# US 2017/0256401 A1 · Emissivity, surface finish and porosity control of semiconductor reactor components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256401 A1
- Document ID: US20170256401A1
- Status: Published application
- Kind: A1
- Application number: 15/596,117
- Filed: 2017-05-16
- Published: 2017-09-07
- Earliest claimed: 2015-07-06
- Assignees: ASM IP Holding B.V.
- Applicants: Asm IP Holding B.V.
- Inventors: Carl Louis White; John Kevin Shugrue
- Web page: https://patentgrep.com/patent/US20170256401A1

## CPC

- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- C25D 11/04: of aluminium or alloys based thereon
- C25D 11/16: Pretreatment {, e.g. desmutting}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

An apparatus and methods are provided related to a surface of a reaction chamber assembly component. The surface may be roughened and/or anodized to provide desirable emissivity and porosity to help reduce burn-in time of a reaction chamber and to help reduce particles within the chamber. The apparatus and methods may be suitable for thin film deposition on semiconductor or other substrates.

## Claims

### Claim 1

A method comprising the steps of:
blasting with blast media a surface of an aluminum alloy reaction chamber assembly component to produce a blasted surface having a surface roughness; and
anodizing the blasted surface to form an anodized surface layer.

### Claim 2 (depends on 1)

The method of claim 1 further comprising the step of cleaning the surface after the step of blasting and before the step of anodizing.

### Claim 3 (depends on 1)

The method of claim 1 wherein the anodized surface layer has a thickness in a range of 3-15 μm and a surface roughness in a range of 0.4-6.3 μm.

### Claim 4 (depends on 3)

The method of claim 3 wherein the anodized surface layer has an emissivity of at least 0.50.

### Claim 5

A method for an aluminum alloy reaction chamber assembly component with an anodized surface layer comprising:
roughening a surface layer of an aluminum alloy reaction chamber component;
cleaning the surface layer of the aluminum alloy reaction chamber component;
anodizing the surface layer of the aluminum alloy reaction chamber component to create an anodized surface layer; and
effecting the installation of the anodized surface layer of the aluminum alloy reaction chamber component into an aluminum alloy reaction chamber configured to fabricate a semiconductor.

### Claim 6 (depends on 5)

The method of claim 5, wherein roughening the surface layer of the aluminum alloy reaction chamber component is accomplished by blasting, with blast media, the surface layer of the aluminum alloy reaction chamber component.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
selecting the blast media from a group comprising (i) alumina grit or particles and (ii) zirconia grit or particles;
wherein the blasting with the blast media is adapted to roughen wetted surfaces to promote adhesion of undesirable reactions and film deposition to prevent additional particles within the aluminum alloy reaction chamber from landing on a substrate surface after shedding into a gas stream.

### Claim 8 (depends on 5)

The method of claim 5, wherein roughening the surface layer of an aluminum alloy reaction chamber component is accomplished by ablating, with a laser, the surface layer of the aluminum alloy reaction chamber component.

### Claim 9 (depends on 5)

The method of claim 5, further comprising
exposing the anodized surface layer to gas within the aluminum alloy reaction chamber prior to a coating or film depositing on the anodized surface layer; and
creating, via film deposition, a coating or film on the anodized surface layer.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
covering, completely, the anodized surface layer entirely with the coating or film such that no portion of the anodized surface layer is exposed.

### Claim 11 (depends on 5)

The method of claim 5, further comprising:
establishing a surface roughness average (Ra) from roughening the surface layer of the aluminum alloy reaction chamber component; and
wherein the Ra is in a range from about 0.4 μm to about 6.3 μm.

### Claim 12 (depends on 11)

The method of claim 11, wherein the Ra is in a range from about 0.8 μm to about 4.5 μm.

### Claim 13 (depends on 12)

The method of claim 12, wherein the Ra is in a range from about 2.0 μm to about 4.25 μm.

### Claim 14 (depends on 13)

The method of claim 13, wherein the Ra is in a range from about 3.75 μm to about 4.25 μm.

### Claim 15 (depends on 5)

The method of claim 5, wherein cleaning the surface layer of the aluminum alloy reaction chamber component further comprises:
removing blast media particles from the surface layer of the aluminum alloy reaction chamber component after the surface layer was roughened via blasting with blast media.

### Claim 16 (depends on 5)

The method of claim 5, wherein cleaning the surface layer of the aluminum alloy reaction chamber component further comprises:
immersing the surface layer of the aluminum alloy reaction chamber component in a heated solution;
rinsing the surface layer of the aluminum alloy reaction chamber component with deionized water;
immersing the surface layer of the aluminum alloy reaction chamber component in a first acidic solution for a first period of time;
rinsing the surface layer of the aluminum alloy reaction chamber component with deionized water for a second time;
immersing the surface layer of the aluminum alloy reaction chamber component in a second acidic solution for a second period of time;
desmutting the surface layer of the aluminum alloy reaction chamber component with a nitric acid solution;
immersing the surface layer of the aluminum alloy reaction chamber component in an ultrasonic tank bath for a third period of time;
immersing the surface layer of the aluminum alloy reaction chamber component in cleanroom heated deionized water for a fourth period of time;
removing the surface layer aluminum alloy reaction chamber component from the cleanroom heated deionized water; and
drying the surface layer of the aluminum alloy reaction chamber component.

### Claim 17 (depends on 5)

The method of claim 5, wherein anodizing the surface layer of the aluminum alloy reaction chamber component to create an anodized surface layer is accomplished by disposing the surface layer of the aluminum alloy reaction chamber component in an acid bath.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
effecting a resultant thickness of the anodized surface layer by controlling the acid bath and the time in which the surface layer of the aluminum alloy reaction chamber component is in the acid bath.

### Claim 19 (depends on 18)

The method of claim 18, wherein the resultant thickness of the anodized surface layer is in a range from about 3 μm to about 15 μm.

### Claim 20 (depends on 18)

The method of claim 18, further comprising:
effecting a resultant emissivity of the anodized surface layer by controlling the acid bath and the time in which the surface layer of the aluminum alloy reaction chamber component is in the acid bath.

### Claim 21 (depends on 20)

The method of claim 20, wherein the resultant emissivity of the anodized surface layer is at least 0.50.

### Claim 22 (depends on 5)

The method of claim 5, wherein the aluminum alloy reaction chamber component is a showerhead and roughening the surface layer of the showerhead is accomplished by blasting, with blast media, the surface layer of the showerhead, wherein the showerhead defines a plurality of drilled holes that are not blasted to roughen the holes in the manner in which the surface layer is roughened.