# US 2017/0253770 A1 · Adhesive film and display member using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253770 A1
- Document ID: US20170253770A1
- Status: Published application
- Kind: A1
- Application number: 15/506,648
- Filed: 2015-06-29
- Published: 2017-09-07
- Earliest claimed: 2014-08-29
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Irina NAM; Young Jong KIM; Hwan Sung CHEON; In Cheon HAN
- Web page: https://patentgrep.com/patent/US20170253770A1

## CPC

- C09J 7/10: without carriers
- C09J 133/06: of esters containing only carbon, hydrogen and oxygen, the oxygen atom being present only as part of the carboxyl radical
- C09J 133/068: {containing glycidyl groups}
- G02F 1/13338: {Input devices, e.g. touch panels}
- C09J 133/14: of esters containing halogen, nitrogen, sulfur or oxygen atoms in addition to the carboxy oxygen
- C09J 2203/318: for the production of liquid crystal displays
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2301/414: presence of a copolymer
- C09J 2433/00: Presence of (meth)acrylic polymer
- G02B 5/30: Polarising elements (light-modulating devices with active elements G02F1/00)
- G02F 2202/28: Adhesive materials or arrangements
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

An adhesive film of the present invention comprises a (meth)acrylate-based copolymer and a cross-linking agent, and a gel fraction thereof is approximately 50-95%, and a ratio of change G′ in storage modulus thereof, represented by the following formula 1, is 20% or less. [Formula 1] G′=(G7−G1)/G1×100 (In formula 1, G1 is a storage modulus at 25° C. when the adhesive film is matured at 23° C. and a relative humidity (RH) of 55% for one day, and G7 represents a storage modulus at 25° C. when the adhesive film is matured at 23° C. and an RH of 55% for seven days.)

## Claims

### Claim 1

A pressure-sensitive adhesive film comprising a (meth)acrylate copolymer and a crosslinker and having a gel fraction of about 50% to about 95% and a storage modulus variation G′ of about 20% or less as represented by Equation 1:
G′=(G7−G1)/G1×100 [Equation 1]
where G1 is the storage modulus of the pressure-sensitive adhesive film at 25° C. after aging at 23° C. and 55% RH for 1 day and G7 is the storage modulus of the pressure-sensitive adhesive film at 25° C. after aging at 23° C. and 55% RH for 7 days.

### Claim 2 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the pressure-sensitive adhesive film has a storage modulus variation G′ of about 0.5% to about 10%.

### Claim 3 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the pressure-sensitive adhesive film has storage moduli G1 and G7 at 25° C. of about 105 Pa to about 106 Pa.

### Claim 4 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the pressure-sensitive adhesive film has a gel fraction difference of about 10% or less as calculated by Equation 2:
Gel fraction difference=GF7−GF1 [Equation 2]
where GF7 is the gel fraction after aging for 7 days as calculated by Equation 3 and GF1 is the gel fraction after aging for 1 day as calculated by Equation 3:
Gel fraction (%)=(WC−WA)/(WB−WA)×100 [Equation 3]
where WA is the weight of a wire mesh; WB is the total weight of 0.5 g of a specimen covered with the wire mesh, in which the specimen is obtained by aging the pressure-sensitive adhesive film at 23° C. and 55% RH for 1 day or 7 days; and WC is the total weight of the pressure-sensitive adhesive film and the wire mesh obtained by placing a specimen, obtained by aging the pressure-sensitive adhesive film and covered with the wire mesh, in a sample bottle and adding 50 cc of ethyl acetate to the sample bottle, followed by storage at 25° C. for 1 day and drying at 100° C. for 12 hours.

### Claim 5 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the pressure-sensitive adhesive film has an acid value of about 0.

### Claim 6 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the (meth)acrylate copolymer has a weight average molecular weight of about 100,000 g/mol to about 1,500,000 g/mol.

### Claim 7 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the (meth)acrylate copolymer has a polydispersity index (PDI) of about 2.5 to about 6.0.

