# US 2017/0253995 A1 · Method for heat-treating silicon single crystal wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253995 A1
- Document ID: US20170253995A1
- Status: Published application
- Kind: A1
- Application number: 15/519,859
- Filed: 2015-09-17
- Published: 2017-09-07
- Earliest claimed: 2014-11-26
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Applicants: Shin-Etsu Handotai Co., Ltd.
- Inventors: Wei Feng QU; Fumio TAHARA; Masahiro SAKURADA; Shuji TAKAHASHI
- Web page: https://patentgrep.com/patent/US20170253995A1

## CPC

- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B 29/06: Silicon
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for heat-treating a silicon single crystal wafer by an RTA treatment, including: putting a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or an Nv region containing an OSF region for the silicon single crystal wafer entire plane into an RTA furnace, performing pre-heating at temperature lower than temperature at which silicon reacts with NH3 while supplying gas that contains NH3 into the RTA furnace, subsequently stopping the supply of the gas containing NH3 and starting supply of Ar gas to start an RTA treatment under Ar gas atmosphere in which the NH3 gas remains. This provide a method for heat-treating a silicon single crystal wafer that give gettering capability without degrading TDDB properties even to a silicon single crystal wafer in which the entire plane is an Nv region or an Nv region containing an OSF region.

## Claims

### Claim at position 1

1-6. (canceled)

### Claim 7

A method for heat-treating a silicon single crystal wafer by a rapid thermal annealing treatment, comprising:
putting a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or an Nv region that contains an OSF region for the entire plane of the silicon single crystal wafer into a rapid thermal annealing furnace,
performing pre-heating at a temperature lower than the temperature at which silicon reacts with NH3 while supplying gas that contains NH3 into the rapid thermal annealing furnace, and subsequently
stopping the supply of the gas that contains NH3 and starting supply of Ar gas to start a rapid thermal annealing treatment under Ar gas atmosphere in which the NH3 gas remains.

### Claim 8 (depends on 7)

The method for heat-treating a silicon single crystal wafer according to claim 7, wherein the rapid thermal annealing treatment is performed under conditions of 1,000 to 1,275° C. for 10 to 30 seconds.

### Claim 9 (depends on 7)

The method for heat-treating a silicon single crystal wafer according to claim 7, wherein the pre-heating is performed at a temperature that is higher than ordinary temperature and is 600° C. or less.

### Claim 10 (depends on 8)

The method for heat-treating a silicon single crystal wafer according to claim 8, wherein the pre-heating is performed at a temperature that is higher than ordinary temperature and is 600° C. or less.

### Claim 11 (depends on 7)

The method for heat-treating a silicon single crystal wafer according to claim 7, wherein the silicon single crystal wafer has an Nv region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma.

### Claim 12 (depends on 8)

The method for heat-treating a silicon single crystal wafer according to claim 8, wherein the silicon single crystal wafer has an Nv region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma.

### Claim 13 (depends on 9)

The method for heat-treating a silicon single crystal wafer according to claim 9, wherein the silicon single crystal wafer has an Nv region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma.

### Claim 14 (depends on 10)

The method for heat-treating a silicon single crystal wafer according to claim 10, wherein the silicon single crystal wafer has an Nv region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma.

### Claim 15 (depends on 7)

The method for heat-treating a silicon single crystal wafer according to claim 7, wherein the silicon single crystal wafer has an Nv region that contains an OSF region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 9 to 11 ppma.

### Claim 16 (depends on 8)

The method for heat-treating a silicon single crystal wafer according to claim 8, wherein the silicon single crystal wafer has an Nv region that contains an OSF region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 9 to 11 ppma.

### Claim 17 (depends on 9)

The method for heat-treating a silicon single crystal wafer according to claim 9, wherein the silicon single crystal wafer has an Nv region that contains an OSF region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 9 to 11 ppma.

### Claim 18 (depends on 10)

The method for heat-treating a silicon single crystal wafer according to claim 10, wherein the silicon single crystal wafer has an Nv region that contains an OSF region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 9 to 11 ppma.

### Claim 19 (depends on 7)

The method for heat-treating a silicon single crystal wafer according to claim 7, wherein, in the rapid thermal annealing treatment, an NH3 concentration in the rapid thermal annealing furnace is set to 0.5% by volume or more and 3% by volume or less when heated to the temperature at which silicon reacts with NH3.

### Claim 20 (depends on 8)

The method for heat-treating a silicon single crystal wafer according to claim 8, wherein, in the rapid thermal annealing treatment, an NH3 concentration in the rapid thermal annealing furnace is set to 0.5% by volume or more and 3% by volume or less when heated to the temperature at which silicon reacts with NH3.

### Claim 21 (depends on 9)

The method for heat-treating a silicon single crystal wafer according to claim 9, wherein, in the rapid thermal annealing treatment, an NH3 concentration in the rapid thermal annealing furnace is set to 0.5% by volume or more and 3% by volume or less when heated to the temperature at which silicon reacts with NH3.

### Claim 22 (depends on 11)

The method for heat-treating a silicon single crystal wafer according to claim 11, wherein, in the rapid thermal annealing treatment, an NH3 concentration in the rapid thermal annealing furnace is set to 0.5% by volume or more and 3% by volume or less when heated to the temperature at which silicon reacts with NH3.

### Claim 23 (depends on 15)

The method for heat-treating a silicon single crystal wafer according to claim 15, wherein, in the rapid thermal annealing treatment, an NH3 concentration in the rapid thermal annealing furnace is set to 0.5% by volume or more and 3% by volume or less when heated to the temperature at which silicon reacts with NH3.