4)2 or PbCO3, the alkaline liquor is selected from a water solution of NaOH, KOH, ammonia, or Ba(OH)2 in which the concentration in weight percentage is 0.5-40%, and the desalting time is 0.5-60 min.

### Claim 3

(canceled)

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The method according to claim 1, wherein, the compound with amino and carboxyl groups is selected from a-amino acid, ethylene diammine diacetate, ethylenediamine tetraacetic acid, propanediamine diacetic acid, iminodiacetic acid, glucosaminic acid, or alginic acid; wherein, the organic amine is selected from methyl amine, ethylene diamine, propylene diamine, diethylene triamine, or triethylene tetramine; wherein, the alcohol amine is selected from ethanolamine, di-ethanolamine, or tri-ethanolamine.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, in the step a, a catalyst is added into the complexing agent solution to accelerate the oxidation-reduction reaction between Pb and PbO2 that generates PbO, wherein, the catalyst is selected from metal powder of Cu, Co, Ni, or Ag, or chlorides, oxides or nitrates of the aforesaid metal.

### Claim 7 (depends on 1)

The method according to claim 1, wherein,
if the content of Pb in the pre-desalted lead paste is lower than the content of PbO2, additional lead is added in the step a, so as to fully reduce PbO2 to PbO; or
if the content of Pb in the pre-desalted lead paste is greater than the content of PbO2, oxygen is blasted into the complexing agent solution in the step a, so as to fully convert Pb into PbO; or
regardless of the content of Pb and the content of PbO2 in the pre-desalted lead paste, the pre-desalted lead paste is treated with adequate H2O2 solution, so as to fully oxidize Pb to PbO, or fully reduce PbO2 to PbO.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The method according to claim 1, wherein, the regenerated complexing agent obtained in the step b is returned to the step a and reused; and/or the regenerated precipitant obtained in the step c is returned to the step b and reused; wherein, both the step a and the step b are executed within a water solution temperature range of 5-110° C.

### Claim 10 (depends on 5)

The method according to claim 5, wherein, the α-amino acid is selected from aspartic acid, methionine, valine, lysine, isoleucine, phenylalanine, tryptophane, threonine, glycine, proline, histidine, glutamic acid, serine, arginine, sarcosine or citrulline.