# US 2017/0256410 A1 · Method and apparatus for depositing amorphous silicon film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256410 A1
- Document ID: US20170256410A1
- Status: Published application
- Kind: A1
- Application number: 15/598,799
- Filed: 2017-05-18
- Published: 2017-09-07
- Earliest claimed: 2013-10-21
- Assignees: Eugene Technology Co., Ltd.
- Applicants: Eugene Technology Co., Ltd.
- Inventors: Seung-Woo SHIN; Hai-Won KIM; Woo-Duck JUNG; Sung-Kil CHO; Wan-Suk OH; Ho-Min CHOI; Koon-Woo LEE
- Web page: https://patentgrep.com/patent/US20170256410A1

## CPC

- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- C23C 16/24: Deposition of silicon only
- C23C 16/4405: {Cleaning of reactor or parts inside the reactor by using reactive gases}
- C23C 16/45563: {Gas nozzles}
- H10D 64/0113: {the conductive layers comprising highly doped semiconductor materials, e.g. polysilicon layers or amorphous silicon layers}
- H10F 71/103: {including only Group IV materials}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3454: {Amorphous}
- H10P 14/416: {of highly doped semiconductor materials, e.g. polysilicon layers or amorphous silicon layers}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method and apparatus for depositing an amorphous silicon film. The method includes supplying a source gas and an atmospheric gas onto a substrate in a state where the substrate is loaded in a chamber to deposit the amorphous silicon film on the substrate. The atmospheric gas includes at least one of hydrogen and helium. The source gas includes at least one of silane (SiH2), disilane (Si2H6), and dichlorosilane (SiCl2H2).

## Claims

### Claim 1

A method for depositing an amorphous silicon film, the method comprising:
supplying a source gas and an atmospheric gas onto a substrate in a state where the substrate is loaded in a chamber; and
depositing the amorphous silicon film on the substrate at a process temperature under a process pressure,
wherein the source gas comprises at least one of silane (SiH2), disilane (Si2H6), and dichlorosilane (SiCl2H2),
wherein the process temperature is adjusted to be in a range of about 540° C. to about 580° C. and the process pressure is adjusted to be in a range of about 8 Torr to about 300 Torr, so that the source gas is pyrolyzed to deposit the amorphous silicon film on the substrate, and
wherein the atmospheric gas comprises at least one of hydrogen and helium.

### Claim 2 (depends on 1)

The method of claim 1, wherein the source gas has a flow rate of about 0.5 sccm to about 300 sccm, and
the atmospheric gas has a flow rate of about 100 sccm to about 25000 sccm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the amorphous silicon film is deposited to have a thickness of about 1000 Å or more.

### Claim 4 (depends on 3)

The method of claim 3, wherein the amorphous silicon film is deposited to have a surface roughness of about 1 nm or less.

### Claim 5 (depends on 1)

The method of claim 1, wherein the substrate is placed on a heater, and the substrate is heated by the heater to the process temperature.