# US 2017/0253964 A1 · Film deposition method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253964 A1
- Document ID: US20170253964A1
- Status: Published application
- Kind: A1
- Application number: 15/439,180
- Filed: 2017-02-22
- Published: 2017-09-07
- Earliest claimed: 2016-03-02
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Hitoshi KATO; Masahiro MURATA; Jun SATO; Shigehiro MIURA
- Web page: https://patentgrep.com/patent/US20170253964A1

## CPC

- C23C 16/345: {Silicon nitride}
- C23C 16/24: Deposition of silicon only
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/4554: {Plasma being used non-continuously in between ALD reactions (C23C16/56 takes precedence)}
- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- C23C 16/45551: {for relative movement of the substrate and the gas injectors or half-reaction reactor compartments}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- H01J 37/3211: {Antennas, e.g. particular shapes of coils}
- H01J 37/32119: {Windows}
- H01J 37/32513: {Sealing means, e.g. sealing between different parts of the vessel}
- H01J 37/32752: {for moving the material across the discharge}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A film deposition method includes steps of: adsorbing a silicon-containing gas on a surface of a substrate, by supplying the silicon-containing gas to the surface of the substrate; depositing a silicon nitride film, by supplying a nitriding gas to the surface of the substrate, while being activated by a first plasma, and nitriding the silicon-containing gas adsorbed on the surface of the substrate; and modifying the silicon nitride film deposited on the surface of the substrate, by supplying a treatment gas containing NH3 and N2 at a given ratio to the surface of the substrate, while being activated by a second plasma.

## Claims

### Claim 1

A film deposition method comprising steps of:
adsorbing a silicon-containing gas on a surface of a substrate, by supplying the silicon-containing gas to the surface of the substrate;
depositing a silicon nitride film, by supplying a nitriding gas to the surface of the substrate, while being activated by a first plasma, and nitriding the silicon-containing gas adsorbed on the surface of the substrate; and
modifying the silicon nitride film deposited on the surface of the substrate, by supplying a treatment gas containing NH3 and N2 at a given ratio to the surface of the substrate, while being activated by a second plasma.

### Claim 2 (depends on 1)

The film deposition method according to claim 1, wherein N2 is higher than NH3 in the given ratio.

### Claim 3 (depends on 2)

The film deposition method according to claim 2, wherein N2 at least twice as much as NH3 is included by the given ratio.

### Claim 4 (depends on 3)

The film deposition method according to claim 3, wherein N2 at least three times as much as NH3 is included by the given ratio.

### Claim 5 (depends on 1)

The film deposition method according to claim 1, wherein the nitriding gas is an NH3-containing gas.

### Claim 6 (depends on 5)

The film deposition method according to claim 5, wherein the nitriding gas is a gas that does not contain N2.

### Claim 7 (depends on 5)

The film deposition method according to claim 5, wherein the nitriding gas further contains Ar and H2.

### Claim 8 (depends on 1)

The film deposition method according to claim 1, wherein the treatment gas further contains Ar.

### Claim 9 (depends on 1)

The film deposition method according to claim 1, wherein a position where the second plasma is generated is closer to the surface of the substrate than a position where the first plasma is generated.

### Claim 10 (depends on 9)

The film deposition method according to claim 9, wherein the step of adsorbing the silicon-containing gas, the step of depositing the silicon nitride film, and the step of modifying the silicon nitride film are successively repeated to deposit the silicon nitride film to have a given thickness.

### Claim 11 (depends on 10)

The film deposition method according to claim 10, further comprising the steps of:
supplying a purge gas to the surface of the substrate between the step of adsorbing the silicon-containing gas and the step of depositing the silicon nitride film; and
supplying the purge gas to the surface of the substrate between the step of modifying the silicon nitride film and the step of adsorbing the silicon-containing gas.

### Claim 12 (depends on 11)

The film deposition method according to claim 11,
wherein the substrate is placed on a surface of a turntable provided in a process chamber along a circumferential direction,
wherein above the turntable in the process chamber, a silicon-containing gas supply area, a first purge gas supply area, a nitriding gas supply area, a treatment gas supply area, and a second purge gas supply area are successively provided along a rotational direction of the turntable, and
wherein the step of adsorbing the silicon-containing gas, the step of supplying the purge gas, the step of depositing the silicon nitride film, the step of modifying the silicon nitride film, and the step of supplying the purge gas are successively repeated, by rotating the turntable to cause the substrate to pass through the silicon-containing gas supply area, the first purge gas supply area, the nitriding gas supply area, the treatment gas supply area, and the second purge gas supply area.

### Claim 13 (depends on 12)

The film deposition method according to claim 12,
wherein a first plasma generator is provided outside the process chamber above the nitriding gas supply area,
wherein a second plasma generator is provided outside the process chamber above the treatment gas supply area, and
wherein the second plasma generator is provided at a position lower than the first plasma generator.