# US 2017/0253998 A1 · Acrylic-fiber manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253998 A1
- Document ID: US20170253998A1
- Status: Published application
- Kind: A1
- Application number: 15/600,096
- Filed: 2017-05-19
- Published: 2017-09-07
- Earliest claimed: 2014-11-21
- Assignees: Kaneka Corporation
- Applicants: Kaneka Corporation
- Inventors: Ryohei Noishiki; Masanobu Tamura
- Web page: https://patentgrep.com/patent/US20170253998A1

## CPC

- D01F 6/02: from homopolymers obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C08L 27/06: Homopolymers or copolymers of vinyl chloride
- C08L 33/08: Homopolymers or copolymers of acrylic acid esters
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01D 10/06: Washing or drying
- D01F 6/10: from polyvinyl chloride or polyvinylidene chloride
- D01F 6/40: Modacrylic fibres, i.e. containing 35 to 85% acrylonitrile
- D01F 6/96: from other synthetic polymers
- D06M 13/244: with compounds containing sulfur or phosphorus
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

A method for manufacturing an acrylic fiber uses a spinning solution in which an acrylic polymer is dissolved in an organic solvent, the method including reducing an amount of organic solvent by repeatedly spraying water onto coagulated filaments obtained by solidifying the spinning solution and pressing the coagulated filaments with nip rolls. The nip rolls may apply a nip pressure of 0.2 MPa or higher. Thus, a method for manufacturing an acrylic fiber with which an organic solvent in the acrylic fiber can be removed within a short period of time without using a water bath is provided.

## Claims

### Claim 1

A method for manufacturing an acrylic fiber using a spinning solution, the method comprising:
reducing an amount of an organic solvent by repeatedly spraying water onto coagulated filaments and pressing the coagulated filaments with nip rolls, wherein the coagulated filaments are obtained by solidifying the spinning solution comprising an acrylic polymer and the organic solvent.

### Claim 2 (depends on 1)

The method for manufacturing an acrylic fiber according to claim 1, wherein the nip rolls apply a nip pressure of 0.2 MPa or higher.

### Claim 3 (depends on 1)

The method for manufacturing an acrylic fiber according to claim 1, wherein the spraying and the pressing are repeatedly performed eight or more times.

### Claim 4 (depends on 1)

The method for manufacturing an acrylic fiber according to claim 1, wherein the organic solvent in the spinning solution is at least one selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, and N,N-dimethylformamide.

### Claim 5 (depends on 1)

The method for manufacturing an acrylic fiber according to claim 1, wherein the reducing is performed after the coagulated filaments have been drawn.

### Claim 6 (depends on 1)

The method for manufacturing an acrylic fiber according to claim 1, wherein the acrylic polymer comprises acrylonitrile in an amount of 20 to 85 mass %, a halogen-containing vinyl and/or a halogen-containing vinylidene in an amount of 15 to 80 mass %, and a sulfonic acid-containing monomer in an amount of 0 to 10 mass % with respect to a total mass of the acrylic polymer, and has a specific viscosity of 0.1 to 0.3.

### Claim 7 (depends on 2)

The method for manufacturing an acrylic fiber according to claim 2, wherein the spraying and the pressing are repeatedly performed eight or more times.

### Claim 8 (depends on 2)

The method for manufacturing an acrylic fiber according to claim 2, wherein the organic solvent in the spinning solution is at least one selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, and N,N-dimethylformamide.

### Claim 9 (depends on 3)

The method for manufacturing an acrylic fiber according to claim 3, wherein the organic solvent in the spinning solution is at least one selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, and N,N-dimethylformamide.

### Claim 10 (depends on 4)

The method for manufacturing an acrylic fiber according to claim 4, wherein the organic solvent in the spinning solution is at least one selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, and N,N-dimethylformamide.

### Claim 11 (depends on 7)

The method for manufacturing an acrylic fiber according to claim 7, wherein the organic solvent in the spinning solution is at least one selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, and N,N-dimethylformamide.