# US 2017/0256776 A1 · Nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256776 A1
- Document ID: US20170256776A1
- Status: Published application
- Kind: A1
- Application number: 15/508,765
- Filed: 2015-09-02
- Published: 2017-09-07
- Earliest claimed: 2014-09-08
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Hideyuki SAKA; Keiichi TAKAHASHI; Hideaki FUJITA; Tatsuya HASHIMOTO
- Web page: https://patentgrep.com/patent/US20170256776A1

## CPC

- H01M 50/578: in response to pressure
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/052: Li-accumulators
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 2004/028: {Positive electrodes}
- H01M 2200/20: Pressure-sensitive devices
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode mixture layer (12) includes a first layer (12a) that has a main surface MS and a second layer (12b) formed closer to the positive electrode current collector (11) side than the first layer (12a). A ratio of the volume of the first layer (12a) to the volume of the positive electrode mixture layer (12) is 20 to 75 vol %. The first layer (12a) contains lithium iron phosphate (LFP) (1) and lithium nickel cobalt manganese composite oxide (NCM) (2). A ratio of the mass of the LFP (1) to the total mass of the LFP (1) and the NCM (2) in the first layer (12a) is more than 0 and 80 mass % or less. The second layer (12b) contains NCM (2). A ratio of the mass of the LFP (1) to the total mass of the positive electrode active material in the positive electrode mixture layer (12) is 7.5 to 20 mass %. A maximum pore size of the first layer (12a) is 0.50 to 0.70 μm.

## Claims

### Claim 1

A nonaqueous electrolyte secondary battery comprising:
a pressure-operated current interrupt device;
a nonaqueous electrolytic solution containing a gas producing agent; and
an electrode group in which a positive electrode and a negative electrode are arranged to face each other with a separator interposed between the positive electrode and the negative electrode, wherein
the positive electrode includes a positive electrode current collector and a positive electrode mixture layer that has a main surface and is formed on the positive electrode current collector,
the positive electrode mixture layer includes a first layer that includes the main surface and a second layer that is formed closer to the positive electrode current collector side than the first layer,
a ratio of a volume of the first layer to a volume of the positive electrode mixture layer is 20 vol % to 75 vol %,
the first layer contains lithium iron phosphate and lithium nickel cobalt manganese composite oxide,
a ratio of a mass of the lithium iron phosphate to a total mass of the lithium iron phosphate and the lithium nickel cobalt manganese composite oxide in the first layer is more than 0 mass % and 80 mass % or less,
the second layer contains lithium nickel cobalt manganese composite oxide,
a ratio of the mass of the lithium iron phosphate to a total mass of a positive electrode active material in the positive electrode mixture layer is 7.5 mass % to 20 mass %, and
a maximum pore size of the first layer is 0.50 μm to 0.70 μm.

### Claim 2 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
a BET specific surface area of the lithium iron phosphate is 8.6 m2/g to 13.2 m2/g.

### Claim 3 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
a ratio of a mass of a conductive material to a mass of the first layer is 5 mass % to 15 mass %.

### Claim 4 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
a ratio of the mass of a conductive material to a mass of the second layer is 3 mass % to 11 mass %.

### Claim 5 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
a mixture density of the positive electrode mixture layer is 2.5 g/cm3 to 3.5 g/cm3.