# US 2017/0256420 A1 · Thermal processing method for wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256420 A1
- Document ID: US20170256420A1
- Status: Published application
- Kind: A1
- Application number: 15/268,006
- Filed: 2016-09-16
- Published: 2017-09-07
- Earliest claimed: 2016-03-03
- Assignees: Zing Semiconductor Corporation
- Applicants: Zing Semiconductor Corporation
- Inventors: DEYUAN XIAO; RICHARD R. CHANG
- Web page: https://patentgrep.com/patent/US20170256420A1

## CPC

- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 95/94: {Hydrogenation or deuterisation, e.g. using atomic hydrogen from a plasma}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a thermal processing method for wafer. A wafer is placed in an environment filled with a non-oxygenated gas mixture comprising deuterium gas and at least one kind of low active gas, and a rapid heating processing process is performed on a surface of the wafer to heat the wafer to a predetermined high temperature. Then, the wafer is placed in an environment filled with an oxygenated gas mixture, and a rapid cooling processing process is performed on a surface of the wafer. As a result, a denuded zone is formed on the surface of the wafer, deuterium atoms, which may be released to improve characteristics at an interface of semiconductor devices in a later fabrication process, are held in the wafer, and bulk micro-defects are formed far from the semiconductor devices.

## Claims

### Claim 1

A thermal processing method for wafer, comprising:
placing at least one wafer in an environment filled with a non-oxygenated gas mixture comprising deuterium gas and at least one kind of low active gas, and performing a rapid heating process on a surface of the least one wafer to heat the least one wafer to a predetermined high temperature; and
after the least one wafer's reaching the predetermined high temperature, placing the least one wafer in an environment filled with an oxygenated gas mixture, and performing a rapid cooling process on a surface of the least one wafer.

### Claim 2 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the at least one kind of low active gas comprises argon gas and nitrogen gas.

### Claim 3 (depends on 2)

The thermal processing method for wafer as claim 2, wherein the gas partial pressure of the argon gas in the non-oxygenated gas mixture falls within 1% to 99%.

### Claim 4 (depends on 2)

The thermal processing method for wafer as claim 2, wherein the gas partial pressure of the nitrogen gas in the non-oxygenated gas mixture falls within 1% to 99%.

### Claim 5 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the gas partial pressure of the deuterium gas in the non-oxygenated gas mixture falls within 1% to 99%.

### Claim 6 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the predetermined high temperature falls within 1200° C. to 1400° C.

### Claim 7 (depends on 1)

The thermal processing method for wafer as claim 1, wherein in the rapid cooling process, the at least one wafer was cooled from the predetermined high temperature with a temperature gradient which falls within 50° C./sec to 150° C./sec.

### Claim 8 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the oxygenated gas mixture comprises oxygen gas, and the gas partial pressure of the oxygen gas in the oxygenated gas mixture falls within 10% to 100%.

### Claim 9 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the oxygenated gas mixture comprises oxygen gas and a kind of nitrogenated gas, the gas partial pressure of the oxygen gas in the oxygenated gas mixture falls within 1% to 99%, and the gas partial pressure of the nitrogenated gas in the oxygenated gas mixture falls within 1% to 99%.

### Claim 10 (depends on 1)

The thermal processing method for wafer as claim 1, wherein a concentration of a nitrogen solid solution in the at least one wafer falls within 1×1012 atom/cm3 to 8×1018 atom/cm3.

### Claim 11 (depends on 1)

The thermal processing method for wafer as claim 1, wherein a concentration of a deuterium solid solution in the at least one wafer falls within 1×1012 atom/cm3 to 8×1018 atom/cm3.

### Claim 12 (depends on 1)

The thermal processing method for wafer as claim 1, wherein a denuded zone is formed at a depth of 3 μm to 30 μm from a surface of the at least one wafer, and a plurality of bulk micro-defects are formed in a bulk zone which is under the denuded zone.

### Claim 13 (depends on 1)

The thermal processing method for wafer as claim 1, wherein the step of placing at least one wafer in an environment filled with a non-oxygenated gas mixture comprising deuterium gas and at least one kind of low active gas, and performing a rapid heating process on a surface of the least one wafer to heat the least one wafer to a predetermined high temperature was performed after forming the at least one wafer by slicing and before fabricating a structure of a plurality of semiconductor devices on the at least one wafer.