# US 2017/0256904 A1 · Laser active medium and process of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256904 A1
- Document ID: US20170256904A1
- Status: Published application
- Kind: A1
- Application number: 15/509,808
- Filed: 2015-08-28
- Published: 2017-09-07
- Earliest claimed: 2014-09-09
- Assignees: Universitaet Wien
- Applicants: Universitaet Wien
- Inventors: Markus ASPELMEYER; Garrett COLE
- Web page: https://patentgrep.com/patent/US20170256904A1

## CPC

- H01S 3/0602: {Crystal lasers or glass lasers (H01S3/063 takes precedence)}
- H01S 3/0071: {Beam steering, e.g. whereby a mirror outside the cavity is present to change the beam direction}
- H01S 3/025: {of solid state lasers, e.g. housings or mountings}
- H01S 3/0405: {Conductive cooling, e.g. by heat sinks or thermo-electric elements}
- H01S 3/0604: {in the form of a plate or disc}
- H01S 5/0071: {for beam steering, e.g. using a mirror outside the cavity to change the beam direction}
- H01S 5/0215: {Bonding to the substrate}
- H01S 5/023: Mount members, e.g. sub-mount members
- H01S 5/02315: Support members, e.g. bases or carriers
- H01S 5/0233: Mounting configuration of laser chips
- H01S 5/0235: Method for mounting laser chips
- H01S 5/02469: {Passive cooling, e.g. where heat is removed by the housing as a whole or by a heat pipe without any active cooling element like a TEC}
- H01S 5/02476: {Heat spreaders, i.e. improving heat flow between laser chip and heat dissipating elements}
- H01S 5/02484: {Sapphire or diamond heat spreaders}
- H01S 3/042: for solid state lasers {(H01S3/0401 takes precedence)}
- H01S 3/0612: {Non-homogeneous structure (H01S3/07 takes precedence)}
- H01S 3/0621: {Coatings on the end-faces, e.g. input/output surfaces of the laser light}
- H01S 3/094038: {End pumping}
- H01S 5/0217: {Removal of the substrate}
- H01S 5/14: External cavity lasers (H01S5/18 takes precedence; mode locking H01S5/065)
- H01S 5/183: having only vertical cavities, e.g. vertical cavity surface-emitting lasers [VCSEL]
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL

## Abstract

A solid-state laser active medium comprising an optical gain material; a heat sink, wherein the heat sink is transparent, in particular over a wavelength range of 200 nm to 4000 nm, preferably with an absorption coefficient of <1 cm−1; the heat sink having a high thermal conductivity, in particular ≧149 W/(m*K); wherein the optical gain material and the heat sink exhibit a root-mean square, RMS, surface roughness of <1 nm; wherein the optical gain material is attached to the transparent heat sink by direct bonding.

## Claims

### Claim 1

A laser active medium for a solid-state laser system comprising:
an optical gain material;
a heat sink, wherein the heat sink is transparent within a threshold;
the heat sink having a high thermal conductivity within a threshold;
wherein the optical gain material and the heat sink exhibit a root-mean square surface roughness of <1 nm; and
wherein the optical gain material is attached to the transparent heat sink by direct bonding.

### Claim 2 (depends on 1)

The laser active medium according to claim 1, wherein the laser active medium further comprises a high reflectivity thin-film stack, wherein the optical gain material is combined with the high reflectivity thin-film stack.

### Claim 3 (depends on 1)

The laser active medium according to claim 1, wherein the optical gain material comprises a semiconductor structure or a doped laser crystal.

### Claim 4 (depends on 3)

The laser active medium according to claim 3, wherein the semiconductor structure is monolithic, combining a high reflectivity stack of alternating high and low index material and semiconductor-based optical gain material in one continuous structure.

### Claim 5 (depends on 4)

The laser active medium according to claim 4, wherein the semiconductor-based optical gain material comprises a semiconductor quantum structure.

### Claim 6 (depends on 3)

The laser active medium according to claim 3, wherein an active element comprises a composite structure including a doped laser crystal combined with a multilayer stack of alternating high and low index materials yielding a high reflectivity mirror.

