# US 2017/0256545 A1 · Method of manufacturing semiconductor integrated circuit device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256545 A1
- Document ID: US20170256545A1
- Status: Published application
- Kind: A1
- Application number: 15/598,670
- Filed: 2017-05-18
- Published: 2017-09-07
- Earliest claimed: 2015-02-25
- Assignees: Sii Semiconductor Corporation
- Applicants: SII Semiconductor Corporation
- Inventors: Hirofumi HARADA; Keisuke UEMURA; Hisashi HASEGAWA; Shinjiro KATO; Hideo YOSHINO
- Web page: https://patentgrep.com/patent/US20170256545A1

## CPC

- H10D 84/856: {the complementary IGFETs having different architectures than each other, e.g. high-voltage and low-voltage CMOS}
- H10D 30/0221: {having asymmetry in the channel direction, e.g. lateral high-voltage MISFETs having drain offset region or extended-drain MOSFETs [EDMOS]}
- H10D 30/603: {having asymmetry in the channel direction, e.g. lateral high-voltage MISFETs having drain offset region or extended drain IGFETs [EDMOS]}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0172: {Manufacturing their gate conductors}
- H10D 84/0191: {Manufacturing their doped wells}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/83138: {the IGFETs characterised by having different shapes or dimensions of their gate conductors}
- H10D 84/8314: {the IGFETs characterised by having gate insulating layers with different properties}
- H10D 84/859: {comprising both N-type and P-type wells, e.g. twin-tub}
- H10D 89/811: {using FETs as protective elements}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 62/116: {adjoining the input or output regions of field-effect devices, e.g. adjoining source or drain regions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a semiconductor integrated circuit device including a first N-channel type high withstanding-voltage MOS transistor and a second N-channel type high withstanding-voltage MOS transistor formed on an N-type semiconductor substrate, the first N-channel type high withstanding-voltage transistor including a third N-type low-concentration impurity region containing arsenic having a depth smaller than a P-type well region in a drain region within the P-type well region, and the second N-channel type high withstanding-voltage MOS transistor including a fourth N-type low-concentration impurity region that is adjacent to the P-type well region and has a bottom surface being in contact with the N-type semiconductor substrate. In this manner, the high withstanding-voltage NMOS transistors capable of operating at 30 V or higher are integrated on the N-type semiconductor substrate.

## Claims

### Claim 1

A method of manufacturing a semiconductor integrated circuit device, comprising:
an N-type well layer formation step of forming a silicon oxide film and a silicon nitride film on an N-type semiconductor substrate, forming an opening through the silicon nitride film present on a region for forming an N-type well layer so as to form a silicon nitride film opening portion, and implanting an N-type impurity comprising phosphorous by an ion implantation;
a P-type well layer formation step of forming a silicon oxide film on the silicon nitride film opening portion and implanting a P-type impurity comprising one of boron and BF2 into a region other than the region for forming the N-type well layer, from which the silicon nitride film is removed, by the ion implantation in a self-aligned manner;
a third N-type low-concentration impurity layer formation step of implanting an N-type impurity comprising arsenic into a region for forming a third N-type low-concentration impurity layer, by the ion implantation;
a well diffusion step of simultaneously forming the N-type well layer, a P-type well layer, and the third N-type low-concentration impurity layer by a thermal treatment;
a second N-type low-concentration impurity layer formation step of forming a silicon oxide film and a silicon nitride film, forming an opening through the silicon nitride film present on a region for forming a second N-type low-concentration impurity region of a high withstanding-voltage NMOS transistor, and implanting an N-type impurity comprising phosphorous by the ion implantation;
a step of forming a silicon oxide film on the region for forming the second N-type low-concentration impurity layer in the silicon nitride film opening portion, to thereby form an insulating film for electric field relaxation between a gate and a drain of the high withstanding-voltage NMOS transistor;
a gate insulating film formation step of forming a gate insulating film of a low withstanding-voltage NMOS transistor, a low withstanding-voltage PMOS transistor, and the high withstanding-voltage NMOS transistor;
a gate electrode formation step of forming a gate electrode on the gate insulating film;
a first N-type low-concentration impurity layer formation step of implanting phosphorus into a region for forming a drain of the low withstanding-voltage NMOS transistor and a region for forming a source of the low withstanding-voltage NMOS transistor;
a P-type low-concentration impurity layer formation step of implanting one of boron and BF2 into a region for forming a drain of the low withstanding-voltage PMOS transistor and a region for forming a source of the low withstanding-voltage PMOS transistor; and
a high-concentration drain/source layer formation step of forming an N-type low-concentration impurity layer containing arsenic in each of the region for forming the drain and the region for forming the source of the low withstanding-voltage NMOS transistor and the region for forming the drain and the region for forming the source of the high withstanding-voltage NMOS transistor, and forming a P-type impurity layer containing BF2 in the region for forming the drain of the low withstanding-voltage PMOS transistor and the region for forming the source of the low withstanding-voltage PMOS transistor.

