# US 2017/0256344 A1 · Method for manufacturing r-t-b based sintered magnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0256344 A1
- Document ID: US20170256344A1
- Status: Published application
- Kind: A1
- Application number: 15/511,299
- Filed: 2015-08-31
- Published: 2017-09-07
- Earliest claimed: 2014-09-17
- Assignees: Hitachi Metals, Ltd.
- Applicants: Hitachi Metals, Ltd.
- Inventors: Teppei SATOH; Futoshi KUNIYOSHI; Rintaro ISHII; Ryouichi YAMAGATA
- Web page: https://patentgrep.com/patent/US20170256344A1

## CPC

- H01F 1/08: pressed, sintered, or bound together
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C21D 6/00: Heat treatment of ferrous alloys
- C22C 33/02: by powder metallurgy
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- H01F 1/0577: {sintered}
- H01F 41/02: for manufacturing cores, coils, or magnets (H01F41/14 takes precedence; for dynamo-electric machines H02K15/00)
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 38/06: containing aluminium
- C22C 38/16: containing copper
- Y02T 10/64: Electric machine technologies in electromobility
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body, the sintered magnet material having a particular composition and satisfying inequality expressions (1) and (2); 2) a high-temperature heat treatment step of heating the sintered magnet material to a heating temperature of 730° C. to 1,020° C. and then cooling the sintered magnet material to 300° C. at a cooling rate of 5° C./min or more; and 3) a low-temperature heat treatment step of heating the sintered magnet material after the high-temperature heat treatment step to 440° C. to 550° C.: [T]−72.3[B]>0 (1) ([T]−72.3[B])/55.85<13[Ga]/69.72 (2) where [T] is a T content in percent by mass, [B] is a B content in percent by mass, and [Ga] is a Ga content in percent by mass.

## Claims

### Claim 1

A method for manufacturing an R-T-B based sintered magnet, which comprises:
1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body, the R-T-B based sintered magnet material comprising:
27.5% or more by mass and 34.0% or less by mass of R
(R being at least one element of rare earth elements and indispensably containing Nd);
0.85% or more by mass and 0.93% or less by mass of B;
0.20% or more by mass and 0.70% or less by mass of Ga;
more than 0.2% by mass and 0.50% or less by mass of Cu;
0.05% or more by mass and 0.5% or less by mass of Al; and
0% or more by mass and 0.1% or less by mass of M
(M being one or both of Nb and Zr), with the balance being T (T being Fe and Co, and 90% or more of T in terms of mass ratio being Fe) and inevitable impurities, the R-T-B based sintered magnet material satisfying inequality expressions (1) and (2) below:
[T]−72.3[B]>0 (1)
([T]−72.3[B])/55.85<13[Ga]/69.72 (2)
where [T] is a T content in percent by mass, [B] is a B content in percent by mass, and [Ga] is a Ga content in percent by mass;
2) a high-temperature heat treatment step of heating the R-T-B based sintered magnet material to a heating temperature of 730° C. or higher and 1,020° C. or lower and then cooling the R-T-B based sintered magnet material to 300° C. at a cooling rate of 5° C./min or more; and
3) a low-temperature heat treatment step of heating the R-T-B based sintered magnet material after the high-temperature heat treatment step to 440° C. or higher and 550° C. or lower.

### Claim 2 (depends on 1)

The method for manufacturing an R-T-B based sintered magnet according to claim 1, wherein, in the step 2), the R-T-B based sintered magnet material is cooled from the heating temperature to 300° C. at a cooling rate of 5° C./min or more and 25° C./min or less.

### Claim 3 (depends on 1)

The method for manufacturing an R-T-B based sintered magnet according to claim 1, wherein, in the step 2), the R-T-B based sintered magnet material is cooled from the heating temperature to 300° C. at a cooling rate of 10° C./min or more and 25° C./min or less.

### Claim 4 (depends on 1)

The method for manufacturing an R-T-B based sintered magnet according to claim 1, wherein, in the step 3), the R-T-B based sintered magnet material after the high-temperature heat treatment step is heated to a temperature of 450° C. or higher and 490° C. or lower.

### Claim 5 (depends on 1)

The method for manufacturing an R-T-B based sintered magnet according to claim 1, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.

### Claim 6 (depends on 2)

The method for manufacturing an R-T-B based sintered magnet according to claim 2, wherein, in the step 3), the R-T-B based sintered magnet material after the high-temperature heat treatment step is heated to a temperature of 450° C. or higher and 490° C. or lower.

### Claim 7 (depends on 3)

The method for manufacturing an R-T-B based sintered magnet according to claim 3, wherein, in the step 3), the R-T-B based sintered magnet material after the high-temperature heat treatment step is heated to a temperature of 450° C. or higher and 490° C. or lower.

### Claim 8 (depends on 2)

The method for manufacturing an R-T-B based sintered magnet according to claim 2, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.

### Claim 9 (depends on 3)

The method for manufacturing an R-T-B based sintered magnet according to claim 3, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.

### Claim 10 (depends on 4)

The method for manufacturing an R-T-B based sintered magnet according to claim 4, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.

### Claim 11 (depends on 6)

The method for manufacturing an R-T-B based sintered magnet according to claim 6, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.

### Claim 12 (depends on 7)

The method for manufacturing an R-T-B based sintered magnet according to claim 7, wherein the R-T-B based sintered magnet material includes 27.5% or more by mass and 31.0% or less by mass of R.