# US 2017/0256671 A1 · Avalanche photodiode with low breakdown voltage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256671 A1
- Document ID: US20170256671A1
- Status: Published application
- Kind: A1
- Application number: 15/442,512
- Filed: 2017-02-24
- Published: 2017-09-07
- Earliest claimed: 2013-06-26
- Assignees: Intel Corporation
- Applicants: Intel Corporation
- Inventors: Yimin Kang; Han-Din Liu
- Web page: https://patentgrep.com/patent/US20170256671A1

## CPC

- H10F 30/2255: {in which the active layers form heterostructures, e.g. SAM structures}
- G02B 6/42: Coupling light guides with opto-electronic elements
- H10F 77/959: {for devices working in avalanche mode}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

An Si/Ge SACM avalanche photodiodes (APD) having low breakdown voltage characteristics includes an absorption region and a multiplication region having various layers of particular thicknesses and doping concentrations. An optical waveguide can guide infrared and/or optical signals or energy into the absorption region. The resulting photo-generated carriers are swept into the i-Si layer and/or multiplication region for avalanche multiplication. The APD has a breakdown bias voltage of well less than 12 V and an operating bandwidth of greater than 10 GHz, and is therefore suitable for use in consumer electronic devices, high speed communication networks, and the like.

## Claims

### Claim at position 1

1-21. (canceled)

### Claim 22

A semiconductor avalanche photodiode (APD), comprising:
a first region that includes n-type doped silicon;
a second region disposed on the first region, wherein the second region includes silicon, and wherein a thickness of the second region is between about 0.07 micrometers and about 0.13 micrometers;
a third region disposed on the second region, wherein the third region includes p-type doped silicon; and
a fourth region disposed on the third region, wherein the fourth region includes germanium.

### Claim 23 (depends on 22)

The APD of claim 22, further comprising:
a substrate, wherein the first region, the second region, the third region, and the fourth region are formed on the substrate.

### Claim 24 (depends on 22)

The APD of claim 22, further comprising:
a fifth region disposed on the fourth region, wherein the fifth region includes p-type doped material.

### Claim 25 (depends on 22)

The APD of claim 22, wherein the thickness of the second region is about 100 nanometers.

### Claim 26 (depends on 22)

The APD of claim 22, wherein the second region has a doping concentration of less than about 5×1015 centimeters−3 (cm−3).

### Claim 27 (depends on 22)

The APD of claim 22, wherein the third region has a doping concentration of between about 2×1018 centimeters−3 (cm−3) and about 3×1018 cm−3.

### Claim 28 (depends on 22)

The APD of claim 22, wherein the second region is disposed directly on the first region, wherein the third region is disposed directly on the second region, and wherein the fourth region is disposed directly on the third region.

### Claim 29 (depends on 22)

The APD of claim 22, wherein the second region is doped differently than the first region and the third region.

### Claim 30 (depends on 22)

The APD of claim 22, wherein the APD is a group-IV APD.

### Claim 31 (depends on 22)

The APD of claim 22, wherein a thickness of the third region is about 20 nanometers.

### Claim 32 (depends on 24)

The APD of claim 24, further comprising:
a metal contact disposed on the fifth region.

### Claim 33

A semiconductor avalanche photodiode (APD), comprising:
a first region that includes n-type doped silicon;
a second region disposed on the first region, wherein the second region includes silicon, and wherein the second region has a doping concentration of less than about 5×1015 centimeter−3 (cm−3);
a third region disposed on the second region, wherein the third region includes p-type doped silicon, and wherein the third region has a doping concentration of between about 2×1018 cm−3 and about 3×1018 cm−3; and
a fourth region disposed on the third region, wherein the fourth region includes germanium.

### Claim 34 (depends on 33)

The APD of claim 33, wherein the second region has a thickness of between about 0.07 micrometers and about 0.13 micrometers.

### Claim 35 (depends on 34)

The APD of claim 34, wherein the thickness of the second region is about 100 nanometers.

### Claim 36 (depends on 33)

The APD of claim 33, further comprising:
a substrate, wherein the first region, the second region, the third region, and the fourth region are formed on the substrate.

### Claim 37 (depends on 33)

The APD of claim 33, wherein the third region has a thickness of about 20 nanometers.

### Claim 38 (depends on 33)

The APD of claim 33, further comprising:
a fifth region disposed on the fourth region, wherein the fifth region includes p-type doped material.

### Claim 39 (depends on 38)

The APD of claim 38, further comprising:
a metal contact disposed on the fifth region.

### Claim 40 (depends on 39)

The APD of claim 39, wherein the metal contact is a first metal contact, and wherein the APD further comprises:
a second metal contact disposed on the first region.

### Claim 41 (depends on 33)

The APD of claim 33, wherein the second region is doped differently than the first region and the third region.