### Claim 2

A method of manufacturing a semiconductor integrated circuit device, comprising:
an N-type well layer formation step of forming a silicon oxide film and a silicon nitride film on an N-type semiconductor substrate, forming an opening through the silicon nitride film present on a region for forming an N-type well layer so as to form a silicon nitride film opening portion, and implanting an N-type impurity comprising phosphorous by an ion implantation;
a first P-type well layer formation step of forming a silicon oxide film on the silicon nitride film opening portion and implanting a P-type impurity comprising one of boron and BF2 into a region other than the region for forming the N-type well layer, from which the silicon nitride film is removed, by the ion implantation in a self-aligned manner;
a third N-type low-concentration impurity layer formation step of peeling off the silicon nitride film, forming another silicon nitride film, forming an opening through the silicon nitride film present on a region for forming a third N-type low-concentration impurity layer, implanting an N-type impurity comprising arsenic by the ion implantation;
a second P-type well layer formation step of forming a silicon oxide film on the silicon nitride film opening portion, and implanting a P-type impurity comprising one of boron and BF2 into a region other than the region for forming the third N-type low-concentration impurity layer and the region for forming the N-type well layer on the N-type semiconductor substrate, from which the silicon nitride film is removed, by the ion implantation in a self-aligned manner;
a well diffusion step of simultaneously forming an N-type well layer, a first P-type well layer, a second P-type well layer, and the third N-type low-concentration impurity layer by a thermal treatment;
a second N-type low-concentration impurity layer formation step of forming a silicon oxide film and a silicon nitride film, forming an opening through the silicon nitride film present on a region for forming a second N-type low-concentration impurity region of a high withstanding-voltage NMOS transistor, and implanting an N-type impurity comprising phosphorous by the ion implantation;
a step of forming a silicon oxide film on the region for forming the second N-type low-concentration impurity layer in the silicon nitride film opening portion, to thereby form an insulating film for electric field relaxation between a gate and a drain of the high withstanding-voltage NMOS transistor;
a gate insulating film formation step of forming a gate insulating film of a low withstanding-voltage NMOS transistor, a low withstanding-voltage PMOS transistor, and the high withstanding-voltage NMOS transistor;
a gate electrode formation step of forming a gate electrode on the gate insulating film;
a first N-type low-concentration impurity layer formation step of implanting phosphorus into a region for forming a drain of the low withstanding-voltage NMOS transistor and a region for forming a source of the low withstanding-voltage NMOS transistor;
a P-type low-concentration impurity layer formation step of implanting one of boron and BF2 into a region for forming a drain of the low withstanding-voltage PMOS transistor and a region for forming a source of the low withstanding-voltage PMOS transistor; and
a high-concentration drain/source layer formation step of forming an N-type low-concentration impurity layer containing arsenic in each of the region for forming the drain and the region for forming the source of the low withstanding-voltage NMOS transistor and the region for forming the drain and the region for forming the source of the high withstanding-voltage NMOS transistor, and forming a P-type impurity layer containing BF2 in the region for forming the drain of the low withstanding-voltage PMOS transistor and the region for forming the source of the low withstanding-voltage PMOS transistor.

### Claim 3 (depends on 2)

A method of manufacturing a semiconductor integrated circuit device according to claim 2, wherein:
an impurity dose amount in the N-type well layer formation step is from 3×1012/cm2 to 3×1013/cm2;
an impurity dose amount in the first P-type well layer formation step is from 2×1012/cm2 to 2×1013/cm2;
an impurity dose amount in the second P-type well layer formation step is from 5×1012/cm2 to 2×1013/cm2;
an impurity dose amount in the third N-type low-concentration impurity layer formation step is from 8×1012/cm2 to 7×1013/cm2;
an impurity dose amount in the second N-type low-concentration impurity layer formation step is from 1×1012/cm2 to 7×1013/cm2;
an impurity dose amount in the first N-type low-concentration impurity layer formation step is from 2×1012/cm2 to 2×1014/cm2;
an impurity dose amount in the P-type low-concentration impurity layer formation step is from 2×1012/cm2 to 2×1014/cm2; and
a dose amount of the N-type impurity and a dose amount of the P-type impurity in the high-concentration drain/source layer formation step are 2×1015/cm2 or larger.