### Claim 8 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the (meth)acrylate copolymer has a glass transition temperature (Tg) of about −40° C. to about −10° C.

### Claim 9 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the (meth)acrylate copolymer is a copolymer of a monomer mixture comprising an alkyl (meth)acrylate monomer, a monomer having a glass transition temperature (Tg) of about 50° C. or higher, and an oxygen-containing heterocyclic ring containing monomer.

### Claim 10

A pressure-sensitive adhesive film comprising:
a (meth)acrylate copolymer, the (meth)acrylate copolymer comprising a copolymer of a monomer mixture comprising an alkyl (meth)acrylate monomer, a monomer having a glass transition temperature (Tg) of about 50° C. or higher and an oxygen-containing heterocyclic ring containing monomer; and a crosslinker.

### Claim 11 (depends on 1)

The pressure-sensitive adhesive film according to claim 1, wherein the (meth)acrylate copolymer comprises about 60 wt % to about 94.9 wt % of the alkyl (meth)acrylate monomer, about 5 wt % to about 30 wt % of the monomer having a glass transition temperature (Tg) of about 50° C. or higher, and about 0.1 wt % to about 10 wt % of the oxygen-containing heterocyclic ring containing monomer.

### Claim 12 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the alkyl (meth)acrylate monomer comprises (meth)acrylate esters having a C1 to C20 linear or branched alkyl group.

### Claim 13 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the monomer having a glass transition temperature (Tg) of about 50° C. or higher comprises at least one of N-vinylpyrrolidone, acrylamide, N-alkyl substituted acrylamide, acryloylmorpholine, isobornyl acrylate, and cyclohexyl methacrylate.

### Claim 14 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the oxygen-containing heterocyclic ring containing monomer comprises at least one oxygen-containing heterocyclic ring of an epoxy group, an oxetane group, and a tetrahydrofurfuryl group.

### Claim 15 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the oxygen-containing heterocyclic ring containing monomer comprises at least one of glycidyl methacrylate, oxetane methacrylate, and tetrahydrofurfuryl acrylate.

### Claim 16

(canceled)

### Claim 17 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the pressure-sensitive adhesive film further comprises a silane coupling agent.

### Claim 18 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the pressure-sensitive adhesive film has a storage modulus variation G′ of about 20% or less as represented by Equation 1:
G′=(G7−G1)/G1×100 [Equation 1]
where G1 is the storage modulus of the pressure-sensitive adhesive film at 25° C. after aging at 23° C. and 55% RH for 1 day and G7 is the storage modulus of the pressure-sensitive adhesive film at 25° C. after aging at 23° C. and 55% RH for 7 days.

### Claim 19 (depends on 18)

The pressure-sensitive adhesive film according to claim 18, wherein the pressure-sensitive adhesive film has storage moduli G1 and G7 at 25° C. of about 105 Pa to about 106 Pa.

### Claim 20

(canceled)

### Claim 21 (depends on 10)

The pressure-sensitive adhesive film according to claim 10, wherein the pressure-sensitive adhesive film has a gel fraction difference of about 10% or less as calculated by Equation 2:
Gel fraction difference=GF7−GF1 [Equation 2]
where GF7 is the gel fraction after aging for 7 days as calculated by Equation 3 and GF1 is the gel fraction after aging for 1 day as calculated by Equation 3:
Gel fraction (%)=(WC−WA)/(WB−WA)×100 [Equation 3]
where WA is the weight of a wire mesh; WB is the total weight of 0.5 g of a specimen covered with the wire mesh, in which the specimen is obtained by aging the pressure-sensitive adhesive film at 23° C. and 55% RH for 1 day or 7 days; and WC is the total weight of the pressure-sensitive adhesive film and the wire mesh obtained by placing the specimen, which is obtained by aging the pressure-sensitive adhesive film and covered with the wire mesh, in a sample bottle and adding 50 cc of ethyl acetate to the sample bottle, followed by storage at 25° C. for 1 day and drying at 100° C. for 12 hours.

### Claim 22 (depends on 1)

A display member comprising the pressure-sensitive adhesive film of claim 1.