# US 2017/0256794 A1 · Nickel-lithium metal composite oxide powder and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256794 A1
- Document ID: US20170256794A1
- Status: Published application
- Kind: A1
- Application number: 15/505,073
- Filed: 2015-08-20
- Published: 2017-09-07
- Earliest claimed: 2014-08-28
- Assignees: CS Energy Materials Ltd.
- Applicants: CS Energy Materials Ltd.
- Inventors: Hiroshi TANI; Ralph OTTERSTEDT
- Web page: https://patentgrep.com/patent/US20170256794A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- B22F 9/02: using physical processes
- B22F 9/16: using chemical processes
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01M 4/02: Electrodes composed of, or comprising, active material
- B22F 2301/054: Alkali metals, i.e. Li, Na, K, Rb, Cs, Fr
- B22F 2301/15: Nickel or cobalt
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

To show an LNCAO-type positive electrode active material for a lithium ion battery having a high discharge capacity per unit volume and excellent discharging capacity-holding properties. Nickel-lithium metal composite oxide powder includes a nickel-lithium metal composite oxide represented by General Formula (1) described below: LixNi1-y-zMyNzO1.7-2.2 (1), in which the breakdown strength of secondary particles is in a range of 80 MPa or less, the density is 3.30 g/cm3 or higher when compressed at a pressure of 192 MPa, and the density is 3.46 g/cm3 or higher when compressed at a pressure of 240 MPa. A method for producing the nickel-lithium metal composite oxide powder includes a water washing step after a firing step for producing a nickel-lithium metal composite oxide powder precursor.

## Claims

### Claim 1

Nickel-lithium metal composite oxide powder comprising:
a nickel-lithium metal composite oxide represented by General Formula (1) described below:
LixNi1-y-zMyNzO1.7-2.2 (1)
in Formula (1), M represents one or more metal elements selected from a group consisting of Co, Mn, Fe, and Cu, N represents one or more metal elements selected from a group consisting of Al, W, Ta, and B, 0.90<x<1.10, 0.01<y<0.15, and 0.005<z<0.10,
wherein the breakdown strength of secondary particles is in a range of 80 MPa or less,
the density is 3.30 g/cm3 or higher when compressed at a pressure of 192 MPa, and
the density is 3.46 g/cm3 or higher when compressed at a pressure of 240 MPa.

### Claim 2 (depends on 1)

The nickel-lithium metal composite oxide powder according to claim 1,
wherein, when 2 g of the nickel-lithium metal composite oxide represented by General Formula (1) is dispersed in 100 g of water, a supernatant has a hydrogen ion concentration of 11.0 or lower in terms of pH and has a content of LiOH of 0.1% by weight or less.

### Claim 3 (depends on 1)

The nickel-lithium metal composite oxide powder according to claim 1,
wherein M in General Formula (1) is Co.

### Claim 4 (depends on 1)

The nickel-lithium metal composite oxide powder according to claim 1,
wherein N in General Formula (1) is Al.

### Claim 5 (depends on 1)

The nickel-lithium metal composite oxide powder according to claim 1,
wherein, in General Formula (1), M is Co, and N is Al.

### Claim 6 (depends on 1)

A positive electrode active material for a lithium ion battery, comprising:
the nickel-lithium metal composite oxide powder according to claim 1.

### Claim 7 (depends on 6)

A positive electrode for a lithium ion battery,
wherein the positive electrode active material for a lithium ion battery according to claim 6 is used.

### Claim 8 (depends on 7)

A lithium ion battery,
wherein the positive electrode for a lithium ion battery according to claim 7 is used.

### Claim 9

A method for producing nickel-lithium metal composite oxide powder including a nickel-lithium metal composite oxide represented by General Formula (1) described below:
LixNi1-y-zMyNzO1.7-2.2 (1)
in Formula (1), M represents one or more metal elements selected from a group consisting of Co, Mn, Fe, and Cu, N represents one or more metal elements selected from a group consisting of Al, W, Ta, and B, 0.90<x<1.10, 0.01<y<0.15, and 0.005<z<0.10,
wherein the breakdown strength of secondary particles is in a range of 80 MPa or less,
the density is 3.30 g/cm3 or higher when compressed at a pressure of 192 MPa, and
the density is 3.46 g/cm3 or higher when compressed at a pressure of 240 MPa, comprising:
a water washing step after a firing step for producing a nickel-lithium metal composite oxide powder precursor.

### Claim 10 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein, when 2 g of the obtained nickel-lithium metal composite oxide powder is dispersed in 100 g of water, a supernatant has a hydrogen ion concentration of 11.0 or lower in terms of pH and has a content of LiOH of 0.1% by weight or less.

### Claim 11 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein M in General Formula (1) is Co.

### Claim 12 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein N in General Formula (1) is Al.

### Claim 13 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein, in General Formula (1), M is Co, and N is Al.

### Claim 14 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein, in the water washing step, the nickel-lithium metal composite oxide is washed with water having a weight that is 10% to 300% of the weight of the nickel-lithium metal composite oxide.

### Claim 15 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein, in the water washing step, the nickel-lithium metal composite oxide is washed with water having a weight that is 50% to 100% of the weight of the nickel-lithium metal composite oxide.

### Claim 16 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9, further comprising:
a dehydration step after the water washing step.

### Claim 17 (depends on 16)

The method for producing nickel-lithium metal composite oxide powder according to claim 16,
wherein, in the dehydration step, dehydration through filtration is carried out.

### Claim 18 (depends on 16)

The method for producing nickel-lithium metal composite oxide powder according to claim 16,
wherein, in the dehydration step, dehydration through filtration and vacuum drying are carried out.

### Claim 19 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9, further comprising:
the dehydration step after the water washing step and a firing step after the dehydration step.

### Claim 20 (depends on 9)

The method for producing nickel-lithium metal composite oxide powder according to claim 9,
wherein the firing step for producing a nickel-lithium metal composite oxide powder precursor is carried out after a powder-mixing step coming after a dissolution step, a precipitation step, a filtration and washing step, and a drying step of a raw material.