# US 2017/0256605 A1 · Method for fabricating electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256605 A1
- Document ID: US20170256605A1
- Status: Published application
- Kind: A1
- Application number: 15/599,743
- Filed: 2017-05-19
- Published: 2017-09-07
- Earliest claimed: 2014-01-14
- Assignees: Sumitomo Electric Device Innovations, Inc.
- Applicants: Sumitomo Electric Device Innovations, Inc.
- Inventors: Yasunori Nonaka
- Web page: https://patentgrep.com/patent/US20170256605A1

## CPC

- H10D 1/694: {comprising noble metals or noble metal oxides}
- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/496: {Capacitor integral with wiring layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating an electronic device is provided, and the method comprises the steps of: forming a lower electrode on a substrate; forming a dielectric film on the lower electrode; forming an upper electrode on the dielectric film, the upper electrode including gold (Au); forming a refractory metal layer on at least one of upper or lower surface of the upper electrode, the refractory metal layer having a melting temperature higher than a melting temperature of the upper electrode; forming an insulating film to cover the lower electrode, the dielectric film, the upper electrode, and the refractory metal layer; and dry-etching the insulating film to form an opening therein, the upper electrode or the refractory metal layer being exposed at the opening.

## Claims

### Claim at position 1

-12. (canceled)

### Claim 13

A method for fabricating an electronic device, comprising steps of:
forming a lower electrode on a substrate;
forming a dielectric film on the lower electrode;
forming an upper electrode on the dielectric film, the upper electrode including gold (Au);
forming an insulating film so as to cover the lower electrode, the dielectric film, and the upper electrode;
heat-treating the insulating film at a temperature not lower than 250° C.; and
dry-etching the insulating film to form an opening, the opening exposing the upper electrode therein,
wherein the upper electrode has an upper surface and a lower surface, and includes a refractory metal layer on at least one of the upper surface and the lower surface thereof.

### Claim 14 (depends on 13)

The method of claim 13,
wherein the insulating film is made of polyimide, and
wherein the step of heat-treating the insulating film includes a step of curing the polyimide at a temperature not lower than 350° C.

### Claim 15 (depends on 13)

The method of claim 13,
wherein the step of forming the upper electrode includes steps of, forming the refractory metal layer so as to be in contact to the dielectric film and fully cover the dielectric film, then,
forming the gold (Au) on the refractory metal layer.

### Claim 16 (depends on 13)

The method of claim 13,
wherein the step of forming the upper electrode includes steps of,
forming the gold (Au) so as to be in contact to the dielectric film, then,
forming the refractory metal layer so as to fully cover the gold (Au).

### Claim 17 (depends on 13)

The method of claim 13,
wherein the dielectric film is made of silicon nitride (SiN),and
wherein the step of forming the dielectric film includes a step of forming the SiN film by chemical vapor deposition (CVD).

### Claim 18 (depends on 13)

The method of claim 13,
wherein the step of dry-etching the insulating film includes a step of forming the opening fully overlapped with the refractory metal layer.

### Claim 19 (depends on 13)

The method of claim 13,
wherein the refractory metal layer has a melting temperature higher than a melting temperature of the gold (Au) in the upper electrode.

### Claim 20 (depends on 19)

The method of claim 19,
wherein the refractory metal layer includes at least one of titanium (Ti), platinum (Pt), tantalum (Ta), molybdenum (Mo), and tungsten (W).

### Claim 21 (depends on 19)

The method of claim 19,
wherein the refractory metal layer has thickness of not thinner than 50 nm.

### Claim 22

A method for forming a metal-insulator-metal (MIM) capacitor on a semiconductor substrate, comprising steps of:
forming a lower electrode on the semiconductor substrate;
forming a dielectric film made of silicon nitride (SiN) on the lower electrode, the dielectric film fully overlapping with the lower electrode;
forming an upper electrode on the dielectric film, the upper electrode including gold (Au);
forming an insulating film on the upper electrode;
recrystallizing the upper electrode by heat-treating the insulating film at a temperature not lower than 250° C. to from gold clusters as leaving gaps therebetween; and
dry-etching the insulating film so as to expose the upper electrode using a gas containing fluorine,
wherein the step of forming the upper electrode includes a step of forming a refractory metal layer in at least one of a bottom in contact to the dielectric layer and a top to be in contact to the insulating film, and
wherein the heat-treatment of the insulating film forms substantially no clusters in the refractory metal layer.

### Claim 23 (depends on 22)

The method of claim 22,
wherein the step of forming the insulating film includes a step of spin-coating a polyimide film.

### Claim 24 (depends on 23)

The method of claim 23,
wherein the step of re-crystallizing the upper electrode includes a step of curing the polyimide film at a temperature not lower than 350° C.

### Claim 25 (depends on 23)

The method of claim 23,
wherein the refractory metal layer has a melting temperature higher than a melting temperature of the gold (Au) in the upper electrode.

### Claim 26 (depends on 25)

The method of claim 25,
wherein the refractory metal layer includes at least one of titanium (Ti), platinum (Pt), tantalum (Ta), molybdenum (Mo), and tungsten (W).

### Claim 27 (depends on 25)

The method of claim 25,
wherein the refractory metal layer has thickness of not thinner than 50 nm.

### Claim 28 (depends on 23)

The method of claim 23,
wherein the step of dry-etching the insulating film includes a step of forming an opening in the insulating film, the opening exposing the upper electrode therein and fully overlapping with the upper electrode.