# US 2017/0254948 A1 · Glass light guide plate, mold, and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0254948 A1
- Document ID: US20170254948A1
- Status: Published application
- Kind: A1
- Application number: 15/230,872
- Filed: 2016-08-08
- Published: 2017-09-07
- Earliest claimed: 2016-03-01
- Assignees: Hon Hai Precision Industry Co., Ltd.
- Applicants: Hon Hai Precision Industry Co., Ltd.
- Inventors: FENG-YUEN DAI; CHAU-JIN HU; CHIN-LUNG CHIU; HSIN-HUA CHANG; YUNG-LUN HUANG; YAO-CHIEN CHUANG; CHUNG-PEI WANG
- Web page: https://patentgrep.com/patent/US20170254948A1

## CPC

- G02B 6/0065: {Manufacturing aspects; Material aspects}
- C03B 23/02: Re-forming glass sheets
- C03B 23/0357: {by suction without blowing, e.g. with vacuum or by venturi effect}
- C03B 40/00: Preventing adhesion between glass and glass or between glass and the means used to shape it {, hold it or support it}
- C22C 45/00: Amorphous alloys (making amorphous non-ferrous alloys C22C1/11)
- G02B 6/0036: {2-D arrangement of prisms, protrusions, indentations or roughened surfaces}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A mold which is made of a porous heat-resistant material comprises a first surface and a second surface opposite to the first surface. A plurality of light guide spots are formed on the first surface. The light guide spots are light guide spots. The first surface is a smooth polished surface, the mold enables direct manufacture of light guide plates for less heat expended.

## Claims

### Claim 1

A mold made of a porous heat-resistant material, the mold comprising:
a first surface and a second surface opposite to the first surface, wherein the first surface is a smooth polished surface;
a plurality of light guide spots formed on the first surface, wherein the light guide spots are substantially hemispherical recesses.

### Claim 2 (depends on 1)

The mold of claim 1, wherein each of the light guide spots has a diameter in a range of 30 microns to 400 microns and a depth in a range of about 3 microns to about 40 microns.

### Claim 3 (depends on 1)

The mold of claim 1, wherein the porous heat-resistant material is selected from one or more of hexagonal boron nitride (HBN), silicon oxide (SiO2), alumina (Al2O3), and hexagonal layers of carbon (C).

### Claim 4 (depends on 1)

The mold of claim 1, wherein the porous heat-resistant material is capable of withstanding temperatures of about 500° C. to about 1500° C.

### Claim 5 (depends on 1)

The mold of claim 1, wherein the porous heat-resistant material is made by holes formed in the mold, the holes are distributed evenly and mutually connected, a size of aperture (d) of the holes is from about 0.1 nanometers (nm) to about 2.1 microns (μm).

### Claim 6

A method of manufacturing a glass light guide plate, comprising:
providing a mold and a glass substrate, the mold being made of a porous heat-resistant material and comprising a first surface and a second surface opposite to the first surface, the first surface being smooth and polished;
forming a plurality of light guide spots in the mold, wherein the light guide spots are substantially hemispherical recesses, the glass substrate comprises an upper surface and a lower surface opposite to the upper surface, a glass transition temperature of the glass substrate is less than a heat resistance temperature of the mold;
heating the mold to the glass transition temperature of the glass substrate;
maintaining the temperature of the mold at the glass transition temperature, placing the lower surface of the glass substrate on the first surface of the mold;
exhausting air from the mold to adhere the glass substrate on the first surface; and
separating the mold from the glass substrate, whereby the glass substrate forms the glass light guide, the light guide plate comprising a plurality of hemispherical protrusions corresponding to the hemispherical recesses.

### Claim 7 (depends on 6)

The method of claim 6, wherein during the step of placing the lower surface of the glass substrate on the first surface of the mold, the glass substrate is softened and fills the plurality of light guide spots to form the substantially hemispherical protrusions.

### Claim 8 (depends on 6)

The method of claim 6, wherein the porous heat-resistant material is capable of withstanding temperatures of about 500° C. to about 1500° C.

### Claim 9 (depends on 6)

The method of claim 6, wherein the porous heat-resistant material is made by forming holes in the mold, the holes are distributed evenly and mutually connected, a size of aperture (d) of the holes are from about 0.1 nanometers (nm) to about 2.1 microns (μm).

### Claim 10 (depends on 6)

A guide plate glass made by the method of claim 6, wherein the glass light guide plate includes an upper surface and a lower surface, the upper surface is opposite to the lower surface, spherical protrusions are formed on the lower surface.