# US 2017/0256422 A1 · Method for introducing at least one cutout or aperture into a sheetlike workpiece

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256422 A1
- Document ID: US20170256422A1
- Status: Published application
- Kind: A1
- Application number: 15/511,272
- Filed: 2015-08-07
- Published: 2017-09-07
- Earliest claimed: 2014-09-16
- Assignees: Lpkf Laser & Electronics AG
- Applicants: LPKF Laser & Electronics AG
- Inventors: Norbert Ambrosius; Roman Ostholt
- Web page: https://patentgrep.com/patent/US20170256422A1

## CPC

- H10W 70/095: {of vias therein}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/382: by boring
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/0025: {by a laser beam}
- H05K 3/0029: {of inorganic insulating material}
- H10W 70/635: {Through-vias}
- B23K 2101/40: Semiconductor devices
- B23K 2103/54: {Glass}
- H05K 3/0017: {Etching of the substrate by chemical or physical means}
- H10W 70/692: Ceramics or glasses
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A method for introducing at least one cutout, in particular in the form of an aperture, into a sheetlike workpiece having a thickness of less than 3 mm, involving detecting a laser beam onto the surface of the workpiece, selecting the exposure time of the laser beam to be extremely short so that only a modification of the workpiece concentrically around a beam axis of the laser beam occurs, such a modified region having defects resulting in a chain of blisters, and, as a result of the action of a corrosive medium, anisotropically removing material by successive etching in those regions of the workpiece that are formed by the defects and have previously been modified by the laser beam, resulting, along the cylindrical zone of action, in producing a cutout as an aperture in the workpiece.

## Claims

### Claim 1

A method for making a recess and/or an opening in a planar workpiece having a thickness of less than 3 mm, the method comprising:
etching a result of a plurality of successive flaws one after the other, thereby allowing the making of the recess and/or opening.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
arranging the flaws along a line.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
making the flaws so as to deviate from a straight line in at least some portions.

### Claim 4 (depends on 1)

The method of claim 1, wherein the flaws do not touch.

### Claim 5 (depends on 1)

The method of claim 1, wherein the flaws extend along an axis from one surface as far as to a second surface.

### Claim 6 (depends on 1)

The method of claim 1, wherein an average thickness of the workpiece is reduced by the etching.

### Claim 7 (depends on 1)

The method of claim 1, comprising:
producing the flaws by a reaction with laser radiation.

### Claim 8 (depends on 7)

The method of claim 7, wherein the laser radiation has a wavelength to which a material of the workpiece is largely transparent.

### Claim 9 (depends on 7)

The method of claim 7, wherein the laser radiation has a pulse length of less than 100 picoseconds.

### Claim 10 (depends on 7)

The method of claim 7, wherein the laser radiation in form of a pulse reacts with a material of the workpiece.

### Claim 11 (depends on 7)

The method of claim 7, comprising:
reacting the laser radiation in form of a pulse sequence with a material of the workpiece, the pulse sequence including no more than 20 individual pulses.

### Claim 12 (depends on 7)

The method of claim 7, wherein a focus of the laser radiation travels through the workpiece along a beam axis with a time lag.

### Claim 13 (depends on 7)

The method of claim 7, comprising:
reacting a focus of the laser radiation along a beam axis over an entire thickness of a material of the workpiece using a spatial beam shape.

### Claim 14 (depends on 7)

The method of claim 7, comprising:
achieving a spatial beam shape by an optical system having high spherical aberration or by a diffractive optical element.

### Claim 15 (depends on 7)

The method of claim 7, wherein a difference between focal point layers of paraxial beams and edge beams of a laser beam along a beam axis is >100 μm.

### Claim 16 (depends on 1)

The method of claim 1, wherein a lateral surface of the recess or opening forms an earthworm structure.

### Claim 17 (depends on 1)

The method of claim 1, wherein a material of the workpiece includes a significant content of glass, silicon, and/or sapphire.

### Claim 18 (depends on 2)

The method of claim 2, wherein the line is an axis or a straight line.

### Claim 19 (depends on 7)

The method of claim 7, wherein the laser radiation has a pulse length of less than 12 picoseconds.

### Claim 20 (depends on 7)

The method of claim 7, wherein a difference between focal point layers of paraxial beams and edge beams of a laser beam along a beam axis is >250 μm.