# US 2017/0256416 A1 · Atomic layer etching of al203 using a combination of plasma and vapor treatments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256416 A1
- Document ID: US20170256416A1
- Status: Published application
- Kind: A1
- Application number: 15/435,838
- Filed: 2017-02-17
- Published: 2017-09-07
- Earliest claimed: 2016-03-01
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Andreas Fischer; Thorsten Lill; Richard Janek; John Boniface
- Web page: https://patentgrep.com/patent/US20170256416A1

## CPC

- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- C23C 16/0245: {by etching with a plasma}
- C23F 1/00: Etching metallic material by chemical means (manufacture of printing surfaces B41C; manufacture of printed circuits H05K)
- C23F 1/12: Gaseous compositions
- C23F 4/00: Processes for removing metallic material from surfaces, not provided for in group C23F1/00 or C23F3/00
- H01J 37/32009: {Arrangements for generation of plasma specially adapted for examination or treatment of objects, e.g. plasma sources (plasma generation in general H05H1/24)}
- H01J 37/32082: {Radio frequency generated discharge (H01J37/32357, H01J37/32366, H01J37/32394 and H01J37/32403 take precedence)}
- H10P 50/244: {comprising alternated and repeated etching and passivation steps}
- H10P 50/267: {using plasmas}
- B81C 2201/0135: Controlling etch progression
- B81C 2201/0142: Processes for controlling etch progression not provided for in B81C2201/0136 - B81C2201/014
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)

## Abstract

A method for performing atomic layer etching (ALE) on a substrate, including the following method operations: performing a surface modification operation on a surface of the substrate, the surface modification operation configured to convert at least one monolayer of the substrate surface to a modified layer; performing a removal operation on the substrate surface, the removal operation configured to remove the modified layer from the substrate surface, wherein removing the modified layer occurs via a ligand exchange reaction that is configured to volatilize the modified layer; performing, following the removal operation, a plasma treatment on the substrate surface, the plasma treatment configured to remove residues generated by the removal operation from the substrate surface, wherein the residues are volatilized by the plasma treatment; repeating the foregoing operations until a predefined thickness has been etched from the substrate surface.

## Claims

### Claim 1

A method for performing atomic layer etching (ALE) on a substrate, comprising:
(a) performing a surface modification operation on a surface of the substrate, the surface modification operation configured to convert at least one monolayer of the substrate surface to a modified layer;
(b) performing a removal operation on the substrate surface, the removal operation configured to remove the modified layer from the substrate surface, wherein removing the modified layer occurs via a ligand exchange reaction that is configured to volatilize the modified layer;
(c) performing, following the removal operation, a plasma treatment on the substrate surface, the plasma treatment configured to remove residues generated by the removal operation from the substrate surface, wherein the residues are volatilized by the plasma treatment;
(d) repeating operations (a) through (c) until a predefined thickness has been etched from the substrate surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein performing the surface modification operation includes exposing the substrate surface to a fluorine-containing plasma, wherein the exposure to the fluorine-containing plasma is configured to convert the at least one monolayer of the substrate surface to a fluoride species.

### Claim 3 (depends on 2)

The method of claim 2,
wherein the surface of the substrate includes a metal, metal oxide, metal nitride, metal phosphide, metal sulfide, or metal arsenide;
wherein the exposure to the fluorine-containing plasma forms a metal fluoride.

### Claim 4 (depends on 2)

The method of claim 2, wherein exposing the surface of the substrate to the fluorine-containing plasma includes introducing a fluorine-containing gas into a chamber in which the substrate is disposed, and igniting a plasma.

### Claim 5 (depends on 4)

The method of claim 4, wherein the exposure to the fluorine-containing plasma is performed at a chamber pressure of about 10 to 500 mTorr, for a duration less than about 15 seconds.

### Claim 6 (depends on 2)

The method of claim 2, wherein performing the removal operation includes exposing the substrate surface to tin-(II) acetylacetonate (Sn(acac)2) vapor, the exposure to the Sn(acac)2 vapor being configured to exchange acac ligands for fluorine atoms in the modified layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein exposing the surface of the substrate to the Sn(acac)2 includes introducing the Sn(acac)2 as a vapor into a chamber in which the substrate is disposed.

### Claim 8 (depends on 7)

The method of claim 7, wherein the exposure to the Sn(acac)2 is performed for a duration of about 1 to 30 seconds.

### Claim 9 (depends on 6)

The method of claim 6, wherein performing the plasma treatment includes exposing the substrate surface to a hydrogen plasma, the exposure to the hydrogen plasma being configured to volatilize tin, tin fluoride or tin oxide residues on the surface of the substrate.

### Claim 10 (depends on 7)

The method of claim 7, wherein exposing the surface of the substrate to the hydrogen plasma includes introducing a hydrogen gas into a chamber in which the substrate is disposed, and igniting a plasma.

### Claim 11 (depends on 10)

The method of claim 10, wherein the exposure to the hydrogen plasma is performed for a duration of about 1 to 30 seconds.

### Claim 12 (depends on 1)

The method of claim 1,
wherein operation (a) is performed in a first chamber;
wherein operation (b) is performed in a second chamber.

### Claim 13 (depends on 12)

The method of claim 12, wherein operation (d) is performed in the first chamber.

### Claim 14 (depends on 12)

The method of claim 12, wherein operation (d) is performed in a third chamber.

### Claim 15

A method for performing atomic layer etching (ALE) on a substrate, comprising:
(a) performing a surface modification operation on a surface of the substrate, the surface modification operation configured to convert at least one monolayer of the substrate surface to a modified layer;
(b) performing a removal operation on the substrate surface, the removal operation configured to remove the modified layer from the substrate surface, wherein removing the modified layer occurs via a ligand exchange reaction that is configured to volatilize the modified layer;
(c) repeating operations (a) and (b) for a predefined number of cycles;
(d) performing, following operation (c), a plasma treatment on the substrate surface, the plasma treatment configured to remove residues generated by the removal operation from the substrate surface, wherein the residues are volatilized by the plasma treatment;
(e) repeating operations (a) through (d) until a predefined thickness has been etched from the substrate surface.

### Claim 16 (depends on 15)

The method of claim 15, wherein performing the surface modification operation includes exposing the substrate surface to a fluorine-containing plasma, wherein the exposure to the fluorine-containing plasma is configured to convert the at least one monolayer of the substrate surface to a fluoride species;
wherein performing the removal operation includes exposing the substrate surface to tin-(II) acetylacetonate (Sn(acac)2) vapor, the exposure to the Sn(acac)2 vapor being configured to exchange acac ligands for fluorine atoms in the modified layer;
wherein performing the plasma treatment includes exposing the substrate surface to a hydrogen plasma, the exposure to the hydrogen plasma being configured to volatilize tin, tin fluoride or tin oxide residues on the surface of the substrate.

### Claim 17 (depends on 16)

The method of claim 16,
wherein the surface of the substrate includes a metal, metal oxide, metal nitride, metal phosphide, metal sulfide, or metal arsenide;
wherein the exposure to the fluorine-containing plasma forms a metal fluoride.

### Claim 18 (depends on 16)

The method of claim 16,
wherein the exposure to the fluorine-containing plasma is performed at a chamber pressure of about 10 to 500 mTorr, for a duration less than about 15 seconds;
wherein the exposure to the Sn(acac)2 is performed for a duration of about 1 to 30 seconds;
wherein the exposure to the hydrogen plasma is performed for a duration of about 1 to 30 seconds.