# US 2017/0256677 A1 · Method for manufacturing nitride semiconductor template

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256677 A1
- Document ID: US20170256677A1
- Status: Published application
- Kind: A1
- Application number: 15/511,886
- Filed: 2015-07-08
- Published: 2017-09-07
- Earliest claimed: 2014-09-17
- Assignees: Sumitomo Chemical Company, Limited
- Applicants: Sumitomo Chemical Company, Limited
- Inventors: Hajime FUJIKURA
- Web page: https://patentgrep.com/patent/US20170256677A1

## CPC

- H10H 20/82: Roughened surfaces, e.g. at the interface between epitaxial layers
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/24: Vacuum evaporation
- C30B 23/025: {characterised by the substrate}
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 29/406: {Gallium nitride}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H 20/825: containing nitrogen, e.g. GaN
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/2925: {Surface structures}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

There is provided a method for manufacturing a nitride semiconductor template, including the steps of: growing and forming a buffer layer to be thicker than a peak width of a projection and in a thickness of not less than 11 nm and not more than 400 nm on a sapphire substrate formed by arranging conical or pyramidal projections on its surface in a lattice pattern; and growing and forming a nitride semiconductor layer on the buffer layer.

## Claims

### Claim 1

A method for manufacturing a nitride semiconductor template, comprising the steps of:
growing and forming a buffer layer to be thicker than a peak width of a projection and in a thickness of not less than 11 nm and not more than 400 nm on a sapphire substrate formed by arranging conical or pyramidal projections on its surface in a lattice pattern; and
growing and forming a nitride semiconductor layer on the buffer layer.

### Claim 2 (depends on 1)

The method for manufacturing a nitride semiconductor template according to claim 1, wherein in the step of growing and forming the buffer layer, a GaN layer or an AlN layer is grown as the buffer layer at a temperature of 600° C. or less.

### Claim 3 (depends on 1)

The method for manufacturing a nitride semiconductor template according to claim 1, wherein in the step of growing and forming the buffer layer, an AlN layer is grown as the buffer layer at a temperature of 1000° C. or more.

### Claim 4 (depends on 1)

The method for manufacturing a nitride semiconductor template according to claim 1, wherein in the step of growing and forming the nitride semiconductor layer, any one of a GaN layer, an AlGaN layer, and an InAlGaN layer is grown and formed as the nitride semiconductor layer.

### Claim 5 (depends on 1)

The method for manufacturing a nitride semiconductor template according to claim 1, wherein the buffer layer and the nitride semiconductor layer are grown by a HYPE method or a MOVPE method.