### Claim 7 (depends on 3)

The laser active medium according to claim 3, wherein the doped laser crystal comprises at least one of YAG doped with Nd, Yb, Er, Tm or combinations thereof; neodymium doped vanadates, neodymium doped tungstates, ytterbium doped tungstates, titanium doped sapphire, chromium doped Al2O3, chromium doped chalcogenides.

### Claim 8 (depends on 1)

The laser active medium according to claim 1, wherein the direct bonding of the optical gain material to the transparent heat sink comprises van der Waals forces.

### Claim 9 (depends on 1)

The laser active medium according to claim 1, wherein the heat sink comprises a transparent and high thermal conductivity material including one of diamond, SiC, and AlN for visible and IR operation in a range of wavelengths from 200 nm to 4000 nm, or single-crystal silicon for near and mid-IR applications in a range of wavelengths from 1200-4000 nm.

### Claim 10

A method for manufacturing a laser active medium comprising a semiconductor-based optical gain material, a heat sink, the heat sink having a high thermal conductivity within a threshold, and being optically transparent within a threshold;
the method comprising the steps of:
providing the semiconductor-based optical gain material, the optical gain material having a root-mean square surface roughness of <1 nm, on a first substrate, wherein the first substrate comprises GaAs, InP, GaN, AlN, Si, or Ge;
providing the heat sink, the heat sink having a polished surface with a root-mean square roughness below 1 nm;
detaching the optical gain material from the first substrate;
attaching the optical gain material to the heat sink by direct bonding.

### Claim 11

A method for manufacturing a laser active medium based on a doped laser crystal, comprising the doped laser crystal as the optical gain material, a heat sink, wherein the heat sink exhibits high thermal conductivity within a threshold, and being optically transparent within a threshold; the method comprising the steps of:
providing the doped laser crystal with a surface roughness below 1 nm root-mean square;
providing the transparent heat sink with a surface roughness below 1 nm root-mean square;
attaching the laser-crystal based optical gain material to the heat sink by direct bonding.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the laser active medium further comprises a high reflectivity thin-film stack, wherein the optical gain material is combined with the high reflectivity thin-film stack; wherein the optical gain material comprises a semiconductor structure or a doped laser crystal.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the optical gain material is directly attached to the heat sink by van der Waals forces and/or covalent bonding.

### Claim 14 (depends on 1)

A solid-state laser system comprising: at least two mirrors for laser feedback; a laser active medium according to claim 1; and a pump light source providing a pump beam, the pump beam being incident on the laser active medium.

### Claim 15 (depends on 1)

The laser active medium according to claim 1, wherein the heat sink is transparent over a wavelength range of 200 nm to 4000 nm, and wherein the heat sink thermal conductivity is greater than or equal to 149 W/m*K.

### Claim 16 (depends on 15)

The laser active medium according to claim 15, wherein the heat sink has an absorption coefficient of <1 cm-1.

### Claim 17 (depends on 8)

The laser active medium according to claim 8, wherein the direct bonding of the optical gain material to the transparent heat sink comprises van der Waals forces and/or covalent bonding.

### Claim 18 (depends on 10)

The method of manufacturing a laser active medium according to claim 10, wherein the heat sink is optically transparent over a wavelength range of 200 nm to 4000 nm, and wherein the heat sink thermal conductivity is greater than or equal to 149 W/m*K.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the heat sink has an absorption coefficient of <1 cm-1.

### Claim 20 (depends on 11)

The method of manufacturing a laser active medium according to claim 11, wherein the heat sink is optically transparent over a wavelength range of 200 nm to 4000 nm, and wherein the heat sink thermal conductivity is greater than or equal to 149 W/m*K.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the heat sink has an absorption coefficient of <1 cm-1.

### Claim 22 (depends on 13)

The method according to claim 13, wherein the direct bonding of the optical gain material to the transparent heat sink comprises van der Waals forces and/or covalent bonding.