# US 2017/0253956 A1 · Coating layer for electronic device manufacturing method thereof and electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253956 A1
- Document ID: US20170253956A1
- Status: Published application
- Kind: A1
- Application number: 15/351,996
- Filed: 2016-11-15
- Published: 2017-09-07
- Earliest claimed: 2016-03-04
- Assignees: Boe Technology Group Co., Ltd.; Beijing Boe Optoelectronics Technology Co., Ltd.
- Applicants: Boe Technology Group Co., Ltd.; Beijing Boe Optoelectronics Technology Co., Ltd.
- Inventors: Dong LIANG; Kaixuan WANG; Wei LI; Hongliang YUAN; Li MA; Yang YOU; Xiaojuan WU; Huishun CHEN; Xiaoqing PENG; Yao BI; Zijing ZHANG; Qi ZHENG
- Web page: https://patentgrep.com/patent/US20170253956A1

## CPC

- C23C 4/10: Oxides, borides, carbides, nitrides or silicides; Mixtures thereof
- B02C 17/1815: {Cooling or heating devices}
- C23C 4/06: Metallic material
- C23C 4/134: Plasma spraying
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})

## Abstract

A coating layer for electronic device and an electronic device are provided. The coating layer includes a composite of chambersite and a metal.

## Claims

### Claim 1

A coating layer for electronic device, wherein the coating layer comprises a composite of chambersite and a metal.

### Claim 2 (depends on 1)

The coating layer according to claim 1, wherein the metal comprises a light metal element or an alloy.

### Claim 3 (depends on 1)

The coating layer according to claim 1, wherein the coating layer is a chambersite/aluminum composite coating layer, a chambersite/copper composite coating layer or a chambersite/magnalium composite coating layer.

### Claim 4 (depends on 1)

The coating layer according to claim 1, wherein the coating layer is formed by spraying precursor powder on a surface of a housing, and the precursor powder is formed by powder of the chambersite and powder of the metal.

### Claim 5

An electronic device, comprising: a housing, wherein a surface of the housing is coated with a coating layer which comprises a composite of chambersite and a metal.

### Claim 6 (depends on 5)

The electronic device according to claim 5, wherein the metal comprises a light metal element or an alloy.

### Claim 7 (depends on 5)

The electronic device according to claim 5, wherein the coating layer is a chambersite/aluminum composite coating layer, a chambersite/copper composite coating layer or a chambersite/magnalium composite coating layer.

### Claim 8 (depends on 5)

The electronic device according to claim 5, wherein the coating layer is formed by spraying precursor powder on the surface of the housing, wherein the precursor powder is formed by powder of the chambersite and powder of the metal.

### Claim 9

A method for manufacturing a coating layer of electronic device, comprising:
spraying precursor powder on a surface of an electronic device housing, wherein the precursor powder is formed by powder of chambersite and powder of a metal.

### Claim 10 (depends on 9)

The manufacturing method according to claim 9, wherein the precursor powder is sprayed on the surface of the electronic device housing, and the precursor powder is formed by the powder of chambersite and powder of aluminum.

### Claim 11 (depends on 10)

The manufacturing method according to claim 10, further comprising:
mixing and grinding the powder of chambersite and the powder of aluminum in nitrogen atmosphere to form the precursor powder.

### Claim 12 (depends on 11)

The manufacturing method according to claim 11, wherein mixing and grinding the powder of chambersite and the powder of aluminum in nitrogen atmosphere to form the precursor powder comprises:
mixing submicron powder of chambersite and superfine powder of aluminum in nitrogen atmosphere to form mixed powder, a particle size of the superfine powder of aluminum is from 200 nm to 500 nm;
premixing the mixed powder and alcohol mechanically for 20 minutes, wherein a volume ratio of the mixed powder to the alcohol is from 1:0.95 to 1:1.59;
mixing the mixed powder after the premixing by high-energy ball-milling for 15-20 minutes, a weight ratio of ball to powder is 11:1, a rotate speed is 1,500-2,000 rounds per minute (R/M);
cooling the mixed powder after the high-energy ball-milling to room temperature in nitrogen atmosphere and drying in a vacuum drying oven; and
grinding the mixed powder after the cooling and the drying in nitrogen atmosphere for 10-15 minutes.

### Claim 13 (depends on 12)

The manufacturing method according to claim 12, wherein a mass fraction of the chambersite in the mixed powder is from 0.5% to 2%.

### Claim 14 (depends on 11)

The manufacturing method according to claim 11, wherein before mixing and grinding the powder of chambersite and the powder of aluminum in nitrogen atmosphere to form the precursor powder, the method further comprises:
high-energy ball-milling the chambersite powder after mineral purification for 50-60 minutes, wherein a weight ratio of ball to powder is 11:1, a rotate speed is 2,000-3,000 R/M;
drying the chambersite powder after high-energy ball-milling in the vacuum drying oven for 5-6 hours, at 65-90° C.; and
grinding the chambersite powder after drying for 20-25 minutes to obtain a submicron powder of chambersite.

### Claim 15 (depends on 9)

The manufacturing method according to claim 9, wherein the precursor powder is sprayed on the surface of the housing through a plasma spraying process.

### Claim 16 (depends on 15)

The manufacturing method according to claim 15, wherein, conditions of the plasma spraying process comprise: an operating voltage is 70-80 V; working gas is argon gas of 38-60 Normal Liter Per Minute (NLPM) and hydrogen of 9-12 Normal Liter Per Minute (NLPM); powder feeding rate is 3-9 gram per minute (g/min); a spraying distance is 90-130 mm; a weight percentage of carbon is 1%-9%.

### Claim 17 (depends on 9)

The manufacturing method according to claim 9, wherein, the precursor powder is sprayed on the surface of the electronic device housing, and wherein the precursor powder is formed by the powder of chambersite and powder of magnalium, to form a chambersite/magnalium composite coating layer.

### Claim 18 (depends on 9)

The manufacturing method according to claim 9, wherein the precursor powder is sprayed on the surface of the electronic device housing, and wherein the precursor powder is formed by the powder of chambersite and powder of copper.

### Claim 19 (depends on 9)

The manufacturing method according to claim 9, wherein the metal comprises a light metal element or an alloy.

### Claim 20 (depends on 9)

The manufacturing method according to claim 9, wherein the coating layer is a chambersite/aluminum composite coating layer, a chambersite/copper composite coating layer or a chambersite/magnalium composite coating layer.