# US 2017/0253953 A1 · Method of annealing aluminium alloy sheet material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253953 A1
- Document ID: US20170253953A1
- Status: Published application
- Kind: A1
- Application number: 15/509,736
- Filed: 2015-09-03
- Published: 2017-09-07
- Earliest claimed: 2014-09-12
- Assignees: Aleris Aluminum Duffel Bvba
- Applicants: Aleris Aluminum Duffel Bvba
- Inventors: Philippe MEYER; Svetlana Emirovna EBZEEVA; Johan Petrus Mariette Guido ARRAS; Dirk Medard Gerard Florent VAN NIEUWERBURGH; Petra BACKX
- Web page: https://patentgrep.com/patent/US20170253953A1

## CPC

- C22F 1/04: of aluminium or alloys based thereon
- C21D 1/42: Induction heating
- C21D 1/52: with flames
- C21D 9/0056: {Furnaces through which the charge is moved in a horizontal straight path (C21D9/0043 takes precedence)}
- C21D 9/0062: {Heat-treating apparatus with a cooling or quenching zone}
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- C23C 22/73: characterised by the process
- C23C 22/78: Pretreatment of the material to be coated
- Y02P 10/25: Process efficiency
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for continuously annealing aluminium alloy sheet at final thickness by continuously moving heat-treatable AlMgSi aluminium alloy sheet through a continuous annealing furnace arranged to heat the moving aluminium sheet to a set soaking temperature (TSET) in the temperature range of 500° C. to 590° C., the continuous annealing furnace has an entry section and an exit section, the moving aluminium sheet moves substantially horizontally through the continuous annealing furnace, wherein the moving aluminium sheet is rapidly cooled on leaving the exit section, wherein before or near the entry section of the continuous annealing furnace the moving aluminium sheet is pre-heated to a temperature of 5° C. to 100° C. below the TSET using an average heat-up rate as function of sheet thickness of at least Y=−31·ln(X)+50, wherein Y is the heat-up rate in ° C./sec and X is the sheet thickness in mm.

## Claims

### Claim 1

A method for continuously annealing aluminium alloy sheet at final thickness, comprising:
continuously moving uncoiled heat-treatable AlMgSi aluminium alloy sheet in the direction of its length through a continuous annealing furnace arranged to heat the moving aluminium sheet to a set soaking temperature (TSET) in the temperature range of 500° C. to 590° C., the continuous annealing furnace has an entry section and an exit section, wherein the moving aluminium sheet moves substantially horizontally through the continuous annealing furnace,
wherein the continuous annealing furnace is heated by convective heating, and
wherein the moving aluminium sheet is rapidly cooled from TSET to below about 100° C. on leaving the exit section, and
wherein before or near the entry section of the continuous annealing furnace the moving aluminium sheet is pre-heated to a temperature of 5° C. to 100° C. below the TSET using an average heat-up rate as function of the sheet thickness of at least Y=−31·ln(X)+50, wherein “Y” is the heat-up rate in ° C./sec and “X” is the sheet thickness in mm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein before or at the entry section of the continuous annealing furnace the moving aluminium sheet is pre-heated to a temperature of 5° C. to 100° C. below the TSET using an average heat-up rate as function of the sheet thickness of at least Y=−50·ln(X)+80, and more preferably of at least Y=−62·ln(X)+100, wherein Y is the heat-up rate in ° C./sec and X is the sheet thickness in mm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the pre-heating is per-formed inductively by induction heating.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the pre-heating is done inductively by a transverse flux induction heating device.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the aluminium alloy sheet at final gauge has a thickness in the range of 0.3 to 4.5 mm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet moves substantially horizontally through the continuous annealing furnace over a length of at least 20 meters.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the soaking time of the moving aluminium sheet at TSET is at least 1 seconds.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is pre-heated to a temperature of 5° C. to 75° C. below the TSET.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is pre-heated to a temperature of 10° C. to 100° C. below the TSET.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the continuous annealing furnace is arranged to heat the moving aluminium sheet to a set soaking temperature (TSET) in the temperature range of 520° C. to 580° C.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is rapidly cooled or quenched after leaving the exit section and is stretched up to 2%, by tension levelling.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the stretched and moving aluminium sheet is subsequently cleaned and provided with a passivation coating.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the stretched aluminium sheet having a passivation coating is heated-treated in a pre-bake heat treatment.

### Claim 14 (depends on 1)

The method according to claim 1, wherein convective heating of the continuous annealing furnace is gas fired.

### Claim 15 (depends on 1)

The method according claim 1, wherein the aluminium alloy sheet at final gauge has a thickness in the range of 0.7 to 4.5 mm.

### Claim 16 (depends on 1)

The method according claim 1, wherein the moving aluminium sheet moves substantially horizontally through the continuous annealing furnace over a length of at least 40 meters.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the soaking time of the moving aluminium sheet at TSET is at least 5 seconds.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the soaking time of the moving aluminium sheet at TSET is at least 20 seconds.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is preheated to a temperature of 5° C. to 60° C. below the TSET.

### Claim 20 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is preheated to a temperature of 10° C. to 75° C. below the TSET.

### Claim 21 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is preheated to a temperature of 10° C. to 60° C. below the TSET.

### Claim 22 (depends on 1)

The method according to claim 1, wherein the moving aluminium sheet is rapidly cooled or quenched after leaving the exit section and is stretched in a range of 0.1% to 0.3%, by means of tension levelling.