# US 2017/0253948 A1 · High-grade method of ilmenite ore, manufacturing method of high-grade tio2 using the said method and high-grade tio2 produced by the said manufacturing method, for ti-raw materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253948 A1
- Document ID: US20170253948A1
- Status: Published application
- Kind: A1
- Application number: 15/435,674
- Filed: 2017-02-17
- Published: 2017-09-07
- Earliest claimed: 2016-02-18
- Assignees: Tohoku University
- Applicants: Tohoku University
- Inventors: Tetsuya NAGASAKA; Yoshihiro ITO; Katsuyuki IIJIMA; Eiichiro YOSHIKAWA; Toru TAKAI; Nobuo NAKAMURA
- Web page: https://patentgrep.com/patent/US20170253948A1

## CPC

- C22B 34/1213: {by wet processes, e.g. using leaching methods or flotation techniques}
- C01G 23/0475: {Purification}
- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2006/80: Compositional purity
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for upgrading an ilmenite ore for yielding a high-TiO2-content titanium source by separating and removing an iron component from ilmenite (FeTiO3), which includes an oxidation step of oxidizing a starting ilmenite; after the oxidation step, a reduction step of reducing the treated ilmenite; and after the reduction step, an extraction step of dissolving the iron component with an acid, to thereby remove the iron component. Also disclosed is a production method for producing a high-TiO2-content titanium source, which includes upgrading an ilmenite ore as described above, and a high-TiO2-content titanium source produced through the production method.

## Claims

### Claim 1

A method for upgrading an ilmenite ore for yielding a high-TiO2-content titanium source by separating and removing an iron component from ilmenite (FeTiO3), characterized in that the method comprises an oxidation step of oxidizing a starting ilmenite;
after the oxidation step, a reduction step of reducing the treated ilmenite; and after the reduction step, an extraction step of dissolving the iron component with an acid, to thereby remove the iron component.

### Claim 2 (depends on 1)

The ilmenite ore upgrading method as claimed in claim 1, wherein, in the oxidation step, an ilmenite phase (FeTiO3) is converted to a hematite phase (Fe2O3) and a rutile phase (TiO2), without forming a pseudo-brookite phase (Fe2TiO5), which is basically insoluble in acid.

### Claim 3 (depends on 2)

The ilmenite ore upgrading method as claimed in claim 2, wherein, in the reduction step, the hematite phase (Fe2O3) is reduced to metallic iron (Fe).

### Claim 4 (depends on 1)

The ilmenite ore upgrading method as claimed in claim 1, wherein the oxidation step is performed at 600° C. to a temperature lower than 800° C.

### Claim 5 (depends on 1)

The ilmenite ore upgrading method as claimed in claim 1, wherein the reduction step is performed at 500° C. to 900° C.

### Claim 6 (depends on 1)

A method for producing a high-TiO2-content titanium source, the method comprising upgrading an ilmenite ore through an ilmenite ore upgrading method claimed in claim 1.

### Claim 7 (depends on 6)

A high-TiO2-content titanium source produced through a production method as claimed in claim 6.