# US 2017/0254153 A1 · Polycrystalline diamond compacts, methods of forming polycrystalline diamond, and earth-boring tools

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0254153 A1
- Document ID: US20170254153A1
- Status: Published application
- Kind: A1
- Application number: 15/060,911
- Filed: 2016-03-04
- Published: 2017-09-07
- Earliest claimed: 2016-03-04
- Assignees: Baker Hughes Incorporated; Diamond Innovations, Inc.
- Applicants: Baker Hughes Incorporated; Diamond Innovations, Inc
- Inventors: Marc W. Bird; Andrew Gledhill
- Web page: https://patentgrep.com/patent/US20170254153A1

## CPC

- E21B 10/56: Button-type inserts (E21B10/52 takes precedence)
- B24D 18/0009: {using moulds or presses}
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- C22C 29/005: {comprising a particular metallic binder}
- B22F 7/062: {involving the connection or repairing of preformed parts}
- B22F 2005/001: {Cutting tools, earth boring or grinding tool other than table ware}
- C22C 2026/006: {with additional metal compounds being carbides}
- C22C 2026/008: {with additional metal compounds other than carbides, borides or nitrides}
- E21B 10/50: the bit being of roller type
- E21B 10/54: the bit being of the rotary drag type, e.g. fork-type bits
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A polycrystalline diamond compact includes a polycrystalline diamond material having a plurality of grains of diamond bonded to one another by inter-granular bonds and an intermetallic gamma prime (γ′) or κ-carbide phase disposed within interstitial spaces between the inter-bonded diamond grains. The ordered intermetallic gamma prime (γ′) or κ-carbide phase includes a Group VIII metal, aluminum, and a stabilizer. An earth-boring tool includes a bit body and a polycrystalline diamond compact secured to the bit body. A method of forming polycrystalline diamond includes subjecting diamond particles in the presence of a metal material comprising a Group VIII metal and aluminum to a pressure of at least 4.5 GPa and a temperature of at least 1,000° C. to form inter-granular bonds between adjacent diamond particles, cooling the diamond particles and the metal material to a temperature below 500° C., and forming an intermetallic gamma prime (γ′) or κ-carbide phase adjacent the diamond particles.

## Claims

### Claim 1

A polycrystalline diamond compact, comprising:
a polycrystalline diamond material comprising a plurality of grains of diamond bonded to one another by inter-granular bonds; and
an intermetallic gamma prime (γ′) or κ-carbide phase disposed within interstitial spaces between the inter-bonded diamond grains, the gamma prime (γ′) or κ-carbide phase comprising a Group VIII metal, aluminum, and a stabilizer.

### Claim 2 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the stabilizer comprises a material selected from the group consisting of titanium, nickel, tungsten, and carbon.

### Claim 3 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the gamma prime (γ′) or κ-carbide phase comprises a metastable Co3Al phase stabilized by the stabilizer.

### Claim 4 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the gamma prime (γ′) or κ-carbide phase comprises a metastable (CoxNi3-x)Al phase stabilized by the stabilizer.

### Claim 5 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the stabilizer comprises carbon.

### Claim 6 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the gamma prime (γ′) or κ-carbide phase exhibits an ordered face-centered cubic structure.

### Claim 7 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the polycrystalline diamond material is disposed over a substrate comprising the Group VIII metal.

### Claim 8 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the polycrystalline diamond material is substantially free of elemental iron, cobalt, and nickel.

### Claim 9 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the gamma prime (γ′) or κ-carbide phase comprises a metastable CoxAly phase having less than about 13% Co by weight.

### Claim 10 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the gamma prime (γ′) or κ-carbide phase comprises a metastable CoxAly phase having less than about 50 mol % Al.

### Claim 11 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the intermetallic gamma prime (γ′) or κ-carbide phase is structurally ordered.

### Claim 12 (depends on 1)

The polycrystalline diamond compact of claim 1, wherein the intermetallic gamma prime (γ′) or κ-carbide phase is structurally disordered.

### Claim 13

A method of forming polycrystalline diamond, comprising:
subjecting diamond particles in the presence of a metal material comprising a Group VIII metal and aluminum to a pressure of at least 4.5 GPa and a temperature of at least 1,000° C. to form inter-granular bonds between adjacent diamond particles;
cooling the diamond particles and the metal material to a temperature below an ordered-disordered transition temperature; and
forming an ordered intermetallic gamma prime (γ′) or κ-carbide phase adjacent the diamond particles, the ordered intermetallic gamma prime (γ′) or κ-carbide phase comprising the Group VIII metal, aluminum, and a stabilizer.

### Claim 14 (depends on 13)

The method of claim 13, wherein subjecting diamond particles to a pressure of at least 4.5 GPa and a temperature of at least 1,000° C. comprises dissolving the stabilizer in a mixture of the Group VIII metal and the aluminum.

### Claim 15 (depends on 14)

The method of claim 14, wherein dissolving the stabilizer in a mixture of the Group VIII metal and the aluminum comprises dissolving carbon originating from the diamond particles into a molten alloy comprising the Group VIII metal and the aluminum.

### Claim 16 (depends on 13)

The method of claim 13, further comprising admixing the diamond particles with particles comprising at least one material selected from the group consisting of the Group VIII metal, the aluminum, and the stabilizer.

### Claim 17 (depends on 13)

The method of claim 13, further comprising disposing the diamond particles in a container with a metal foil comprising at least one material selected from the group consisting of the Group VIII metal, the aluminum, and the stabilizer.

### Claim 18 (depends on 13)

The method of claim 13, further comprising forming the polycrystalline diamond in the form of a finished cutting element comprising a diamond table including the ordered intermetallic gamma prime (γ′) or κ-carbide phase comprising the Group VIII metal, aluminum, and the stabilizer.

### Claim 19 (depends on 13)

The method of claim 13, further comprising at least substantially entirely filling interstitial spaces between the diamond particles with the gamma prime (γ′) or κ-carbide phase.

### Claim 20

An earth-boring tool, comprising:
a bit body; and
a polycrystalline diamond compact secured to the bit body, the polycrystalline diamond compact comprising:
a polycrystalline diamond material comprising a plurality of grains of diamond bonded to one another by inter-granular bonds; and
an intermetallic gamma prime (γ′) or κ-carbide phase disposed within interstitial spaces between the inter-bonded diamond grains, the intermetallic gamma prime (γ′) or κ-carbide phase comprising a Group VIII metal, aluminum, and a stabilizer.